摘要:
The present invention relates to a water-absorbing material obtainable by a process comprising the steps of: a) obtaining, optionally coated, post-crosslinked water-absorbing polymeric particles; b) exposing said particles of step a) to a vacuum-treatment, at a pressure of from 0.0001 mbar to 700 mbar; and c) optionally exposing said particles of step b) to a plasma-treatment, and processes for their production.
摘要:
The present disclosure relates to an absorbent structure for use in a diaper for babies and infants, a feminine hygiene article and/or an incontinence article, said absorbent structure comprising a water-absorbing material, the water-absorbing material being obtainable by a process comprising the steps of A) treating a particulate, non-surface-crosslinked, water-absorbing polymer with a mixture comprising an aqueous solvent and at least one salt of a transition metal and B) irradiating the polymer treated according to A) with UV radiation, and to a process for its production.
摘要:
The present invention relates to an absorbent structure suitable in, or being an adult or infant diaper or feminine hygiene article, comprising a water-absorbing material comprising water-absorbing particles that comprise a film coating, comprising an elastic film-forming polymer and an antioxidant.The invention also relates to an absorbent structure comprising a water absorbent material obtainable by a process of: a) spray-coating water-absorbing polymeric particles with an elastic film-forming polymer in a fluidized bed reactor at a temperature in the range from 0° C. to 150° C. and b) heat-treatment of the coated polymeric particles at a temperature above 50° C., wherein in step a) and/or b) an antioxidant is added.
摘要:
The present invention relates to a process for producing a water-absorbing material comprising the steps of a) spray-coating water-absorbing polymeric particles with an elastic film-forming polymer in a fluidized bed reactor in the range from 00 C to 15O0 C and b) heat-treatment of the coated particles at a temperature above 50° C., wherein in step a) and/or b) a coalescing agent is added and the water-absorbing material obtainable by this process.
摘要:
The present invention relates to a process for producing a water-absorbing material comprising the steps of a) spray-coating water-absorbing polymeric particles with an elastic film-forming polymer in a fluidized bed reactor in the range from 0° C. to 1500° C. and b) heat-treatment of the coated particles at a temperature above 50° C., wherein in step a) and/or b) an antioxidant is added and the water-absorbing material obtainable by this process.
摘要:
The present invention relates to an absorbent structure suitable in, or being an adult or infant diaper or feminine hygiene article, comprising a water-absorbing material comprising water-absorbing particles that comprise a film coating, comprising an elastic film-forming polymer and a coalescing agent. The invention also relates to an absorbent structure comprising a water absorbent material obtainable by a process of: a) spray-coating water-absorbing polymeric particles with an elastic film-forming polymer in a fluidized bed reactor at a temperature in the range from 0° C. to 150° C. and b) heat-treatment of the coated polymeric particles at a temperature above 50° C., wherein in step a) and/or b) a coalescing agent is added.
摘要:
Emulsifier-free antifoams are obtainable by mixing a) from 80 to 99% by weight of at least one finely divided, virtually water-insoluble, inert solid with b) from 1 to 20% by weight of at least one hydrophobic, organic compound which has an antifoam action and is solid at room temperature in the absence of a solvent in a shear gradient such that the particle size of the compounds (b) which have an antifoam action is reduced to a mean particle size of from 0.5 to 15 μm, emulsifier-free oil-in-water dispersions of mixtures of (a) and (b) are prepared by mixing the component (a) in an amount of from 80 to 99% by weight with the compounds of component (b) in an amount of from 1 to 20% by weight in the absence of emulsifiers in an extruder or kneader in a manner such that the mean particle size of the component (b) in the mixture is brought to 0.5 to 15 μm, at up to 100° C., and emulsifying the mixture in water, and the oil-in-water dispersions thus obtainable are used as antifoams and/or deaerators for aqueous, disperse or nondisperse liquids, in particular as antifoams and/or deaerators in the paper industry, in the food industry and in wastewater treatment plants.
摘要:
The present invention relates to a water absorbing material obtainable by a process comprising the steps of bringing particles of a non surface-crosslinked water-absorbing polymer in contact with a) at least one postcrosslinker, b) 10-1000 ppm, based on the non surface-crosslinked water-absorbing polymer, of at least one Nitrogen-containing water-soluble polymer of which the Nitrogen can be protonated, and c) at least one hydrophobic polymer and heat-treating the particles thus obtained at a temperature in the range from 120° C. to 300° C. and a method for the production thereof.
摘要:
A mixture of superabsorbents having differing surface postcrosslinking, more particularly a mixture of differingly surface-postcrosslinked sieve cuts of a base polymer, exhibits improved absorption and retention over a unitarily surface-postcrosslinked superabsorbent.
摘要:
The present invention relates to a water absorbing material obtainable by a process comprising the steps of bringing particles of a non surface-crosslinked water-absorbing polymer in contact with a) at least one post-crosslinker, b) 0.1-1.0 wt. % of at least one water-insoluble metal phosphate, based on the non surface-crosslinked water-absorbing polymer, and at least one further ingredient selected from c) at least one Nitrogen-containing water-soluble polymer of which the Nitrogen can be protonated, and d) at least one hydrophobic polymer and heat-treating the particles thus obtained at a temperature in the range from 120° C. to 300° C. and a method for the production thereof.