公开(公告)号:US20170248809A1
公开(公告)日:2017-08-31
申请号:US15593914
申请日:2017-05-12
Applicant: FUJIFILM Corporation
Inventor: Tatsuya OBA , Tomonari OGAWA , Keisuke OKU
IPC: G02F1/1335 , F21V8/00
CPC classification number: G02F1/1336 , F21V9/30 , G02B6/005 , G02F1/1303 , G02F2001/133614 , G02F2202/36
Abstract: The wavelength conversion member includes: a first substrate; a second substrate; and a wavelength conversion layer disposed between the first substrate and the second substrate and including quantum dots which are excited by excitation light to emit fluorescence. The wavelength conversion layer is a cured layer obtained by curing a polymerizable composition which includes the quantum dots and a polymerizable compound having a molecular weight of 200 or lower, and the number of bubble-shaped defects having a diameter of 0.1 mm or more in the wavelength conversion layer is less than 10 per 100 cm2.
-
公开(公告)号:US20170090248A1
公开(公告)日:2017-03-30
申请号:US15355787
申请日:2016-11-18
Applicant: FUJIFILM Corporation
Inventor: Hiroyuki YONEYAMA , Hideaki ITOU , Tomonari OGAWA , Satoshi KUNIYASU
IPC: G02F1/1335
CPC classification number: G02F1/133617 , B29D11/0073 , B29D11/00788 , B32B7/02 , B32B7/12 , B32B27/08 , B32B27/36 , B32B37/1284 , B32B37/203 , B32B2037/243 , B32B2255/10 , B32B2255/20 , B32B2255/205 , B32B2255/26 , B32B2264/10 , B32B2264/102 , B32B2307/412 , B32B2307/422 , B32B2307/546 , B32B2307/7244 , B32B2307/732 , B32B2310/0831 , B32B2457/12 , B32B2457/14 , B32B2457/20 , B32B2457/202 , B82Y20/00 , C09K11/02 , C09K11/08 , G02B6/00 , G02F1/1303 , G02F1/133504 , G02F1/133528 , G02F1/133615 , G02F1/133621 , G02F2001/133614 , G02F2202/023 , G02F2202/28 , G02F2202/36 , G02F2203/05
Abstract: Provided is manufacturing method of a quantum dot-containing laminated body including: forming a coating film by applying a quantum dot-containing composition which contains quantum dots, a curable compound, and a thixotropic agent and has a viscosity in a case of a shear rate of 500 s−1 of 3 to 100 mPa·s and a viscosity in a case of a shear rate of 1 s−1 of equal to or greater than 300 mPa·s, onto a first base material; laminating a second base material onto the coating film; and applying external stimuli to the coating film sandwiched between the first base material and the second base material for hardening, and forming a quantum dot-containing layer. The manufacturing method realizes high productivity, obtains a quantum dot-containing layer without coating streaks, and has slight film thickness unevenness of the quantum dot-containing laminated body.
-