HETEROPHASIC POLYPROPYLENE WITH PROPYLENE HEXENE RANDOM COPOLYMER AS MATRIX

    公开(公告)号:US20210246290A1

    公开(公告)日:2021-08-12

    申请号:US17049799

    申请日:2019-05-07

    Applicant: BOREALIS AG

    Abstract: The present invention is directed to a heterophasic polypropylene composition of high transparency based on excellent compatibility of the propylene 1-hexene random copolymer used as matrix with different types of external modifiers dispersed within the matrix. The present invention is further directed to a process for producing such a polypropylene composition and to a film, in particular a cast film, obtained from such a polypropylene composition. The polypropylene composition comprising a blend of a propylene copolymer comprising 2.5 to 12.0 wt % of 1-hexene as a comonomer, and having a melt flow rate MFR2 of 0.1 to 100 g/10 min, and an ethylene homo- or copolymer having a melt flow rate MFR2 of 0.05 to 30.0 g/10 min and a density of 850 to 920 kg/m3, wherein the melt flow rate MFR2 of the polypropylene composition is from 1.0 to 12.0 g/10 min.

    Heterophasic polypropylene composition

    公开(公告)号:US11084920B2

    公开(公告)日:2021-08-10

    申请号:US16769510

    申请日:2018-12-18

    Applicant: BOREALIS AG

    Abstract: The invention relates to a new soft heterophasic propylene copolymer with increased melting temperature, improved stiffness and optical properties, as well as the process by which the heterophasic propylene copolymer is produced. Further the present invention is directed to articles made of the inventive heterophasic propylene copolymer, particularly to blow moulded, extrusion blow moulded or injection moulded articles and their use in e.g. medical, pharmaceutical or alimentary applications.

    POLYPROPYLENE PIPE COMPOSITION
    135.
    发明申请

    公开(公告)号:US20210108058A1

    公开(公告)日:2021-04-15

    申请号:US17050048

    申请日:2019-05-07

    Applicant: BOREALIS AG

    Abstract: Polypropylene composition having a melting temperature Tm of 135° C. to 140° C. (DSC according to ISO 11357/part 3), —an MFR2 of 0.05 to 0.50 g/10 min (2.16 kg, 230° C., IS01133), a XS according to IS016152 of 0.2 to 2.5 wt.-%, and a molecular weight distribution Mw/Mn of at least 2.8 and less than 6.0, wherein Mn is the number average molecular weight and Mw is the weight average molecular weight both being determined by Gel Permeation Chromatography (GPC) according to ISO 16014-4:2003, and ASTM D 6474-99, whereby the polypropylene composition comprises units derived from 1-hexene in an amount of 1.80 wt.-% to 5.0 wt.-%.