Wet-grinding gypsum with polycarboxylates
    21.
    发明授权
    Wet-grinding gypsum with polycarboxylates 有权
    用多羧酸盐湿法研磨石膏

    公开(公告)号:US07861955B2

    公开(公告)日:2011-01-04

    申请号:US11985515

    申请日:2007-11-15

    IPC分类号: B02C19/00

    摘要: The process of the present invention includes obtaining a feed material having an initial median particle size. A solution of a polycarboxylate dispersant in water is formed, then the feed material is added to the solution to form a slurry. The slurry is wet-ground to reduce the median particle size of the feed material. Optionally, the total amount of polycarboxylate dispersant is divided into a plurality of doses that are added periodically over the total grinding time.

    摘要翻译: 本发明的方法包括获得具有初始中值粒度的进料。 形成聚羧酸酯分散剂在水中的溶液,然后将原料加入到溶液中形成浆料。 将浆料湿磨以减少进料的中值粒度。 任选地,多羧酸盐分散剂的总量被分成在总研磨时间内周期性加入的多个剂量。

    Surface enhancing coating for gypsum-containing floor underlayments
    23.
    发明授权
    Surface enhancing coating for gypsum-containing floor underlayments 有权
    含石膏地板底层的表面增强涂层

    公开(公告)号:US07276549B2

    公开(公告)日:2007-10-02

    申请号:US10755786

    申请日:2004-01-12

    IPC分类号: C08K3/30 C04B28/36

    摘要: A coating for preparing a floor underlayment to receive an adhesive includes a water-soluble, latex polymer, a defoamer and a dual-function surface enhancing agent. The surface enhancing agent includes a set accelerator that also functions to cross link the adhesive, hardening the surface of the underlayment using at least two mechanisms. One embodiment of the invention is a dry mixture that forms a coating when added to water. The dry mixture includes from about 10% to about 50% of the redispersible polymer by weight based on the mixture, from about 50% to about 90% of the surface enhancing agent and from about 0.15% to about 0.25% of the defoamer by weight based on the mixture. Other embodiments describe a liquid coating formed by adding from about 1 to about 8 pails water to 1 part of the dry mixture on a volumc basisby volume based on the mixture.

    摘要翻译: 用于制备底层底层以接收粘合剂的涂层包括水溶性胶乳聚合物,消泡剂和双功能表面增强剂。 表面增强剂包括一种既可以使粘合剂交联的功能的固化加速剂,也可以使用至少两种机制来硬化底层的表面。 本发明的一个实施方案是当添加到水中时形成涂层的干燥混合物。 干燥混合物包含基于混合物重量的约10%至约50%的可再分散聚合物,按重量计约50%至约90%的表面增强剂和约0.15%至约0.25%的消泡剂 基于混合物。 其它实施方案描述了通过基于混合物以体积计体积从约1至约8个桶中加入1份干燥混合物而形成的液体涂料。

    Surface enhancing coating for gypsum-containing floor underlayments
    27.
    发明申请
    Surface enhancing coating for gypsum-containing floor underlayments 有权
    含石膏地板底层的表面增强涂层

    公开(公告)号:US20060264548A1

    公开(公告)日:2006-11-23

    申请号:US11491333

    申请日:2006-07-21

    IPC分类号: C08K3/30

    摘要: A coating for preparing a floor underlayment to receive an adhesive includes a water-soluble, latex polymer, a defoamer and a dual-function surface enhancing agent. The surface enhancing agent includes a set accelerator that also functions to cross link the adhesive, hardening the surface of the underlayment using at least two mechanisms. One embodiment of the invention is a dry mixture that forms a coating when added to water. The dry mixture includes from about 10% to about 50% of the redispersible polymerby weight based on the mixture, from about 50% to about 90% of the surface enhancing agent and from about 0.15% to about 0.25% of the defoamerby weight based on the mixture. Other embodiments describe a liquid coating formed by adding from about 1 to about 8 parts water to 1 part of the dry mixture by volume based on the mixture.

    摘要翻译: 用于制备底层底层以接收粘合剂的涂层包括水溶性胶乳聚合物,消泡剂和双功能表面增强剂。 表面增强剂包括一种既可以使粘合剂交联的功能的固化加速剂,也可以使用至少两种机制来硬化底层的表面。 本发明的一个实施方案是当添加到水中时形成涂层的干燥混合物。 基于混合物,干混合物包含约10%至约50%的可再分散聚合物,约50%至约90%的表面增强剂和约0.15%至约0.25%的消泡剂重量,基于 混合物。 其它实施方案描述了通过基于混合物按体积添加约1至约8份水至1份干燥混合物而形成的液体涂料。

    METHOD AND APPARATUS FOR PRESSURIZED CALCINATION OF GYPSUM
    29.
    发明申请
    METHOD AND APPARATUS FOR PRESSURIZED CALCINATION OF GYPSUM 有权
    方法和装置用于压力计算

    公开(公告)号:US20090257946A1

    公开(公告)日:2009-10-15

    申请号:US12388793

    申请日:2009-02-19

    IPC分类号: C01F11/46 B01J19/00

    摘要: A method for calcining gypsum in a pressurized reactor by injecting combustion gases and air into the pressurized reactor to create a fluidized bed of gypsum, and heating the fluidized bed of gypsum in the pressurized reactor sufficiently to form a calcined hemihydrate.

    摘要翻译: 一种通过将加压反应器中的燃烧气体和空气注入加压反应器中以产生石膏流化床并在加压反应器中充分加热石膏流化床以形成煅烧半水合物的方式来在加压反应器中煅烧石膏。