公开(公告)号:US20220106474A1
公开(公告)日:2022-04-07
申请号:US17421855
申请日:2020-01-07
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: MONICA GALVAN , MICHELE GRAZZI , MARCO CIARAFONI , CLAUDIO CAVALIERI
IPC: C08L23/16
Abstract: A polyolefin composition made from or containing: A) 5-35% by weight of a propylene homopolymer; B) 20-50% by weight of an ethylene homopolymer; and C) 30-60% by weight of a terpolymer of ethylene, propylene and 1-butene derived units.
-
公开(公告)号:US20190055333A1
公开(公告)日:2019-02-21
申请号:US15768875
申请日:2016-10-22
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: PAOLA MASSARI , CAROLINE CATHELIN , GIAMPIERO MORINI , FABRIZIO PIEMONTESI , GIANNI VITALE , MARCO CIARAFONI , CLAUDIO CAVALIERI , ROBERTO PANTALEONI , MICHELE GRAZZI
Abstract: A polypropylene composition made from or containing: A) from 50 wt % to 90 wt %; of a propylene homopolymer; B) from 10 wt % to 50 wt %; of a copolymer of propylene having from 30.0 wt % to 70.0 wt %, of ethylene derived units, based upon the total weight of the copolymer; the sum of the amount of component A) and B) being 100; the polypropylene composition having: i) an intrinsic viscosity of the fraction soluble in xylene at 25° C. between 2.2 to 4.0 dl/g; ii) a MFR L (Melt Flow Rate according to ISO 1133, condition L, at 230° C. and 2.16 kg load) from 0.5 to 100 g/10 min; iii) a xylene soluble fraction ranging from 20 wt % to 50 wt %, based upon the total weight of the polypropylene composition; wherein the polypropylene composition being obtained by a polymerization process wherein the catalyst system contains bismuth.
-
公开(公告)号:US20170183485A1
公开(公告)日:2017-06-29
申请号:US15313482
申请日:2015-04-28
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: CLAUDIO CAVALIERI , MICHELE GRAZZI , ROBERTO PANTALEONI
IPC: C08L23/06 , C08L23/08 , C08F210/02
CPC classification number: C08L23/06 , C08F210/02 , C08L23/08 , C08L2205/025 , C08L2207/02 , C08L23/16
Abstract: Ethylene polymer composition having a fusion enthalpy ΔHfus, measured by Differential Scanning calorimetry with a heating rate of 20° C. per minute, of 60 J/g or more, comprising, all per cent amounts being by weight: A) 25-55% of an ethylene polymer containing 10% or less, referred to the weight of A), of a fraction XSA soluble in xylene at 25° C.; B) 45-75% of a copolymer of ethylene and propylene containing from 45% to 70%, of ethylene and 60% or more of a fraction XSB soluble in xylene at 25° C., both the ethylene of the copolymer and XSB amounts being referred to the weight of B); wherein the amounts of A) and B) are referred to the total weight of A)+B).
-
-