METHOD FOR PREPARING LITHIUM IRON PHOSPHATE NANOPOWDER
    11.
    发明申请
    METHOD FOR PREPARING LITHIUM IRON PHOSPHATE NANOPOWDER 审中-公开
    制备磷酸铁锂纳米粒子的方法

    公开(公告)号:US20150024266A1

    公开(公告)日:2015-01-22

    申请号:US14510495

    申请日:2014-10-09

    Applicant: LG Chem, Ltd.

    Abstract: The present invention relates to a method for preparing a lithium iron phosphate nanopowder, including the steps of (a) preparing a mixture solution by adding a lithium precursor, an iron precursor and a phosphorus precursor in a glycerol solvent, and (b) putting the mixture solution into a reactor and heating to prepare the lithium iron phosphate nanopowder under pressure conditions of 10 bar to 100 bar, and a lithium iron phosphate nanopowder prepared by the method. When compared to a common hydrothermal synthesis method and a supercritical hydrothermal synthesis method, a reaction may be performed under a relatively lower pressure. When compared to a common glycothermal synthesis method, a lithium iron phosphate nanopowder having effectively controlled particle size and particle size distribution may be easily prepared.

    Abstract translation: 本发明涉及一种制备磷酸铁锂纳米粉末的方法,包括以下步骤:(a)通过在甘油溶剂中加入锂前体,铁前体和磷前体制备混合溶液,和(b)将 混合溶液加入到反应器中并加热以在10巴至100巴的压力条件下制备磷酸铁锂纳米粉末,并通过该方法制备磷酸铁锂纳米粉末。 当与常用的水热合成法和超临界水热合成法相比时,可以在相对较低的压力下进行反应。 当与普通的糖热合成方法相比时,可以容易地制备具有有效控制粒度和粒度分布的磷酸铁锂纳米粉末。

    METHOD FOR PREPARING LITHIUM IRON PHOSPHATE NANOPOWDER COATED WITH CARBON
    12.
    发明申请
    METHOD FOR PREPARING LITHIUM IRON PHOSPHATE NANOPOWDER COATED WITH CARBON 审中-公开
    用碳酸钙制备磷酸铁锂纳米粒子的方法

    公开(公告)号:US20150236347A1

    公开(公告)日:2015-08-20

    申请号:US14421633

    申请日:2014-01-09

    Applicant: LG Chem, Ltd.

    Abstract: The present invention relates to a method for preparing a lithium iron phosphate nanopowder coated with carbon, including the steps of (a) preparing a mixture solution by adding a lithium precursor, an iron precursor and a phosphorus precursor in a glycol-based solvent, (b) putting the mixture solution into a reactor, heating and concentrating to prepare a metal glycolate slurry, (c) drying the metal glycolate slurry to form a solid content, and (d) firing the solid content to prepare the lithium iron phosphate nanopowder coated with carbon, and a lithium iron phosphate nanopowder coated with carbon prepared by the method.

    Abstract translation: 本发明涉及一种制备涂覆有碳的磷酸铁锂纳米粉末的方法,包括以下步骤:(a)通过在二醇系溶剂中加入锂前体,铁前体和磷前体制备混合溶液( b)将混合溶液放入反应器中,加热并浓缩以制备金属乙醇酸盐浆料,(c)干燥金属乙醇酸盐浆料以形成固体含量,和(d)焙烧固体含量以制备涂覆有磷酸铁锂的纳米粉末 用碳和通过该方法制备的涂覆有碳的磷酸铁锂纳米粉末。

    METHOD FOR PREPARING LITHIUM IRON PHOSPHATE NANOPOWDER COATED WITH CARBON
    13.
    发明申请
    METHOD FOR PREPARING LITHIUM IRON PHOSPHATE NANOPOWDER COATED WITH CARBON 有权
    用碳酸钙制备磷酸铁锂纳米粒子的方法

    公开(公告)号:US20150037666A1

    公开(公告)日:2015-02-05

    申请号:US14516810

    申请日:2014-10-17

    Applicant: LG Chem, Ltd.

    Abstract: The present invention relates to a method for preparing a lithium iron phosphate nanopowder coated with carbon, including the steps of (a) preparing a mixture solution by adding a lithium precursor, an iron precursor and a phosphorus precursor in a triethanolamine solvent, (b) putting the mixture solution into a reactor and reacting to prepare amorphous lithium iron phosphate nanoseed particle, and (c) heat treating the lithium iron phosphate nanoseed particle thus to prepare the lithium iron phosphate nanopowder coated with carbon on a portion or a whole of a surface of a particle, and a lithium iron phosphate nanopowder coated with carbon prepared by the above method. The lithium iron phosphate nanopowder coated with carbon having controlled particle size and particle size distribution may be prepared in a short time by performing two simple steps.

    Abstract translation: 本发明涉及一种涂覆有碳的磷酸铁锂纳米粉末的制备方法,包括以下步骤:(a)通过在三乙醇胺溶剂中加入锂前体,铁前体和磷前体制备混合溶液,(b) 将混合溶液放入反应器中并反应制备无定形磷酸铁锂纳米颗粒,和(c)热处理磷酸铁锂纳米颗粒,从而制备在表面的一部分或全部涂覆有碳的磷酸铁锂纳米粉末 的颗粒,和通过上述方法制备的涂覆有碳的磷酸铁锂纳米粉末。 通过执行两个简单的步骤,可以在短时间内制备涂覆有具有受控粒度和粒度分布的碳的磷酸铁锂纳米粉末。

    METHOD FOR PREPARING LITHIUM IRON PHOSPHATE NANOPOWDER
    14.
    发明申请
    METHOD FOR PREPARING LITHIUM IRON PHOSPHATE NANOPOWDER 有权
    制备磷酸铁锂纳米粒子的方法

    公开(公告)号:US20150030918A1

    公开(公告)日:2015-01-29

    申请号:US14510370

    申请日:2014-10-09

    Applicant: LG Chem, Ltd.

    Abstract: The present invention relates to a method for preparing a lithium iron phosphate nanopowder, including the steps of (a) preparing a mixture solution by adding a lithium precursor, an iron precursor and a phosphorus precursor in a glycerol solvent, and (b) putting the mixture solution into a reactor and heating to prepare the lithium iron phosphate nanopowder under pressure conditions of 1 bar to 10 bar, and a lithium iron phosphate nanopowder prepared by the method. When compared to a common hydrothermal synthesis method, a supercritical hydrothermal synthesis method and a glycothermal synthesis method, a reaction may be performed under a relatively lower pressure. Thus, a high temperature/high pressure reactor is not necessary and process safety and economic feasibility may be secured. In addition, a lithium iron phosphate nanopowder having uniform particle size and effectively controlled particle size distribution may be easily prepared.

    Abstract translation: 本发明涉及一种制备磷酸铁锂纳米粉末的方法,包括以下步骤:(a)通过在甘油溶剂中加入锂前体,铁前体和磷前体制备混合溶液,和(b)将 混合溶液加入到反应器中并加热以在1巴至10巴的压力条件下制备磷酸铁锂纳米粉末,并通过该方法制备磷酸铁锂纳米粉末。 当与通常的水热合成法,超临界水热合成法和糖热合成法相比时,可以在相对较低的压力下进行反应。 因此,不需要高温/高压反应器,并且可以确保工艺安全性和经济可行性。 此外,可以容易地制备具有均匀粒度和有效控制粒度分布的磷酸铁锂纳米粉末。

    METHOD FOR PREPARING LITHIUM IRON PHOSPHATE NANOPOWDER
    15.
    发明申请
    METHOD FOR PREPARING LITHIUM IRON PHOSPHATE NANOPOWDER 有权
    制备磷酸铁锂纳米粒子的方法

    公开(公告)号:US20150024271A1

    公开(公告)日:2015-01-22

    申请号:US14510472

    申请日:2014-10-09

    Applicant: LG CHEM, LTD.

    Abstract: The present invention relates to a method for preparing a lithium iron phosphate nanopowder, including the steps of (a) preparing a mixture solution by adding a lithium precursor, an iron precursor and a phosphorus precursor in a triethanolamine solvent, and (b) putting the mixture solution into a reactor and heating to prepare the lithium iron phosphate nanopowder under pressure conditions of 10 bar to 100 bar, and a lithium iron phosphate nanopowder prepared by the method. When compared to a common hydrothermal synthesis method and a supercritical hydrothermal synthesis method, a reaction may be performed under a relatively lower pressure. When compared to a common glycothermal synthesis method, a lithium iron phosphate nanopowder having effectively controlled particle size and particle size distribution may be easily prepared.

    Abstract translation: 本发明涉及一种制备磷酸铁锂纳米粉末的方法,包括以下步骤:(a)通过在三乙醇胺溶剂中加入锂前体,铁前体和磷前体制备混合溶液,和(b)将 混合溶液加入到反应器中并加热以在10巴至100巴的压力条件下制备磷酸铁锂纳米粉末,并通过该方法制备磷酸铁锂纳米粉末。 当与常用的水热合成法和超临界水热合成法相比时,可以在相对较低的压力下进行反应。 当与普通的糖热合成方法相比时,可以容易地制备具有有效控制粒度和粒度分布的磷酸铁锂纳米粉末。

    METHOD FOR PREPARING LITHIUM IRON PHOSPHATE NANOPOWDER
    16.
    发明申请
    METHOD FOR PREPARING LITHIUM IRON PHOSPHATE NANOPOWDER 有权
    制备磷酸铁锂纳米粒子的方法

    公开(公告)号:US20150024265A1

    公开(公告)日:2015-01-22

    申请号:US14510356

    申请日:2014-10-09

    Applicant: LG Chem, Ltd.

    Abstract: The present invention relates to a method for preparing a lithium iron phosphate nanopowder, including the steps of (a) preparing a mixture solution by adding a lithium precursor, an iron precursor and a phosphorus precursor in a triethanolamine solvent, and (b) putting the mixture solution into a reactor and heating to prepare the lithium iron phosphate nanopowder under pressure conditions of 1 bar to 10 bar, and a lithium iron phosphate nanopowder prepared by the method. When compared to a common hydrothermal synthesis method, a supercritical hydrothermal synthesis method and a glycothermal synthesis method, a reaction may be performed under a relatively lower pressure. Thus, a high temperature/high pressure reactor is not necessary and process safety and economic feasibility may be secured. In addition, a lithium iron phosphate nanopowder having uniform particle size and effectively controlled particle size distribution may be easily prepared.

    Abstract translation: 本发明涉及一种制备磷酸铁锂纳米粉末的方法,包括以下步骤:(a)通过在三乙醇胺溶剂中加入锂前体,铁前体和磷前体制备混合溶液,和(b)将 混合溶液加入到反应器中并加热以在1巴至10巴的压力条件下制备磷酸铁锂纳米粉末,并通过该方法制备磷酸铁锂纳米粉末。 当与通常的水热合成法,超临界水热合成法和糖热合成法相比时,可以在相对较低的压力下进行反应。 因此,不需要高温/高压反应器,并且可以确保工艺安全性和经济可行性。 此外,可以容易地制备具有均匀粒度和有效控制粒度分布的磷酸铁锂纳米粉末。

    Method for preparing lithium iron phosphate nanopowder
    20.
    发明授权
    Method for preparing lithium iron phosphate nanopowder 有权
    磷酸铁锂纳米粉末的制备方法

    公开(公告)号:US09543582B2

    公开(公告)日:2017-01-10

    申请号:US14510356

    申请日:2014-10-09

    Applicant: LG Chem, Ltd.

    Abstract: The present invention relates to a method for preparing a lithium iron phosphate nanopowder, including the steps of (a) preparing a mixture solution by adding a lithium precursor, an iron precursor and a phosphorus precursor in a triethanolamine solvent, and (b) putting the mixture solution into a reactor and heating to prepare the lithium iron phosphate nanopowder under pressure conditions of 1 bar to 10 bar, and a lithium iron phosphate nanopowder prepared by the method. When compared to a common hydrothermal synthesis method, a supercritical hydrothermal synthesis method and a glycothermal synthesis method, a reaction may be performed under a relatively lower pressure. Thus, a high temperature/high pressure reactor is not necessary and process safety and economic feasibility may be secured. In addition, a lithium iron phosphate nanopowder having uniform particle size and effectively controlled particle size distribution may be easily prepared.

    Abstract translation: 本发明涉及一种制备磷酸铁锂纳米粉末的方法,包括以下步骤:(a)通过在三乙醇胺溶剂中加入锂前体,铁前体和磷前体制备混合溶液,和(b)将 混合溶液加入到反应器中并加热以在1巴至10巴的压力条件下制备磷酸铁锂纳米粉末,并通过该方法制备磷酸铁锂纳米粉末。 当与通常的水热合成法,超临界水热合成法和糖热合成法相比时,可以在相对较低的压力下进行反应。 因此,不需要高温/高压反应器,并且可以确保工艺安全性和经济可行性。 此外,可以容易地制备具有均匀粒度和有效控制粒度分布的磷酸铁锂纳米粉末。