摘要:
A method of cooling syngas in a gasifier is provided. The method includes channeling cooling fluid through at least one tube-bundle that includes at least three tubes coupled together within a radiant syngas cooler and extends through a reaction zone of the gasifier, and circulating reactant fluid around the at least one tube-bundle to facilitate transferring heat from the reactant fluid to the cooling fluid.
摘要:
Improved methods and containers for forming billets using hot isostatic pressing are provided. The methods and containers have features that control the deformations of the container during the high temperatures and pressures experienced in such processing so that the loss or removal of material from the resulting billet can be optimized.
摘要:
Components and methods of processing such components from precipitation-strengthened alloys so that the components exhibit desirable grain sizes following a supersolvus heat treatment. The method includes consolidating a powder of the alloy to form a billet having an average grain size. The billet is then forged at a temperature below the solvus temperature to form a forging having an average grain size of not coarser than the grain size of the billet. The billet is then forged at a total strain of at least 5%, after which at least a portion of the forging is heat treated at a temperature below the solvus temperature to pin grains within the portion. The entire forging can then be heat treated at a temperature above the solvus temperature of the alloy without coarsening the grains in the portion.
摘要:
According to various embodiments, a system includes a gasifier that includes a shell made of a first material exposed to a gasification region inside the gasifier and a patterned anode layer coupled to the shell inside the gasifier. The patterned anode layer is made of a second material, and the patterned anode layer is configured to protect the shell from corrosion by condensing hot gas in the gasification region.
摘要:
A casting process for producing metal alloy castings, facecoats and apparatuses suitable for carrying out the process, and castings produced by the process. The casting process entails the use of a mold having a cavity with a continuous aluminum-containing solid facecoat on its surface. A molten quantity of a metal alloy is introduced into the mold cavity so that the molten alloy contacts the solid facecoat. The mold is then allowed to cool to solidify the molten alloy and form a cast product. During the casting process, aluminum in the solid facecoat diffuses into the cast product to form an aluminum-containing surface region at the casting surface. Following removal of the cast product from the mold, an alumina-containing scale grows on the casting surface as a result of oxidation of the casting surface region.
摘要:
A system and method for online monitoring of corrosion of a pressure vessel is disclosed. First and second electrodes may be isolated from each other in a wall of the pressure vessel and exposed to a corrosive environment within the pressure vessel. Additionally, the first and second electrodes may be electrically coupled such that, when an electrical potential difference exists between the electrodes, an electrical current flows between the first electrode and the second electrode. The electrical potential difference and/or the electrical current flowing between the electrodes may then be measured and analyzed to determine when to perform a corrective action on the pressure vessel.
摘要:
An improved container and method for forming billets using hot isostatic pressing is provided. The method and container allows for adjusting the volume of the container so as to obtain a billet of the desired shape based on selected powder charge for the container. In addition, the corner of the container can be adjusted to allow for elimination of edge effects and further shape control in the resulting billet.
摘要:
A cast nickel-iron-base alloy component having by weight about 12.0% to about 16.5% Cr, about 1.0% to about 2.0% Al, about 2.0% to about 3.0% Ti, about 2.0% to about 3.0% W, about 3.0 to about 5.0% Mo, up to about 0.1% Nb, up to about 0.2% Mn, up to about 0.1% Si, about 0.05% to about 0.10% C, about 0.003 to about 0.010% B, about 35% to about 37% Fe, and balance essentially Ni and inevitable impurities. The nickel-iron-base alloy component has a creep rupture life greater than about 1000 hours at about 25 ksi to about 30 ksi at about 1400° F. A method for forming the cast nickel-iron-base alloy component is also disclosed.
摘要:
An improved container and method for forming billets using hot isostatic pressing is provided. The method and container allows for adjusting the volume of the container so as to obtain a billet of the desired shape based on selected powder charge for the container. In addition, the corner of the container can be adjusted to allow for elimination of edge effects and further shape control in the resulting billet.
摘要:
Disclosed is a turbine, a turbine seal structure, and a process of servicing a turbine. The turbine includes the seal structure. The seal structure is mechanically secured within the hot gas path of the turbine. The process of servicing includes positioning the seal structure within the hot gas path of the turbine and mechanically securing the seal structure within the turbine.