Abstract:
A process of stripping a dispersion of organic extender particles with volatile organic compounds and a method of reducing volatile organic compounds.
Abstract:
A coalescent consisting essentially of a residue from a process for forming propyleneglycol phenyl ether, the coalescent consisting essentially of 65%-75% by weight, based on the weight of the residue, dipropyleneglycol phenyl ether, 8%-10% by weight, based on the weight of the coalescent, monopropyleneglycol phenyl ether, 4%-6% by weight, based on the weight of the coalescent, tripropyleneglycol phenyl ether, and 0.1%-10% by weight, based on the weight of the coalescent, alkalinity (reported as NaOH) is provided. Also provided is a method for forming certain low-VOC, low cost, coalesced aqueous polymeric dispersions including, as copolymerized units, from 70% to 100% by weight, based on the solids weight of the aqueous polymeric dispersion, vinyl acetate monomer and an aqueous coating composition including the coalesced aqueous polymeric dispersion.
Abstract:
A new binder composition comprising, by dry weight based on the total dry weight of the binder composition, i) from 93% to 99.96% of polymer particles comprising, as polymerized units, by dry weight based on the total weight of the polymer particles, from 25% to 95% of a vinyl acetate; and from 5% to 75% of a vinyl ester of versatic acid and/or a vinyl ester of 2-ethyl hexanoic acid; and ii) from 0.04% to 7% of a low water soluble cyclodextrin.
Abstract:
A composition comprising:(a) from 20 to 60 wt % of a saccharide component comprising from two to five sugar ring units having polymerized units of at least one alkylene oxide selected from the group consisting of ethylene oxide, propylene oxide and butylene oxide bonded to oxygen atoms on said sugar rings and at least three acetoacetyl groups bonded to terminal oxygen atoms of said polymerized units of at least one alkylene oxide; and(b) from 40 to 80 wt % of a non-saccharide component comprising a polyol unit not containing a sugar ring and having a hydroxyl functionality from two to five; said polyol unit having polymerized units of at least one alkylene oxide selected from the group consisting of ethylene oxide, propylene oxide and butylene oxide bonded to hydroxyl oxygen atoms of the polyol and at least two acetoacetyl groups bonded to terminal oxygen atoms of said polymerized units of at least one alkylene oxide;wherein total polymerized units of at least one alkylene oxide comprise from 20 to 80 wt % of said multi-functional additive.
Abstract:
The present invention relates to a process comprising contacting methyl methacrylate or styrene; a C1-C10-alkyl acrylate; and a polymerizable carboxylic acid monomer with a stable aqueous dispersion of first polymer particles, under emulsion polymerization conditions, to form a stable aqueous dispersion of second polymer particles. The first polymer particles have a Tg in the range of from −30° C. to 30° C., and the monomers have a calculated Tg in the range of 50° C. to 120° C. The present invention also relates to the dispersion of second polymer particles, which is useful as a binder to improve freeze-thaw stability in a coatings formulation.
Abstract:
An aqueous dispersion of multistage polymer particles comprising at least three polymers with low minimum film formation temperature and also providing aqueous coating compositions with balanced properties.
Abstract:
The present invention relates to a benzophenone derivative and an aqueous copolymer dispersion comprising the benzophenone derivative. This invention also relates to an aqueous coating composition comprising the aqueous copolymer dispersion. The benzophenone derivative provides better crosslinking efficiency and improvement to dirt pick up resistance performance.
Abstract:
An aqueous polymer dispersion is composed of (i) an emulsion polymer having a weight average molecular weight of from 2,000 to 30,000 daltons, wherein the emulsion polymer comprises as polymerized units, based on the dry weight of the emulsion polymer, (a) from 10% to 90% by weight of an ethylenically unsaturated ionic monomer, (b) from 5% to 90% by weight of a photosensitive monomer, and (c) from 0 to 85% by weight of an ethylenically unsaturated nonionic monomer; and (ii) from 3.5% to 50% by weight of TEMPO and/or a derivative thereof, based on the total dry weight of the aqueous polymer dispersion. An aqueous coating composition comprising the aqueous polymer dispersion and a binder provides coatings with improved durability.
Abstract:
An aqueous polymer dispersion and an aqueous coating composition comprising the aqueous polymer dispersion that provides coatings with improved durability.
Abstract:
A composition comprising: (a) from 20 to 60 wt % of a saccharide component comprising from two to five sugar ring units having polymerized units of at least one alkylene oxide selected from the group consisting of ethylene oxide, propylene oxide and butylene oxide bonded to oxygen atoms on said sugar rings and at least three acetoacetyl groups bonded to terminal oxygen atoms of said polymerized units of at least one alkylene oxide; and (b) from 40 to 80 wt % of a non-saccharide component comprising a polyol unit not containing a sugar ring and having a hydroxyl functionality from two to five; said polyol unit having polymerized units of at least one alkylene oxide selected from the group consisting of ethylene oxide, propylene oxide and butylene oxide bonded to hydroxyl oxygen atoms of the polyol and at least two acetoacetyl groups bonded to terminal oxygen atoms of said polymerized units of at least one alkylene oxide; wherein total polymerized units of at least one alkylene oxide comprise from 20 to 80 wt % of said multi-functional additive.