Sealing glass and use thereof
    11.
    发明授权

    公开(公告)号:US11964909B2

    公开(公告)日:2024-04-23

    申请号:US17218592

    申请日:2021-03-31

    Applicant: SCHOTT AG

    CPC classification number: C03C8/06 C03C3/118

    Abstract: A sealing glass is provided that includes SiO2, Al2O3 having a content of less than 2% by weight, is free of PbO except for unavoidable impurities, a coefficient of linear thermal expansion (α20-300) of more than 10*10−6/K, a dielectric constant (εr) in the range from at least 7.10 to not more than 7.80 at a measurement frequency of 1 MHz and a temperature of 25° C., and a glass transition temperature (Tg) in a range from 400 to 550° C.

    HIGH-INDEX GLASS
    12.
    发明公开
    HIGH-INDEX GLASS 审中-公开

    公开(公告)号:US20240109804A1

    公开(公告)日:2024-04-04

    申请号:US18478144

    申请日:2023-09-29

    Applicant: Schott AG

    CPC classification number: C03C3/068

    Abstract: A glass having a refractive index at a wavelength of about 587.6 nm of 1.95 to 2.05 and a dispersion of 22 to less than 35 includes the following components in % by weight: 4-12 SiO2; 4-11 B2O3;

    Light guide plate for augmented reality devices

    公开(公告)号:US11906746B2

    公开(公告)日:2024-02-20

    申请号:US17956258

    申请日:2022-09-29

    Applicant: Schott AG

    CPC classification number: G02B27/0172 G02B6/0065

    Abstract: A light guide plate includes: an optical glass, the optical glass having a refractive index nd of at least 1.75 or of at least 1.80 and including Nb2O5 in an amount of at least 15 mol % and P2O5 in an amount of at least 19 mol %, the light guide plate having an internal transmission of at least 0.80 or of at least 0.90, measured at a wavelength of 440 nm and a sample thickness of 10 mm.

    OPTICAL GLASS WITH LOW DENSITY
    15.
    发明申请

    公开(公告)号:US20210340054A1

    公开(公告)日:2021-11-04

    申请号:US17307572

    申请日:2021-05-04

    Applicant: Schott AG

    Abstract: A glass has a low ratio of density ρ and refractive index nd. The glass has a refractive index nd in a range of 1.80 to 2.00, an internal transmission of at least 80% (450 nm, 10 mm), a dispersion vd of 19.0 to 27.0, and a ratio ρ/nd of

    OPTICAL GLASS HAVING NEGATIVE ANOMALOUS PARTIAL DISPERSION / SPECIAL SHORT FLINT GLASSES

    公开(公告)号:US20170137317A1

    公开(公告)日:2017-05-18

    申请号:US15355845

    申请日:2016-11-18

    Applicant: SCHOTT AG

    CPC classification number: C03C3/097

    Abstract: The present invention relates to optical glasses, in particular special short flint glasses (KZFS) and optical elements and components, which comprise these glasses, and use thereof and a method for producing such optical glasses. The optical glasses of the present invention are characterized by a pronounced short flint character and additionally by an excellent transmission and chemical resistance and workability. At that, the glasses of the invention can stand out due to lower costs of production caused by lower costs of raw materials and lower processing costs, due to their crystallization properties that can be handled also in smaller melting aggregates, and due to good environmental compatibility.

    SENSITIZED, PHOTO-SENSITIVE GLASS AND ITS PRODUCTION
    18.
    发明申请
    SENSITIZED, PHOTO-SENSITIVE GLASS AND ITS PRODUCTION 有权
    敏感的,感光玻璃及其生产

    公开(公告)号:US20160340228A1

    公开(公告)日:2016-11-24

    申请号:US15158182

    申请日:2016-05-18

    Applicant: SCHOTT AG

    Abstract: A sensitized, photo-structurable glasses and methods for producing are provided. The glasses includes Si4+, one or more crystal-agonist, one or more crystal-antagonist, and one or more pair of nucleating agents. The glasses are sensitized in that the glass reacts more sensitive to irradiation with UV-light and can be crystallized easier and with higher aspect ratios than a non-sensitized glass with equal composition. Furthermore, the sensitized glasses of this invention have smaller crystal sizes after irradiation and tempering than a non-sensitized glass with equal composition. The invention also relates to a structured glass product. Such product can be obtained by submitting the crystallized glass product to a subsequent etching step. The structured product can be used in components or as component for the application fields micro-technology, micro-reaction-technology, electronic packaging, micro-fluidics, FED spacer, bio-technology, interposer, and/or three-dimensional structured antennae.

    Abstract translation: 提供致敏的光可结晶眼镜和制造方法。 玻璃包括Si4 +,一种或多种结晶激动剂,一种或多种结晶拮抗剂和一种或多种成核剂。 玻璃被致敏,因为玻璃对UV照射的反应更敏感,并且可以比具有相同组成的非致敏玻璃更容易且具有更高的纵横比结晶。 此外,本发明的敏化玻璃在照射和回火后具有比具有相同组成的非致敏玻璃更小的晶体尺寸。 本发明还涉及一种结构化玻璃制品。 可以通过将结晶的玻璃制品提交到随后的蚀刻步骤来获得这样的产品。 结构化产品可用于微型技术,微反应技术,电子封装,微流体学,FED垫片,生物技术,插入器和/或三维结构化天线的组件或组件。

    METHOD FOR PRODUCING PHOTO-STRUCTURABLE GLASS BODIES BY A REDRAWING METHOD
    19.
    发明申请
    METHOD FOR PRODUCING PHOTO-STRUCTURABLE GLASS BODIES BY A REDRAWING METHOD 审中-公开
    通过重制方法生产可结晶玻璃体的方法

    公开(公告)号:US20160340227A1

    公开(公告)日:2016-11-24

    申请号:US15158223

    申请日:2016-05-18

    Applicant: SCHOTT AG

    Abstract: A method for production of a photo-structurable glass element is provided. The method includes the steps of: fixing a blank of photo-structurable glass at a first end; heating of a deformation zone of the blank; and drawing the blank. The glass includes Si4+, a crystal-agonist, a crystal-antagonist, and a pair of nucleating agents. The crystal-agonist is selected from the group consisting of Na+, K+, Li+, and any combinations thereof. The crystal-antagonist is selected from the group consisting of Al3+, B3+, Zn2+, Sr2+, Sb3+, and any combinations thereof. The pair of nucleating agents include cerium and an agent selected from the group consisting of silver, gold, copper, and any combinations thereof. The crystal-agonist has a molar proportion cat.-% in relation to a molar proportion of Si4+ that is at least 0.3 and at most 0.85.

    Abstract translation: 提供了一种制造可光结晶玻璃元件的方法。 该方法包括以下步骤:在第一端固定可光结晶玻璃的坯料; 加热坯料的变形区; 并绘制空白。 该玻璃包括Si4 +,晶体激动剂,晶体拮抗剂和一对成核剂。 晶体激动剂选自Na +,K +,Li +及其任何组合。 晶体拮抗剂选自Al3 +,B3 +,Zn2 +,Sr2 +,Sb3 +及其任何组合。 一对成核剂包括铈和选自银,金,铜及其任何组合的试剂。 晶体激动剂的摩尔比例相对于Si 4+的摩尔比例为至少0.3并且至多0.85,其摩尔比为。

    Highly refractive glass
    20.
    发明授权

    公开(公告)号:US11958770B2

    公开(公告)日:2024-04-16

    申请号:US17389865

    申请日:2021-07-30

    Applicant: Schott AG

    CPC classification number: C03C3/068

    Abstract: A glass includes the following components in % by weight: 2-10 wt-% SiO2, 2-10 wt-% B2O3, 40-55 wt-% La2O3, 4-11 wt-% Gd2O3, 6-14 wt-% Nb2O5, 8-18.5 wt-% TiO2, and 5-11 wt-% ZrO2. The glass has a refractive index nd of at least 2.02, a sum of the portions of La2O3, Nb2O5, TiO2 and ZrO2 is at least 76.5% by weight, and a weight ratio of a sum of the portions of La2O3, Nb2O5 and ZrO2 to the portion of TiO2 is at least 3.85:1.