Abstract:
Disclosed is a light-emitting device including a light-emitting element emitting primary light, and a light converter absorbing a part of the primary light emitted from the light-emitting element and emitting secondary light having a longer wavelength than the primary light. The light converter contains a green light-emitting phosphor and a red light-emitting phosphor. The green light-emitting phosphor is composed of at least one phosphor selected from a divalent europium-activated oxynitride phosphor substantially represented by the following formula: EuaSibAlcOdNe and a divalent europium-activated silicate phosphor substantially represented by the following formula: 2 (Ba1-f-gMIfEug)O.SiO2, while the red light-emitting phosphor is composed of at least one phosphor selected from tetravalent manganese-activated fluoro-tetravalent metalate phosphors substantially represented by the following formulae: MII2(MIII1-hMnh)F6 and/or MIV(MIII1-hMnh)F6. Consequently, the light-emitting device has excellent color gamut (NTSC ratio).
Abstract:
Provided is a phosphor particle group of divalent europium-activated oxynitride green light emitting phosphor particles each of which is a β-type SiAlON substantially represented by a general formula: EuaSibAlcOdNe, where 0.0055≦a≦0.4, b+c=12, d+e=16, wherein 60% or more of the phosphor particle group is composed of the phosphor particles in which a value obtained by dividing a longer particle diameter by a shorter particle diameter is greater than 1.0 and not greater than 3.0. A high-efficiency and stable light emitting apparatus using a β-type SiAlON, which includes a light converter using the phosphor particle group, and a phosphor particle group therefor are also provided.
Abstract translation:提供了一种二价铕激活的氮氧化物绿色发光荧光体颗粒的荧光体颗粒基团,其各自是基本上由通式:EuaSibAlcOdNe表示的“SiAlON”,其中0.0055和nlE; a≦̸ 0.4,b + c = 12, d + e = 16,其中,荧光体粒子群的60%以上由荧光体粒子构成,其中通过将更长的粒径除以更短的粒径而获得的值大于1.0且不大于3.0。 还提供了一种使用包含使用荧光体颗粒基团的光转换器和其荧光体粒子群的“SiAlON”的高效稳定的发光装置。
Abstract:
A green-emitting phosphor is activated by cerium and terbium and is represented by the general formula:(Re.sub.1-a-b-3c Tb.sub.a Ce.sub.b A.sub.3c).sub.2 O.sub.3.mP.sub.2 O.sub.5.nSiO.sub.2wherein Re is at least one member selected from the group consisting of yttrium, lanthanum, and gadolinium; A is at least one member selected from the group consisting of lithium (Li), sodium (Na), potassium (K), rubidium (Rb), and cesium (Cs); and a>0, b>0, c>0, 0 0, and n>0.The green-emitting phosphor of the invention may be widely applied to fluorescent lamps for copying machine light sources, or high luminous efficacy and high color rendering property fluorescent lamps such as three peak emission system fluorescent lamps.