1.
公开(公告)号:US20190077710A1
公开(公告)日:2019-03-14
申请号:US16121381
申请日:2018-09-04
Applicant: HONEYWELL INTERNATIONAL INC.
Inventor: Ruixing Yuan , Yue Wen Liu , Wei Wang , Yuansheng Shen
Abstract: Asphalt emulsions, methods of forming asphalt emulsions, and composite pavement structures formed from the asphalt emulsions are provided herein. In an embodiment, an asphalt emulsion includes a base asphalt component, water, and an oxidized high density polyethylene. The base asphalt component is present in an amount of from about 15 to about 70 weight %, the water is present in an amount of at least about 25 weight %, and the oxidized high density polyethylene is present in an amount of from about 1 to about 20 weight %, where all amounts are based on the total weight of the asphalt emulsion. The oxidized high density polyethylene has an acid value of from about 5 to about 50 mgKOH/g. The asphalt emulsion is free of aggregate and other mineral materials.
-
2.
公开(公告)号:US11174200B2
公开(公告)日:2021-11-16
申请号:US16121381
申请日:2018-09-04
Applicant: HONEYWELL INTERNATIONAL INC.
Inventor: Ruixing Yuan , Yue Wen Liu , Wei Wang , Yuansheng Shen
Abstract: Asphalt emulsions, methods of forming asphalt emulsions, and composite pavement structures formed from the asphalt emulsions are provided herein. In an embodiment, an asphalt emulsion includes a base asphalt component, water, and an oxidized high density polyethylene. The base asphalt component is present in an amount of from about 15 to about 70 weight %, the water is present in an amount of at least about 25 weight %, and the oxidized high density polyethylene is present in an amount of from about 1 to about 20 weight %, where all amounts are based on the total weight of the asphalt emulsion. The oxidized high density polyethylene has an acid value of from about 5 to about 50 mgKOH/g. The asphalt emulsion is free of aggregate and other mineral materials.
-
公开(公告)号:US20190185725A1
公开(公告)日:2019-06-20
申请号:US16192016
申请日:2018-11-15
Applicant: HONEYWELL INTERNATIONAL INC.
Inventor: Yonghong Ruan , Ruixing Yuan , Scott Martin Hacker
IPC: C09J195/00 , C09J11/06 , C09J11/08
CPC classification number: C09J195/00 , C08L23/06 , C08L23/14 , C08L23/30 , C08L55/005 , C09J11/06 , C09J11/08
Abstract: Asphalt adhesive compositions and methods of producing the same are provided. In an exemplary embodiment, an asphaltic adhesive useful for self-adhering membranes includes asphalt at from about 40 to about 70 weight percent, based on a total weight of the adhesive. The adhesive also includes a low molecular weight (LMW) polyolefin at from about 1 to about 10 weight percent, based on the total weight of the adhesive. The LMW polyolefins have a weight average molecular weight (Mw) of from about 500 to about 20,000 Daltons. The adhesive has an aged peeling strength greater than an aged peeling strength of a comparable comparison adhesive, wherein the comparison adhesive includes from about 40 to about 70 weight percent asphalt but is free of a LMW polyolefin, as determined by Guobiao recommended (GB/T) 328.20-2007 in specification Guobiao (GB) 23441-2009 (self-adhering polymer modified bituminous waterproof sheet.)
-
公开(公告)号:US20190071587A1
公开(公告)日:2019-03-07
申请号:US15318434
申请日:2014-07-16
Applicant: Ruixing YUAN , Jun LI , Sean SHEN , HONEYWELL INTERNATIONAL INC.
Inventor: Ruixing Yuan , Jun Li , Sean Shen
IPC: C09D195/00 , C09D7/65 , C09D7/61 , C09D7/80
Abstract: An asphalt coating for roofing waterproof membranes is provided and comprises: from about 30 to about 88 weight percent (wt %) of asphalt; from about 0.1 to about 15 wt % of a low molecular weight (MW) polyethylene; from about 1 to about 30 wt % of a thermoplastic elastomer; from about 5 to about 48 wt % of an inorganic filler; and from about 1 to about 20 wt % of a softening agent; all based on the total weight of the asphalt coating.
-
公开(公告)号:US20170190618A1
公开(公告)日:2017-07-06
申请号:US15370683
申请日:2016-12-06
Applicant: HONEYWELL INTERNATIONAL INC.
Inventor: Wei Wang , Ruixing Yuan , Yuansheng Shen , Xiang Wang , Jun Li
CPC classification number: C04B26/26 , C04B24/2611 , C04B2111/0075 , C08L95/00 , C08L2555/30 , C08L2555/34 , E01C7/18 , Y02W30/95 , C04B18/167 , C04B38/10 , C04B40/0082 , C08L23/30
Abstract: Foamed asphalt compositions, recycled asphalt compositions, asphalt pavement, and methods of forming asphalt pavement using the foamed asphalt compositions are provided herein. An exemplary foamed asphalt composition is in a cellular matrix form and includes a base asphalt component and oxidized high density polyethylene. An exemplary asphalt pavement includes a recycled asphalt layer that includes the foamed asphalt composition and a recycled asphalt component. An exemplary method of forming asphalt pavement includes combining a base asphalt component and an oxidized high density polyethylene to form an asphalt mixture. The asphalt mixture is foamed using water and compressed air to form a foamed asphalt composition. The foamed asphalt composition and a recycled asphalt component are combined to form a recycled asphalt composition. A recycled asphalt layer is formed with the recycled asphalt composition.
-
-
-
-