Abstract:
A hermetically sealed package includes: at least one cover substrate and a substrate arranged so as to adjoin the at least one cover substrate, which together define at least part of the package, the at least one cover substrate being in a thermally prestressed state and bonded to the substrate adjoining the at least one cover substrate in a hermetically sealing manner by at least one laser bonding line, the at least one cover substrate being made of a material which has a different characteristic value of a coefficient of thermal expansion than the adjoining substrate and a thermal prestress is established in the package; and at least one functional area enclosed in the package.
Abstract:
The present disclosure relates to a method for at least section-wise separating a glass element into at least two glass sub-elements along a separation face and a glass sub-element which is manufactured and/or can be manufactured in particular by the method according to the disclosure.
Abstract:
An improved measurement method and a corresponding measurement device are provided that measure the edge strength of plate-shaped elements made of brittle-fracture material. For this purpose, a long sample is drawn apart at the short edges, wherein the force transmission points lie next to the center of gravity of the base surface of the sample.
Abstract:
A hermetically sealed enclosure is shown, comprising at least a first substrate and a second substrate, a function zone that is circumferentially enclosed in the enclosure, wherein the second substrate is transparent at least in part and/or at least for a bandwidth of wavelengths, at least one laser weld line to hermetically weld the substrates of the enclosure with each other and/or to hermetically seal the function zone, and at least one reduction zone for reducing an amount of molecules in the function zone.
Abstract:
An optical layered composite includes: a substrate having a front face, a back face, a thickness ds between the front face and the back face and a refractive index ns; and a coating applied to the front face. The coating comprises one or more coating layers. For at least one wavelength λg in the range from 390 nm to 700 nm, the coating satisfies one of the following criterion: nc ns, and
Abstract:
The present disclosure relates to a layered optical composite, in particular for use in an augmented reality device. In particular, the disclosure relates to a layered optical composite and a process for its preparation, a device comprising the layered optical composite and a process for its preparation, and the use of a layered optical composite in an augmented reality device. The present disclosure relates to a layered optical composite comprising: a. a substrate having a front face and a back face, b. a coating comprising: i. a type T layer, and ii. a type C region comprising one or more type C layers; in which the substrate has: i. a thickness tG in the range from 0.2 to 1.2 mm; ii. a refractive index nG at a wavelength λ in the range from 1.6 to 2.4; and iii. an optical absorption coefficient KG at the wavelength λ of less than 10 cm−1; in which the type C layers individually and independently have: i. a thickness tC in the range from 9 to 250 nm; ii. a refractive index nC at the wavelength λ in the range from 1.35 to 2.43; and iii. an optical absorption coefficient KC at the wavelength λ of less than 106 cm−1; in which at least one type C layer has: i. an optical absorption coefficient at the wavelength λ of at least 100 cm−1; in which the type T layer has: i. a thickness tT in the range from 50 to 300 nm; ii. a refractive index nT at the wavelength λ in the range from 1.35 to 1.96; and iii. an optical absorption coefficient KT of less than 80 cm−1; in which the type C region and the type T layer are each superimposed over one face of the substrate with the type C region further than the type T layer from the substrate; in which λ is in the range from 430 to 670 nm.
Abstract:
A glass ribbon in the form of a glass roll is provided that is optimized with respect to the requirements of a long service life and at the same time compact dimensions. A bending radius on the inner side of the thin glass roll is determined by performing breakage tests on samples of the glass material, statistical parameters are determined on the basis of the breakage tests, and the statistical parameters are converted into a range of bending radii which meet the requirements on service life and the most compact dimensions possible of the thin glass roll.
Abstract:
A method and an apparatus for examining the fracture strength of flat samples made of brittle-fracture material are provided. The margin of the respective sample is subjected to tensile stress by bending the material in a circular arc shape.
Abstract:
A method and an apparatus for examining the fracture strength of flat samples made of brittle-fracture material are provided. The margin of the respective sample is subjected to tensile stress by bending the material in a circular arc shape.
Abstract: