摘要:
This invention is directed to coated water-swellable materials, typically solid, particulate, water-swellable materials, i.e. materials that comprise hydrogel-forming polymers, whereof at least a part is coated with a coating, which substantially does not break when the polymers swell, as set out in the method herein. Said coating is present at a level of at least 1% by weight of the water-swellable material.The coating comprises preferably an elastomeric polymeric material. The invention also relates products, e.g., disposable absorbent articles, comprising such coated water-swellable material.
摘要:
This invention is directed to coated water-swellable materials, typically solid, particulate, water-swellable materials, i.e. materials that comprise hydrogel-forming polymers, whereof at least a part is coated with a coating, which substantially does not break when the polymers swell, as set out in the method herein. Said coating is present at a level of at least 1% by weight of the water-swellable material.The coating comprises preferably an elastomeric polymeric material. The invention also relates products, e.g., disposable absorbent articles, comprising such coated water-swellable material.
摘要:
The present invention relates to an absorbent structure suitable in, or being an adult or infant diaper or feminine hygiene article, comprising a water-absorbing material comprising water-absorbing particles that comprise a film coating, comprising an elastic film-forming polymer and a coalescing agent.The invention also relates to an absorbent structure comprising a water absorbent material obtainable by a process of: a) spray-coating water-absorbing polymeric particles with an elastic film-forming polymer in a fluidized bed reactor at a temperature in the range from 0° C. to 150° C. and b) heat-treatment of the coated polymeric particles at a temperature above 50° C., wherein in step a) and/or b) a coalescing agent is added.
摘要:
An absorbent structure formed from a process of providing water-swellable material that includes water-swellable polymer particles, which are coated with a coating agent. The coating agent is a phase-separating elastomeric material that has a first and second glass transition temperature. The coated water-swellable polymer particles are able to swell without breakage of the coating.
摘要:
An absorbent structure formed from a process of providing water-swellable material that includes water-swellable polymer particles, which are coated with a coating agent. The coating agent is a phase-separating elastomeric material that has a first and second glass transition temperature. The coated water-swellable polymer particles are able to swell without breakage of the coating.
摘要:
This invention relates to a water-swellable material comprising water-swellable polymers that are coated with a coating agent that comprises a phase-separating elastomeric material, which allows swelling of the water-swellable polymers, without breakage of the coating. The invention also relates to a process of making specific coated water-swellable polymers using a phase-separating elastomeric material, and materials obtainable by such a process.
摘要:
The present invention relates to a water-absorbing material obtainable by a process comprising the steps of a) spray-coating water-absorbing polymeric particles with an elastic film-forming polymer in a fluidized bed reactor in the range from 00 C. to 500 C and b) heat-treating the coated particles at a temperature above 500 C. and also to a process for its production.
摘要:
The present invention relates to a process for producing a water-absorbing material comprising the steps of a) spray-coating water-absorbing polymeric particles with an elastic film-forming polymer in a fluidized bed reactor in the range from 00 C to 1500 C and b) heat-treatment of the coated particles at a temperature above 50° C., wherein in step b) the duration of the heat-treatment is chosen that the CS-SFC value of the obtained polymeric particles is at least 10% of the optimum CS-SFC value, and the water-absorbing material obtainable by this process.
摘要:
The present invention relates to an absorbent structure suitable in, or being an adult or infant diaper or feminine hygiene article, comprising a water-absorbing material comprising water-absorbing particles that comprise a film coating, comprising an elastic film-forming polymer and an antioxidant.The invention also relates to an absorbent structure comprising a water absorbent material obtainable by a process of: a) spray-coating water-absorbing polymeric particles with an elastic film-forming polymer in a fluidized bed reactor at a temperature in the range from 0° C. to 150° C. and b) heat-treatment of the coated polymeric particles at a temperature above 50° C., wherein in step a) and/or b) an antioxidant is added.
摘要:
This invention relates to an absorbent structure that comprises water-swellable material, which comprises water-swellable polymers that are coated with a coating agent said coating agent comprising a phase-separating elastomeric material, which allows swelling of the water-swellable polymers, without breakage of the coating.