Abstract:
There is provided a polymer film which includes: a base film layer including a polyamide-based resin having a particular relative viscosity and a copolymer including a polyamide-based segment and a polyether-based segment having a specific content; and an adhesive layer formed on at least one side of the base film layer, wherein a ratio of the melt viscosity of the copolymer to the melt viscosity of the polyamide resin is 0.65 to 1.2 at a shear rate of 1000 s−1 and a temperature of 260° C.
Abstract:
There is provided a polymer film which includes a base film layer having an absolute weight average molecular weight of 50,000 to 1,000,000 and an adhesive layer, and a method for manufacturing the polymer film. This film for a tire inner liner can endow an excellent gas barrier property even to tires having a relatively thin thickness so that weight of the tire can be reduced and fuel efficiency of automobiles can be improved. Further, the present film facilitates molding in a tire manufacturing process, and exhibits excellent adhesion force to a carcass layer while having excellent mechanical properties such as high durability and fatigue resistance together with excellent moldability.
Abstract:
This disclosure relates to a film for an inner liner including a base film layer and an adhesive layer, the base film layer including a polyamide-based resin, a specific copolymer, and a polymer crystallization retardant, and a method for manufacturing the same.