摘要:
Provided is a method for the simple and highly accurate assay of PSA by a one-step reaction that does not use carriers having different average grain sizes. Also provided is a reagent therefor. The PSA assay method comprises sensitizing insoluble carriers having the same average grain size within a range of greater than 0.20 μm but 0.40 μm or less using two types of anti-PSA monoclonal antibodies having different epitopes that are anti-PSA monoclonal antibodies that will react with both free PSA and PSA-ACT, which is a complex of free PSA and α1-antichymotrypsin, and bringing the carriers into contact with a sample in the presence of an aggregation promoter.
摘要:
Toner contains a binder resin containing a crystalline resin having a urethane and/or urea bonding; and a colorant, wherein in a diffraction spectrum of the toner as measured by an X-ray diffraction instrument, a ratio {C/(C+A)} of an integral intensity C of the spectrum derived from the crystalline structure to an integral intensity A of the spectrum derived from the non-crystalline structure is 0.12 or greater, wherein the toner satisfies the following relation 1: T1−T2≦30° C. (Relation 1), where T1 represents the maximum endothermic peak in the first temperature rising from 0° C. to 100° C. at the temperature rising rate of 10° C./min and T2 represents the maximum exothermic peak in the first temperature falling from 100° C. to 0° C. at the temperature falling rate of 10° C./min as T1 and T2 are measured by diffraction scanning calorimetry (DSC).
摘要:
Provided is a toner that comprises a binder resin, a releasing agent, and a colorant, wherein the mass average particle diameter of the toner is 3 μm to 8 μm, the content of particles having a particle diameter of no more than 5 μm is from 60% by number to 90% by number, the binder resin comprises a polyester resin (A) having a softening temperature Tm(A) from no lower than 120° C. to no higher than 160° C. and a polyester resin (B) having a softening temperature Tm(B) from no lower than 80° C. to lower than 120° C., and at least one of the polyester resins (A) and (B) is prepared by condensation polymerization between an alcohol component and a carboxylic acid component, and the alcohol component comprises divalent alcohol of 1,2-propanediol in a content of no less than 65% by mole and consists substantially of aliphatic alcohol; and also provided is a developer that comprises the toner and a carrier.
摘要:
A toner including a binder resin; and a colorant, wherein a hexafluoroisopropanol (HFIP)-soluble component satisfies the following relationship: 2,000 ≦Mn ≦7,000 and 1.5 ≦Mn/Mw ≦10 wherein Mn represents a number-average molecular weight and Mw represents a weight-average molecular weight.
摘要:
An external additive for a toner for electrophotography which contains oxide fine particles which contain silicon, in which the oxide fine particles have a primary particle diameter of 30 nm to 300 nm in number average, a standard deviation σ of a particle size distribution of the primary particle diameter satisfies a relation of: R/4≦σ≦R, in which the R expresses the primary particle diameter,the oxide fine particles are substantially spherical having a circularity SF1 defined as equation (1) of 100 to 130 and a circularity SF2 defined as equation (2) of 100 to 125; SF1=(L2/A)×(π/4)×100 equation (1) SF2=(P2/A)×(1/4π)×100 equation (2), in the equations, “L” expresses the absolute maximum length of the oxide fine particles; “A” expresses a projected area of the oxide fine particles; and “P” expresses a maximum perimeter of the oxide fine particles.
摘要:
A toner which is negatively charged to develop an electrostatic latent image is provided that contains a colorant; and a binder resin, wherein the toner has an acid value of from 5 to 20 mg KOH/g and an amine value of from 0.5 to 10 mg KOH/g.
摘要:
It is an object of the present invention to provide a toner that can sustain favorable transferability and cleaning ability for prolonged periods; prevent photoconductor filming; exhibit no variation in image nonuniformity or external additive immersion induced by developer agitation at the time of use; excels in stability with flowability and charge stability over prolonged periods. Therefore, provided is the toner of which the quantity of aggregate of residual external additives found on the sieve of 635-mesh and 452 cm2 of mesh area, after 0.2 g of the toner on the sieve is blasted with air at a blow pressure of 0.2 MPa from 160 mm above the sieve while being air-suctioned at a suction force of 5 mmHg, and then air-suctioned at a suction force of 20 mmHg, is 4,500 or less and 5 or more.
摘要:
A toner containing toner particles having a core-shell structure containing a binder resin, a colorant and a release agent. The toner particles are prepared by dissolving or dispersing at least one of the binder resin and a precursor thereof in an organic solvent or a polymeric monomer and reacting the resultant in an aqueous medium for reaction, wherein the toner satisfies the following relationship: ΔTm=Tm1−Tm2>10 ° C., wherein Tm1 represents half efflux temperature of the toner and Tm2 represents half efflux temperature of a toner which is prepared by melting and kneading the toner particles and wherein a content of the release agent existing close to the surface portion of the toner particles is from 7 to 30% by volume based on an entire portion close to the surface portion of the toner particles when the content is determined by Fourier Transform Infrared Spectroscopy Attenuated Total Reflection (FTIR-ATR) method.
摘要:
A toner for developing an electrostatic image, includes: a colorant; and a binder resin. The toner has a particle including at least one pore having a diameter of 10 nm or over, and a porosity thereof is in a range from 0.01 to 0.60.