Abstract:
A method comprising a) contacting a solvent, a carboxylic acid, and a peroxide-containing compound to form an acidic mixture wherein a weight ratio of solvent to carboxylic acid in the acidic mixture is from about 1:1 to about 100:1; b) contacting a titanium-containing compound and the acidic mixture to form a solubilized titanium mixture wherein an equivalent molar ratio of titanium-containing compound to carboxylic acid in the solubilized titanium mixture is from about 1:1 to about 1:4 and an equivalent molar ratio of titanium-containing compound to peroxide-containing compound in the solubilized titanium mixture is from about 1:1 to about 1:20; and c) contacting a chromium-silica support comprising from about 0.1 wt. % to about 20 wt. % water and the solubilized titanium mixture to form an addition product and drying the addition product by heating to a temperature in a range of from about 50° C. to about 150° C. and maintaining the temperature in the range of from about 50° C. to about 150° C. for a time period of from about 30 minutes to about 6 hours to form a pre-catalyst.
Abstract:
A method comprising a) contacting a solvent, a carboxylic acid, and a peroxide-containing compound to form an acidic mixture wherein a weight ratio of solvent to carboxylic acid in the acidic mixture is from about 1:1 to about 100:1; b) contacting a titanium-containing compound and the acidic mixture to form a solubilized titanium mixture wherein an equivalent molar ratio of titanium-containing compound to carboxylic acid in the solubilized titanium mixture is from about 1:1 to about 1:4 and an equivalent molar ratio of titanium-containing compound to peroxide-containing compound in the solubilized titanium mixture is from about 1:1 to about 1:20; and c) contacting a chromium-silica support comprising from about 0.1 wt. % to about 20 wt. % water and the solubilized titanium mixture to form an addition product and drying the addition product by heating to a temperature in a range of from about 50° C. to about 150° C. and maintaining the temperature in the range of from about 50° C. to about 150° C. for a time period of from about 30 minutes to about 6 hours to form a pre-catalyst.
Abstract:
A method comprising a) contacting a solvent, a carboxylic acid, and a peroxide-containing compound to form an acidic mixture wherein a weight ratio of solvent to carboxylic acid in the acidic mixture is from about 1:1 to about 100:1; b) contacting a titanium-containing compound and the acidic mixture to form a solubilized titanium mixture wherein an equivalent molar ratio of titanium-containing compound to carboxylic acid in the solubilized titanium mixture is from about 1:1 to about 1:4 and an equivalent molar ratio of titanium-containing compound to peroxide-containing compound in the solubilized titanium mixture is from about 1:1 to about 1:20; and c) contacting a chromium-silica support comprising from about 0.1 wt. % to about 20 wt. % water and the solubilized titanium mixture to form an addition product and drying the addition product by heating to a temperature in a range of from about 50° C. to about 150° C. and maintaining the temperature in the range of from about 50° C. to about 150° C. for a time period of from about 30 minutes to about 6 hours to form a pre-catalyst.
Abstract:
A pre-catalyst composition comprising a) a silica support comprising silica wherein an amount of silica ranges from about 70 wt. % to about 95 wt. % based upon a total weight of the silica support, b) a chromium-containing compound wherein an amount of chromium ranges from about 0.1 wt. % to about 5 wt. % based upon the amount of silica, c) a titanium-containing compound wherein an amount of titanium ranges from about 0.1 wt. % to about 20 wt. % based upon the amount of silica, d) a carboxylic acid wherein an equivalent molar ratio of titanium-containing compound to carboxylic acid ranges from about 1:1 to about 1:10, and e) a nitrogen-containing compound with a molecular formula containing at least one nitrogen atom wherein an equivalent molar ratio of titanium-containing compound to nitrogen-containing compound ranges from about 1:0.5 to about 1:10.
Abstract:
The present invention discloses processes for forming polythiol compositions from olefinic hydrocarbons such as cyclooctadiene, cyclododecatriene, and trivinylcyclohexane. The polythiol compositions produced from these processes, including the sulfur-containing compounds of these compositions, also are described.
Abstract:
The present invention discloses processes for forming polythiol compositions from olefinic hydrocarbons such as cyclooctadiene, cyclododecatriene, and trivinylcyclohexane. The polythiol compositions produced from these processes, including the sulfur-containing compounds of these compositions, also are described.
Abstract:
Methods for modifying a catalyst system component are disclosed in which a feed mixture containing a fluid and from 1 to 15 wt. % of a catalyst system component is introduced into an inlet of a hydrocyclone, an overflow stream containing from 0.1 to 5 wt. % solids and an underflow stream containing from 10 to 40 wt. % solids are discharged from the hydrocyclone, and the underflow stream is spray dried to form a modified catalyst component. Often, from 4 to 20 wt. % of the catalyst system component in the feed mixture has a particle size of less than or equal to 20 μm, or less than or equal to 10 μm.
Abstract:
Methods for modifying a catalyst system component are disclosed in which a feed mixture containing a fluid and from 1 to 15 wt. % of a catalyst system component is introduced into an inlet of a hydrocyclone, an overflow stream containing from 0.1 to 5 wt. % solids and an underflow stream containing from 10 to 40 wt. % solids are discharged from the hydrocyclone, and the underflow stream is spray dried to form a modified catalyst component. Often, from 4 to 20 wt. % of the catalyst system component in the feed mixture has a particle size of less than or equal to 20 μm, or less than or equal to 10 μm.
Abstract:
A method comprising a) contacting a solvent, a carboxylic acid, and a peroxide-containing compound to form an acidic mixture wherein a weight ratio of solvent to carboxylic acid in the acidic mixture is from about 1:1 to about 100:1; b) contacting a titanium-containing compound and the acidic mixture to form a solubilized titanium mixture wherein an equivalent molar ratio of titanium-containing compound to carboxylic acid in the solubilized titanium mixture is from about 1:1 to about 1:4 and an equivalent molar ratio of titanium-containing compound to peroxide-containing compound in the solubilized titanium mixture is from about 1:1 to about 1:20; and c) contacting a chromium-silica support comprising from about 0.1 wt. % to about 20 wt. % water and the solubilized titanium mixture to form an addition product and drying the addition product by heating to a temperature in a range of from about 50° C. to about 150° C. and maintaining the temperature in the range of from about 50° C. to about 150° C. for a time period of from about 30 minutes to about 6 hours to form a pre-catalyst.
Abstract:
A method comprising a) contacting a solvent, a carboxylic acid, and a peroxide-containing compound to form an acidic mixture wherein a weight ratio of solvent to carboxylic acid in the acidic mixture is from about 1:1 to about 100:1; b) contacting a titanium-containing compound and the acidic mixture to form a solubilized titanium mixture wherein an equivalent molar ratio of titanium-containing compound to carboxylic acid in the solubilized titanium mixture is from about 1:1 to about 1:4 and an equivalent molar ratio of titanium-containing compound to peroxide-containing compound in the solubilized titanium mixture is from about 1:1 to about 1:20; and c) contacting a chromium-silica support comprising from about 0.1 wt. % to about 20 wt. % water and the solubilized titanium mixture to form an addition product and drying the addition product by heating to a temperature in a range of from about 50° C. to about 150° C. and maintaining the temperature in the range of from about 50° C. to about 150° C. for a time period of from about 30 minutes to about 6 hours to form a pre-catalyst.