Abstract:
There is provided an optical film comprising a layer formed on a base film by curing a curable composition containing the specific component (A) in an amount of 50 to 99% by mass and the specific component (B) in an amount of 1 to 50% by mass, based on the total solid content of the curable composition when the total solid content of the curable composition is set to 100% by mass.
Abstract:
A method for producing an optical film including: laminating a hard coat layer on one side of an optical substrate in roll form, the hard coat layer having a transparent support and an optical anisotropic layer. The transparent support is laminated on the optical anisotropic layer, the one side is a transparent support-side of the optical substrate, the hard coat layer is obtained by coating, drying and curing a composition for forming a hard coat layer containing a curable monomer, a photo-polymerization initiator, and a solvent. The solvent is a mixture of at least one solvent selected from (S-1) and (S-2) and at least one solvent selected from (S-3), or a mixture of at least one solvent selected from (S-1) and at least one solvent selected from (S-2): (S-1) solvents dissolving the transparent support; (S-2) solvents swelling the transparent support; and (S-3) solvents neither dissolving nor swelling the transparent support.
Abstract:
There is provided an optical film to be used as a surface film for image display device, which comprises an optically anisotropic layer and a hard coat layer in this order on one surface of a transparent support, the optically anisotropic layer and the hard coat layer being brought into direct contact with each other, wherein the optically anisotropic layer is formed of an optically anisotropic layer forming composition containing a liquid crystalline compound having an unsaturated double bond; the hard coat layer is formed of a hard coat layer forming composition containing a compound having an unsaturated double bond and has a film thickness of from 3 to 30 μm; and the optical film has an in-plane retardation of from 80 to 200 nm at a wavelength of 550 nm.