摘要:
A birefringent pattern builder, having an optically anisotropic layer containing a polymer having unreacted reactive groups,wherein the optically anisotropic layer is produced by a method containing the steps [1] and [2] in this order: [1] coating and drying a solution containing a liquid crystalline compound having at least two kinds of reactive groups; and [2] reacting one kind of the at least two kinds of reactive groups by applying heat or irradiating ionizing radiation.
摘要:
A viewer for authenticating a birefringent pattern having at least two regions having a different birefringence from each other, wherein the viewer contains a polarizing plate and at least one optically anisotropic layer laminated on the polarizing plate, a front retardation of the at least one optically anisotropic layer is 5 nm or more and the total of the front retardation of the at least one optically anisotropic layer and a maximum value of front retardation of the birefringent pattern is greater than λ/2.
摘要:
A transfer material comprising an optically anisotropic layer formed of a liquid crystalline composition comprising a monomer having an acidic group and/or a monomer which generates a monomer having an acidic group by an action of an acid or a base, and a photosensitive polymer layer, which is useful for forming an optically anisotropic layer in a liquid crystal cell, is provided. A process for easily producing a laminated structure having a patterned optically anisotropic layer, which comprises the following steps [1] and [2]: [1] subjecting the transfer material to patterned light exposure using photomask; and [2] removing the non-exposed parts of the transfer material by development with an aqueous alkaline solution, is also provided.
摘要:
A polymerizable liquid crystal compound is represented by the following formula (1): P-Sp1-L1-M1-L2-Sp2-Ox (1) wherein P represents a polymerizable group; one of Sp1 and Sp2 represents a branched alkylene group, or an alkylene group containing, in the chain thereof, at least one divalent linking group selected from the group consisting of —O—, —C≡C— and —S—; the other of Sp1 and Sp2 represents a straight chain alkylene group; each of L1 and L2 independently represents a divalent linking group; M1 represents a mesogenic group; and Ox represents a substituent containing an oxetanyl group.
摘要:
A method of producing a patterned birefringent product, containing at least steps (I) to (III) in this order: (I) providing a birefringent pattern builder having an optically anisotropic layer containing a polymer; (II) subjecting two or more regions of the birefringent pattern builder to exposure to light under exposure conditions different from each other; and (III) heating a laminated structure obtained after the step (II) at 50° C. or higher and 400° C. or lower.
摘要:
A transfer material comprising at least one optically anisotropic layer and at least one photosensitive polymer layer on at least one support, wherein said optically anisotropic layer comprises one or more compounds having a reactive group, and said photosensitive polymer layer comprises two or more types of photopolymerization initiators having different photoreaction mechanisms to each other, and a compound having a reactive group which can react with one or more of the reactive groups present in the optically anisotropic layer by the action of the at least one of said photopolymerization initiators. By using the transfer material, a color filter which contributes to reducing viewing angle dependence of color of a liquid crystal display device, and a liquid crystal display device having less corner non-uniformities and less viewing angle dependence of color.
摘要:
A birefringent pattern builder, having an optically anisotropic layer containing a polymer having unreacted reactive groups,wherein the optically anisotropic layer is produced by a method containing the steps [1] and [2] in this order: [1] coating and drying a solution containing a liquid crystalline compound having at least two kinds of reactive groups; and [2] reacting one kind of the at least two kinds of reactive groups by applying heat or irradiating ionizing radiation.
摘要:
A method of producing a patterned birefringent product, having at least steps (I) to (III) in this order: (I) providing a birefringent pattern builder having an optically anisotropic layer containing a polymer having unreacted reactive groups; (II) heating a region of the birefringent pattern builder; and (III) subjecting the birefringent pattern builder to a process that reacts at least a part of the unreacted reactive groups in the optically anisotropic layer.
摘要:
A medium for preventing forgery having a hologram layer and at least one patterned optically anisotropic layer, wherein the patterned optically anisotropic layer has two or more regions comprising different birefringence property, and wherein all the regions are formed of the same composition.
摘要:
A process of readily producing a patterned birefringent product excellent in resolution and heat-resistance is provided. Said process comprises at least the following steps [1] to [3] in order: [1] preparing a birefringence pattern builder which comprises an optically anisotropic layer comprising a polymer, and said optically anisotropic layer has a retardation disappearance temperature in the range higher than 20° C., at said retardation disappearance temperature in-plane retardation becomes 30% or lower of the retardation at 20° C. of the same optically anisotropic layer, and said retardation disappearance temperature rises by light exposure; [2] subjecting the birefringence pattern builder to patterned light exposure; [3] heating the laminated structure obtained after the step [2] at 50° C. or higher and 400° C. or lower.