Very low melt viscosity resin
    1.
    发明授权
    Very low melt viscosity resin 失效
    非常低的熔融粘度树脂

    公开(公告)号:US06992146B2

    公开(公告)日:2006-01-31

    申请号:US10998411

    申请日:2004-11-29

    IPC分类号: C08F8/06

    摘要: A process is provided for the production of a very low melt viscosity (high melt flow index) polymer resin, suitable for use in spunbond or meltblown processing. According to the process of the current invention, a high melt viscosity (low melt flow index) resin is subjected to post-reactor molecular weight alteration by extrusion with a chemical prodegradant. The process produces a very low melt viscosity resin that can be used in spunbond or meltblown processing without further treatment to reduce the average molecular weight of the resin. Further, the very low melt viscosity resins produced according to the process of the current invention contain very little or no residual prodegradant.

    摘要翻译: 提供了一种生产适用于纺粘或熔喷处理的非常低熔体粘度(高熔体流动指数)聚合物树脂的方法。 根据本发明的方法,通过用化学降解剂进行挤出,使高熔体粘度(低熔体流动指数)树脂进行后反应器分子量改变。 该方法产生非常低的熔体粘度树脂,其可以用于纺粘或熔喷处理,而不需要进一步处理以降低树脂的平均分子量。 此外,根据本发明的方法生产的非常低的熔体粘度树脂含有很少或没有残留的降解剂。

    Very low melt viscosity resin
    2.
    发明授权
    Very low melt viscosity resin 失效
    非常低的熔融粘度树脂

    公开(公告)号:US06855777B2

    公开(公告)日:2005-02-15

    申请号:US10224715

    申请日:2002-08-22

    摘要: A process is provided for the production of a very low melt viscosity (high melt flow index) polymer resin, suitable for use in meltblown processing. According to the process of the current invention, a high melt viscosity (low melt flow index) resin is subjected to post-reactor molecular weight alteration by extrusion with a chemical prodegradant. The process produces a very low melt viscosity resin that can be used in meltblown processing without further treatment to reduce the average molecular weight of the resin. Further, the very low melt viscosity resins produced according to the process of the current invention contain very little or no residual prodegradant.

    摘要翻译: 提供了一种生产适用于熔喷处理的非常低的熔体粘度(高熔体流动指数)聚合物树脂的方法。 根据本发明的方法,通过用化学降解剂进行挤出,使高熔体粘度(低熔体流动指数)树脂进行后反应器分子量改变。 该方法产生非常低的熔融粘度树脂,其可以用于熔喷处理而不进行进一步处理以降低树脂的平均分子量。 此外,根据本发明的方法生产的非常低的熔体粘度树脂含有很少或没有残留的降解剂。

    Polyolefin additive packages for producing articles with enhanced stain resistance
    3.
    发明授权
    Polyolefin additive packages for producing articles with enhanced stain resistance 有权
    用于生产具有增强的耐污性的制品的聚烯烃添加剂包

    公开(公告)号:US06777470B2

    公开(公告)日:2004-08-17

    申请号:US09867198

    申请日:2001-05-29

    IPC分类号: C08L517

    摘要: The present invention provides additive packages for polyolefins The additive packages of the present invention comprise at least one non-phenolic antioxidant and a hindered amine light stabilizer. The additive packages may contain other additives as needed, and may optionally include an acid scavenger. Articles made from the resultant polymers, such as radiator surge tanks, exhibit enhanced stain and discoloration resistance upon exposure to high temperatures and harsh chemicals such as those experienced in “under the hood” spaces of modern automobiles.

    摘要翻译: 本发明提供了用于聚烯烃的添加剂包。本发明的添加剂包含至少一种非酚类抗氧化剂和受阻胺光稳定剂。 添加剂包可以根据需要含有其它添加剂,并且可任选地包括酸清除剂。 由所得聚合物制成的制品,例如散热器缓冲罐,暴露在高温下,显示出增强的污渍和耐变色性,以及诸如现代汽车“底罩”空间之类的恶劣化学品。

    Clarity, low haze polymer
    4.
    发明授权
    Clarity, low haze polymer 有权
    澄清度,低雾度聚合物

    公开(公告)号:US07452919B2

    公开(公告)日:2008-11-18

    申请号:US10855922

    申请日:2004-05-27

    IPC分类号: C08J11/04

    摘要: A method of manufacturing an improved clarity, low haze, low melt flow rate homopolymer polypropylene and thermoformed parts therefrom using an additive package such that the additive package alone provides the improved qualities, and process adjustments at the thermoforming stage are not required. The additive package does not contain a phosphite antioxidant, and the homopolymer polypropylene is either virgin material or virgin material mixed with at least 25 percent reground homopolymer polypropylene of the improved formulation described herein and combined with the improved clarity additive package.

    摘要翻译: 使用添加剂包装制造改进的澄清度,低雾度,低熔体流动速率的均聚物聚丙烯和其热成型部件的方法,使得仅添加剂包装提供改进的质量,并且不需要在热成型阶段的工艺调整。 添加剂包不含亚磷酸酯抗氧化剂,均聚聚丙烯是与本文所述改进制剂的至少25%重复均聚聚丙烯混合的原始材料或原始材料,并与改进的澄清添加剂包合并。