摘要:
The present invention provides a propylene polymer composition having excellent transparency, flexibility, heat resistance, scratch resistance and rubber elasticity with a good balance. The propylene polymer composition comprises 1 to 40 parts by weight of isotactic polypropylene (i) and 60 to 99 parts by weight of a propylene/ethylene/α-olefin copolymer (ii) which contains 45 to 89% by mol of a propylene component, 10 to 25% by mol of an ethylene component, and optionally, 0 to 30% by mol of constituent units (a) derived from an α-olefin of 4 to 20 carbon atoms.
摘要:
A syndiotactic propylene-based polymer composition which retains the inherent features of the conventional non-crosslinked or partially crosslinked olefin-based thermoplastic elastomer, and also has excellent abrasion resistance and flexibility.The syndiotactic propylene-based polymer composition comprises 1 to 40 parts by weight of the syndiotactic polypropylene (B), and 5 to 60 parts by weight of the syndiotactic structured propylene-α-olefin copolymer (C) comprising 95 to 65 mol % of a syndiotactic structured propylene component and 5 to 35 mol % of an α-olefin (except propylene) component having 2 to 20 carbon atoms, based on 100 parts by weight of the non-crosslinked or partially crosslinked olefin-based thermoplastic elastomer (A).
摘要:
The invention provides a propylene polymer composition well balanced and excellent in transparency, flexibility, heat resistance, scratch resistance and rubber elasticity, and a medical tube made from the propylene polymer composition. The propylene polymer composition satisfies all the following properties (A), (B), (C) and (D): (A) the composition shows a loss tangent (tan δ) peak at a temperature in the range of −20 to 25° C. according to dynamic viscoelasticity measurement (10 rad/s) in a torsion mode, and the peak is 0.5 or above; (B) the storage elastic modulus G′ at 20° C. from the dynamic viscoelasticity measurement is in the range of 1.0×107 to 4.9×108 dyn/cm2; (C) the penetration temperature (° C.) determined in accordance with JIS K 7196 is in the range of 60 to 160° C.; and (D) the composition has a permanent set of not more than 30% as determined after the composition fixed between chucks 30 mm apart is 100% strained at a stress rate of 30 mm/min, maintained for 10 minutes and released for 10 minutes. The medical tube is made from the propylene polymer composition.
摘要:
The present invention provides a propylene polymer composition having excellent transparency, flexibility, heat resistance, scratch resistance and rubber elasticity with a good balance. The propylene polymer composition comprises 1 to 40 parts by weight of isotactic polypropylene (i) and 60 to 99 parts by weight of a propylene/ethylene/α-olefin copolymer (ii) which contains 45 to 89% by mol of a propylene component, 10 to 25% by mol of an ethylene component, and optionally, 0 to 30% by mol of constituent units (a) derived from an α-olefin of 4 to 20 carbon atoms.
摘要:
The invention provides a propylene polymer composition well balanced and excellent in transparency, flexibility, heat resistance, scratch resistance and rubber elasticity, and a medical tube made from the propylene polymer composition. The propylene polymer composition satisfies all the following properties (A), (B), (C) and (D): (A) the composition shows a loss tangent (tan δ) peak at a temperature in the range of −20 to 25° C. according to dynamic viscoelasticity measurement (10 rad/s) in a torsion mode, and the peak is 0.5 or above; (B) the storage elastic modulus G′ at 20° C. from the dynamic viscoelasticity measurement is in the range of 1.0×107 to 4.9×108 dyn/cm2; (C) the penetration temperature (° C.) determined in accordance with JIS K 7196 is in the range of 60 to 160° C.; and (D) the composition has a permanent set of not more than 30% as determined after the composition fixed between chucks 30 mm apart is 100% strained at a stress rate of 30 mm/min, maintained for 10 minutes and released for 10 minutes. The medical tube is made from the propylene polymer composition.
摘要:
A syndiotactic propylene-based polymer composition which retains the inherent features of the conventional non-crosslinked or partially crosslinked olefin-based thermoplastic elastomer, and also has excellent abrasion resistance and flexibility. The syndiotactic propylene-based polymer composition comprises 1 to 40 parts by weight of the syndiotactic polypropylene (B), and 5 to 60 parts by weight of the syndiotactic structured propylene-α-olefin copolymer (C) comprising 95 to 65 mol % of a syndiotactic structured propylene component and 5 to 35 mol % of an α-olefin (except propylene) component having 2 to 20 carbon atoms, based on 100 parts by weight of the non-crosslinked or partially crosslinked olefin-based thermoplastic elastomer (A).
摘要:
The present invention proposes a molded product having excellent moldability and ability to be processed into parts, as well as excellent scratch resistance. The invention provides a multilayered laminate composed of two or more layers, having a structure in which a layer (I) comprising at least one selected from an olefinic thermoplastic elastomer composition (A) and an olefinic resin (B), and a layer (II) comprising an olefinic thermoplastic elastomer composition (C) are laminated. The olefinic thermoplastic elastomer composition (C) is a composition comprising [1] a specific syndiotactic polypropylene copolymer (c), and [2] at least one selected from a polypropylene resin (d) and an olefinic thermoplastic elastomer (e).
摘要:
A composition having excellent transparency, flexibility, rubber elasticity, thermal resistance, impact resistance, abrasion resistance and the like, a composition having excellent rigidity and impact resistance as well as excellently balanced in whitening resistance, abrasion resistance and heat sealability, and a composition having excellent rubbery properties, thermal resistance, abrasion resistance and flexibility are provided.A composition comprising a specific propylene•α-olefin copolymer for which, in a signal chart measured by 13C-NMR and predetermined such that the peak present at the highest magnetic field among the signals originating from CH (methine) of the constituent unit derived from an α-olefin having 4 to 20 carbon atoms is to be at 34.4 ppm, an absorption intensity A at about 22.0 to 20.9 ppm and an absorption intensity B at about 19.0 to 20.6 ppm satisfy the following relational expressions (i) and (ii) with respect to an absorption intensity C at about 19.0 to 22.0 ppm, which is assignable to propylene methyl: (A/C)×100≦8 (i), and (B/C)×100≧60 (ii), a molded product thereof, and the α-olefin-based copolymer are provided.
摘要:
A material for vibration control of the invention includes a propylene polymer (A) containing a constitutional unit (a) derived from propylene in the proportion of 40 to 100 mol % and a constitutional unit (b) derived from α-olefin having 2 to 20 carbon atoms excluding propylene in the proportion of 60 to 0 mol % [provided that the total of (a) and (b) is 100 mol %], and having a melting point measured by DSC of 90° C. or below or no observed melting point, and the material has excellent vibration controllability such as vibration damping property, vibration preventing property, sound insulating property, and sound absorbing property.
摘要:
[Task] To provide a solar battery sealing material obtained by using an olefin-based (co)polymer, which is excellent in flexibility, stress-absorbing property, transparency, and impact-resistant strength at low temperature, and with which the productivity is improved by omitting a cross-linking treatment if necessary.[Solving Means] A solar battery sealing material containing 1 to 40 parts by weight of polypropylene (i) which has a propylene unit of more than 90 mol %; and 60 to 99 parts by weight of a propylene.ethylene-based copolymer (ii) which has a propylene unit of 45 to 90 mol %, an ethylene unit of 10 to 25 mol %, and an α-olefin unit (a) having 4 to 20 carbon atoms of 0 to 30 mol % ((i)+(ii)=100 parts by weight). The solar battery sealing material further contains 5 to 95 parts by weight of an ethylene.α-olefin copolymer (B), based on 95 to 5 parts by weight of the total amount of (i) and (ii) ((i)+(ii)+(B)=100 parts by weight).