公开(公告)号:US11965066B2
公开(公告)日:2024-04-23
申请号:US17251324
申请日:2019-06-11
Applicant: INEOS STYROLUTION GROUP GMBH
Inventor: Tobias Schulz , Christian Ruthard
IPC: C08L25/12 , C08F220/18 , C08J3/00 , C08J3/20 , C08K3/013 , C08K5/00 , C08L51/00 , C08L83/04 , C08L83/10
CPC classification number: C08J3/005 , C08F220/1804 , C08J3/20 , C08K3/013 , C08K5/0041 , C08L25/12 , C08L51/003 , C08L83/04 , C08L83/10 , C08L2201/08 , C08L2201/52 , C08L2203/30 , C08L2205/025 , C08L2205/035 , C08L2205/18 , C08L2205/22
Abstract: The present invention relates to a method of improving UV resistance of a vinylaro-maticmolding mass by means of compounding a thermoplastic polymer composition which comprises at least one graft copolymer with an organopolysiloxane compound and optionally further components.
-
2.
公开(公告)号:US12152099B2
公开(公告)日:2024-11-26
申请号:US17262018
申请日:2019-07-22
Applicant: INEOS STYROLUTION GROUP GMBH
Inventor: Tobias Schulz , Wolfgang Fischer , Norbert Niessner , Christian Ruthard , Hannes Kerschbaumer
IPC: C08F257/02 , C08F2/22 , C08F212/08 , C08F220/44 , C08F265/06 , C08L25/12 , C08L33/20 , C08L51/04
Abstract: Polyacrylate graft rubber copolymer B and an impact modified thermoplastic molding composition thereof, where the graft copolymer B is composed of: B1: 50 to 70 wt.-% crosslinked acrylate polymer graft base B1 B2: 30 to 50 wt.-% graft shell B2 comprising a first layer B21 of vinylaromatic monomers, and a second layer B22 of vinylaromatic monomers B21-1 and nitrile monomers B22-2: wherein the particle diameter dw of the graft base BI is 255 to 290 nm; the fraction of B21 is 10 to 26 wt.-%; and the amount of B22-2, is 20 to 30 wt.-%.
-
公开(公告)号:US10047220B2
公开(公告)日:2018-08-14
申请号:US14900748
申请日:2014-07-01
Applicant: INEOS STYROLUTION GROUP GMBH
Inventor: Norbert Niessner , Brian Banaszak , Rudy Verstraeten , Gisbert Michels , Wolfgang Fischer , Christian Ruthard , Ulrich Jansen
IPC: B29B7/46 , C08L25/12 , B29B7/48 , B29C47/40 , B29C47/60 , B29C47/64 , B29C47/76 , B29C47/92 , C08L55/02 , B29B7/18
Abstract: A process for preparing a thermoplastic polymer composition or a thermoplastic polymer blend, comprising: —from 20 to 80% by weight of at least one water-moist elastomer component A containing up to 40%, preferably up to 30% by weight of residual water, —from 20 to 80% by weight of at least one thermoplastic polymer B, —from 0 to 40% by weight of at least one further polymer C, and —from 0 to 60% by weight of additive(s) D, by mixing the elastomer component A with the thermoplastic polymer B and, if present, the further polymer C and, if present, the additive(s) D in an extruder, comprising the steps of precipitating the elastomer component A, and mechanical dewatering of the elastomer component A leads to improved salt-free products.
-
-