Abstract:
Polyolefin compositions made from or containing:(A) about 5 to about 35% by weight of a propylene-based polymer containing about 90% by weight or more of propylene units and containing about 10% by weight or less of a fraction soluble in xylene at 25° C. (XSA); (B) about 25 to about 50% by weight, of a copolymer of ethylene and a C3-C8 alpha-olefin containing from about 0.1% to about 15% by weight of alpha-olefin units and containing about 75% by weight or less of a fraction soluble in xylene at 25° C. (XSB); and (C) about 30 to about 60% by weight, of a copolymer of ethylene and propylene containing from about 45% to about 75% by weight of ethylene units and containing from about 55% to about 95% by weight, of a fraction soluble in xylene at 25° C. (XSC).
Abstract:
Multilayer film (BOPP) structure comprising at least: A) a skin (outer) layer substantially consisting of a crystalline low seal Initiation temperature propylene copolymer; B) a tie layer substantially consisting of a butene-1 copolymer having flexural modulus (MEF) of 75 MPa or less; C) a core layer substantially consisting of one or more polypropylene homopolymers designed for BOPP.
Abstract:
A polyolefin composition made from or containing: A) 5-35% by weight of a propylene ethylene copolymer; B) 20-50% by weight of an ethylene homopolymer; and C) 30-60% by weight of a terpolymer of ethylene, propylene and 1-butene derived units.
Abstract:
A polypropylene composition made from or containing: A) from 50 wt % to 90 wt %, based upon the total weight of the polypropylene composition, of a propylene homopolymer; and B) from 10 wt % to 50 wt %, based upon the total weight of the polypropylene composition, of a copolymer of propylene and ethylene having from 30.0 wt % to 70.0 wt %, based upon the total weight of the copolymer, of ethylene derived units; the polypropylene composition having: i) an intrinsic viscosity of the fraction soluble in xylene at 25° C. between 2.2 and 4.0 dl/g; ii) a MFR L from 0.5 to 100 g/10 min; and iii) a xylene soluble fraction ranging from 10 wt % to 50 wt %, based upon the total weight of the polypropylene composition.
Abstract:
A multilayer film made from or containing at least one core layer made from or containing a polypropylene composition made from or containing: A) from 95 wt % to 60 wt %; of a propylene homopolymer having a fraction insoluble in xylene at 25° C. greater than 90 wt %, based upon the total weight of the propylene homopolymer; and B) from 5 wt % to 40 wt %; of an heterophasic propylene ethylene copolymer, the sum of the amounts of A) and B) being 100.
Abstract:
Composition comprising (A) from 30 to 60 by weight, of a soft polyolefin composition comprising, 10-50% by weight of a copolymer (a) of propylene, which copolymer contains from 1 to 8% of comonomer content; 50-90wt % of a copolymer (b) of ethylene and other alpha-olefin(s), containing from 57 to 80% of ethylene; wherein the weight ratio of the content of copolymer component (b) to the fraction XS soluble in xylene at room temperature (about 25° C.), both (b and XS) referred to the total weight of (a)+(b), is of 1.5 or less, and the intrinsic viscosity [η] of the said XS fraction is of 3 dl/g or more; and the total quantity of copolymerized ethylene is preferably from 30% to 65% by weight; (B) from 5 to 30 wt % of a glass fiber filler; (C) from 0 to 5% by weight of a compatibilizer; (D) from 10 to 40 by weight of a polypropylene component selected from propylene homopolymers, propylene copolymers containing up to 5% by moles of ethylene and/or C4-C10 α-olefin(s) and combinations of such homopolymers and copolymers, wherein the Melt Flow Rate, of the polypropylene component D) is generally from 0.3 to 2500 g/10 min.
Abstract:
A propylene 1-hexene copolymer containing from about 5.5 to about 9.0% by weight, based upon the total weight of the copolymer, of 1-hexene derived units having: a) two melting temperature peaks in the DSC plot having a difference in height ranging from 0 to 5 mW; b) the higher melting temperature, measured by DSC, ranging from about 141.0° C. to about 151.0° C.; and c) Melt Flow Rate (MFR, measured according to ASTM D 1238, 230° C./2.16 kg) from about 3.5 to about 8.0 g/10 min.
Abstract:
Polyolefin composition made from or containing:(A) about 5 to about 35% by weight of a propylene-based polymer containing about 90% by weight or more of propylene units and containing about 10% by weight or less of a fraction soluble in xylene at 25° C. (XSA); (B) about 25 to about 50% by weight, of an ethylene homopolymer containing about 5% by weight or less of a fraction soluble in xylene at 25° C. (XSB) referred to the weight of (B); and (C) about 30 to about 60% by weight, of a copolymer of ethylene and propylene containing from about 25% to about 75% by weight of ethylene units and containing from about 55% to about 95% by weight, of a fraction soluble in xylene at 25° C. (XSC). Following progressive fractionation having first, second, and third dissolution temperatures, the composition has about 20% by weight or less collected at second dissolution temperature.
Abstract:
The present disclosure relates to highly filled polyolefin compositions with improved balance of properties particularly for applications where puncture and tear resistance is requested comprising a flexible heterophasic polyolefin composition (I), consisting of a crystalline polymer fraction (A) consisting of a copolymer of propylene with ethylene having a fraction insoluble in xylene at 25° C. of at least 90% by weight, and an elastomeric fraction (B) consisting of a copolymer or blend of copolymers of ethylene with propylene; the copolymer or blend containing units derived from ethylene in a quantity lower than 40% by weight. The fraction soluble in xylene at 25° C. of the polyolefin composition having an IVgpc lower than 2.5 dl/g, a broad molecular weight distribution Mw/Mn (GPC) equal to or higher than 4, and a Mz/Mw (GPC) equal to or higher than 2.5. The filled polyolefin composition further comprises inorganic filler (II) and a butene-1 copolymer having: a flexural modulus (ISO 178) lower than 60 MPa, a Shore A (ISO 868) lower than 90 and a Tg (DMTA) lower than −20° C.
Abstract:
An injection molded article made from or containing a propylene-based composition made from or containing: T1) from 90 wt % to 50 wt % of a propylene homopolymer; and T2) from 10 wt % to 50 wt % of a polymer composition made from or containing A) 5-35% by weight of a propylene homopolymer or a propylene ethylene copolymer; B) 20-50% by weight of a copolymer of ethylene and a C3-C8 alpha-olefin containing from 0.1% to 20% by weight of alpha-olefin units; and C) 30-60% by weight of a copolymer of ethylene and propylene containing from 25% to 75% by weight of ethylene units.