Provided is a piezoelectric material having a good piezoelectric property and Curie temperature (Tc) of 150° C. or higher, and a piezoelectric device using the piezoelectric material. The piezoelectric material includes a sintered body made of a perovskite-type metal oxide represented by the following general formula (1): xBi(Mg1/2Ti1/2)O3−(1−x)BaTiO3 (1), where x satisfies 0.17≦x≦0.8, in which an average grain size of grains contained in the sintered body is 0.5 μm or larger to 10 μm or smaller, and the sintered body is polycrystal. In addition, the piezoelectric device includes a piezoelectric material and a pair of electrodes disposed in contact with the piezoelectric material, in which the piezoelectric material is the above-mentioned piezoelectric material.
摘要:
Provided is a piezoelectric material having good piezoelectric properties and a Curie temperature (Tc) of 150° C. or higher, and a piezoelectric device using the piezoelectric material. The piezoelectric material includes a sintered body made of a perovskite-type metal oxide represented by the following general formula (1): xBi(Mg1/2Ti1/2)O3-(1-x)BaTiO3 (1), where x satisfies 0.17≦x≦0.8, in which an average grain size of grains contained in the sintered body is 0.5 μm or larger to 10 μm or smaller, and the sintered body is polycrystalline. In addition, the piezoelectric device includes a piezoelectric material and a pair of electrodes disposed in contact with the piezoelectric material, in which the piezoelectric material is the above-mentioned piezoelectric material.
摘要:
Provided is a piezoelectric material having good piezoelectric properties and a Curie temperature (Tc) of 150° C. or higher, and a piezoelectric device using the piezoelectric material. The piezoelectric material includes a sintered body made of a perovskite-type metal oxide represented by the following general formula (1): xBi(Mg1/2Ti1/2)O3-(1-x)BaTiO3 (1), where x satisfies 0.17≦x≦0.8, in which an average grain size of grains contained in the sintered body is 0.5 μm or larger to 10 μm or smaller, and the sintered body is polycrystalline. In addition, the piezoelectric device includes a piezoelectric material and a pair of electrodes disposed in contact with the piezoelectric material, in which the piezoelectric material is the above-mentioned piezoelectric material.
摘要:
An oxynitride piezoelectric material, which exhibits ferroelectricity and has good piezoelectric properties, and a method of producing the oxynitride piezoelectric material. The oxynitride piezoelectric material includes a tetragonal perovskite-type oxynitride represented by the following general formula (1): A1−xBix+δ1B1−yB′y+δ2O3−zNz (1), where A represents a divalent element, B and B′ each represent a tetravalent element, x represents a numerical value of 0.35 or more to 0.6 or less, y represents a numerical value of 0.35 or more to 0.6 or less, z represents a numerical value of 0.35 or more to 0.6 or less, and δ1 and δ2 each represent a numerical value of −0.2 or more to 0.2 or less, in which the A includes at least one kind selected from Ba, Sr, and Ca and the B and the B′ each include at least one kind selected from Ti, Zr, Hf, Si, Ge, and Sn.
摘要:
Provided are an oxynitride piezoelectric material which exhibits ferroelectricity and has good piezoelectric properties and a method of producing the oxynitride piezoelectric material. The oxynitride piezoelectric material includes a tetragonal perovskite-type oxynitride represented by the following general formula (1): A1-xBix+δ1B1-yB′y+δ2O3-zNz (1) where A represents a divalent element, B and B′ each represent a tetravalent element, x represents a numerical value of 0.35 or more to 0.6 or less, y represents a numerical value of 0.35 or more to 0.6 or less, z represents a numerical value of 0.35 or more to 0.6 or less, and δ1 and δ2 each represent a numerical value of −0.2 or more to 0.2 or less, in which the A includes at least one kind selected from Ba, Sr, and Ca and the B and the B′ each include at least one kind selected from Ti, Zr, Hf, Si, Ge, and Sn.
摘要:
Provided is a piezoelectric material having good piezoelectric properties and a Curie temperature (Tc) of 150° C. or higher, and a piezoelectric device using the piezoelectric material. The piezoelectric material includes a sintered body made of a perovskite-type metal oxide represented by the following general formula (1): xBi(Mg1/2Ti1/2)O3-(1-x)BaTiO3 (1), where x satisfies 0.17≦x≦0.8, in which an average grain size of grains contained in the sintered body is 0.5 μm or larger to 10 μm or smaller, and the sintered body is polycrystalline. In addition, the piezoelectric device includes a piezoelectric material and a pair of electrodes disposed in contact with the piezoelectric material, in which the piezoelectric material is the above-mentioned piezoelectric material.
摘要:
A lead-free piezoelectric material that does not undergo depolarization in a wide operating temperature range and has a good piezoelectric constant is provided. A piezoelectric material include a perovskite-type metal oxide represented by (Ba1-xCax)a(Ti1-yZry)O3 (where 1.00≦a≦1.01, 0.125≦x≦0.175, and 0.055≦y≦0.090) as a main component, and manganese incorporated in the perovskite-type metal oxide. The manganese content relative to 100 parts by weight of the perovskite-type metal oxide is 0.02 parts by weight or more and 0.10 parts by weight or less on a metal basis.
摘要:
A lead-free piezoelectric material that does not undergo depolarization in a wide operating temperature range and has a good piezoelectric constant is provided. A piezoelectric material include a perovskite-type metal oxide represented by (Ba1-xCax)a(Ti1-yZry)O3 (where 1.00≦a≦1.01, 0.125≦x≦0.175, and 0.055≦y≦0.090) as a main component, and manganese incorporated in the perovskite-type metal oxide. The manganese content relative to 100 parts by weight of the perovskite-type metal oxide is 0.02 parts by weight or more and 0.10 parts by weight or less on a metal basis.
摘要:
A lead-free piezoelectric material that has stable, excellent piezoelectric constant and mechanical quality factor in a wide operating temperature range is provided. A piezoelectric material include a perovskite-type metal oxide represented by (Ba1-xCax)a(Ti1-yZry)O3 (where 1.00≦a≦1.01, 0.155≦x≦0.300, 0.041≦y≦0.069) as a main component, and manganese incorporated in the perovskite-type metal oxide. The manganese content relative to 100 parts by weight of the perovskite-type metal oxide is 0.12 parts by weight or more and 0.40 parts by weight or less on a metal basis.
摘要:
A lead-free piezoelectric material that has stable, excellent piezoelectric constant and mechanical quality factor in a wide operating temperature range is provided. A piezoelectric material include a perovskite-type metal oxide represented by (Ba1-xCax)a(Ti1-yZry)O3 (where 1.00≦a≦1.01, 0.155≦x≦0.300, 0.041≦y≦0.069) as a main component, and manganese incorporated in the perovskite-type metal oxide. The manganese content relative to 100 parts by weight of the perovskite-type metal oxide is 0.12 parts by weight or more and 0.40 parts by weight or less on a metal basis.