Abstract:
A method for producing a laminated body including a base material and a coating layer laminated on the base material, includes: applying a coating liquid containing cellulose nanofibers onto the base material composed of at least acid-resistant paper, thereby forming the coating layer. In addition, an average fiber diameter of the cellulose nanofibers is 2 nm or more and 2000 nm or less, a content of the cellulose nanofibers in the coating liquid is 10 mass % or more of solid contents of the coating liquid, and a coating amount of the coating layer is 0.2 g/m2 or more in dry mass.
Abstract:
Provided is a laminate having at least a base material and a fine cellulose layer which includes fine cellulose having a carboxyl group, the laminate characterized in being obtained by laminating two or more of the fine cellulose layer. Also provided is a method for manufacturing a laminate, comprising the steps of (1) coating the base material with a liquid dispersion that includes fine cellulose having a carboxyl group, (2) forming a fine cellulose layer by drying the liquid dispersion used for coating, and (3) laminating fine cellulose layers by repeating steps (1) and (2).
Abstract:
A method for preparing a cellulose dispersion includes oxidizing cellulose; preparing cellulose nanofibers by defibrating the oxidized cellulose; and adding a water-soluble polymer and inorganic particles to the dispersion containing the cellulose nanofibers.
Abstract:
A paper cup includes barrier paper, the barrier paper including at least a paper base material, a reinforcing layer containing cellulose nanofibers which is formed on the paper base material, and a sealant layer formed on the reinforcing layer, in which after the paper cup is caused to free-fall 5 times towards a concrete floor surface from a height of 1 m with the bottom portion being disposed downward, the paper cup has a buckling strength of 350 N or more in a case of being sandwiched between two parallel plate surfaces and compressed in a height direction of the body portion, and has a lateral pressing strength of 4 N or more in a case where the body portion is pressed by 10 mm at a ⅔ height, from a bottom, of the entire height of the paper cup.