Abstract:
Disclosed are an alkoxysilylated isocyanurate epoxy compound, a composite of which exhibiting low CTE and high glass transition temperature or Tg-less and/or a cured product of which exhibiting good flame retardant property, a method of preparing the same, a composition including the same, a cured product formed of the composition, and a use of the composition. An isocyanurate epoxy compound having an alkoxysilyl group and an epoxy group in a core; a method of manufacturing the epoxy compound by the epoxidation and alkoxysilylation of a starting material; an epoxy composition including the epoxy compound; and a cured product and a use thereof, are provided. A composite of the epoxy composition has improved bonding efficiency between alkoxysilyl group and filler and between alkoxysilyl groups, and has good heat resistance, low CTE, and high glass transition temperature or Tg-less. A cured product formed of the epoxy composition has good flame retardant property.
Abstract:
Provided is a color lighting control method including a lighting device having a plurality of lighting unit, the method including the steps of: (a) applying predetermined input voltages to the plurality of lighting units respectively and obtaining image data through the camera; (b) calculating an image histogram that is a distribution graph for displaying the number of pixels corresponding to each monochrome level intensity through the image data; (c) calculating a standard deviation of the image histogram; and (d) calculating an optimal input voltage value for each of the plurality of lighting units within an adjustment range of the predetermined input voltages, wherein the optimal input voltage value maximizes the standard deviation.
Abstract:
The present invention relates to a self-adhesive protection film having improved release properties and a product attached with the same, and in particular, to a multilayered self-adhesive protection film having particularly enhanced release properties by comprising monodisperse beads in a carrier layer or the carrier layer being embo patterned, and to a product attached with the self-adhesive protection film.
Abstract:
Disclosed is an aluminum alloy for die casting which comprises 1.0 weight % to 2.0 weight % of magnesium (Mg), 0.5 weight % to 1.6 weight % of iron (Fe), and 0.5 weight % to 0.9 weight % of silicon (Si), with the remainder being aluminum (Al) and inevitable impurities.
Abstract:
The present invention relates to a desulfurizing agent of improved oxidation resistance, ignition resistance and productivity, and a method for manufacturing the desulfurizing agent. The desulfurizing agent may include a plurality of magnesium-aluminum alloy grains with grain boundaries, and a compound of one selected from consisting of magnesium and aluminum and one selected from consisting of alkaline metal and alkaline earth metal, the compound exists in the grain boundaries and is not inside but outside of the magnesium-aluminum alloy grains.
Abstract:
According to the apparatus and method, metals can be molded under a low extrusion pressure, the life of the apparatus is prolonged, the strength of the metal products is improved, the ignition of the metals is inhibited during processing, the amount of a protective gas used is reduced, and the formation of welding lines is inhibited.
Abstract:
According to the apparatus and method, metals can be molded under a low extrusion pressure, the life of the apparatus is prolonged, the strength of the metal products is improved, the ignition of the metals is inhibited during processing, the amount of a protective gas used is reduced, and the formation of welding lines is inhibited.
Abstract:
The present invention relates to a desulfurizing agent of improved oxidation resistance, ignition resistance and productivity, and a method for manufacturing the desulfurizing agent. The desulfurizing agent may include a plurality of magnesium-aluminum alloy grains with grain boundaries, and a compound of one selected from consisting of magnesium and aluminum and one selected from consisting of alkaline metal and alkaline earth metal, the compound exists in the grain boundaries and is not inside but outside of the magnesium-aluminum alloy grains.
Abstract:
A method for manufacturing a melt-spun nonwoven fabric, in which fibers obtained by melt-spinning a thermoplastic polymer through a spinning nozzle having at least one or more nozzle holes are collected by high-speed air stream according to a spunbond method, includes: the steps of: allowing the melt-spun fibers to pass through local nozzle heaters of a nozzle heating mantle located just on the underside of the spinning nozzle during the spinning; and allowing the melt-spun fibers to be subjected to momentary local heating with a temperature difference of 0.1 to 1,000° C. from a temperature of a pack body. Polypropylene (PP) having a melt flow index (MFI) of 3 to 900 or polyethylene terephthalate (PET) having intrinsic viscosity (I.V.) of 0.5 to 3.0 is subjected to momentary local heating to a high temperature during the spinning to thus perform fiber fineness.
Abstract:
Proposed is a Fe-based alloy and a filler metal including the same. The Fe-based alloy contains 15% to 25% by weight of nickel (Ni), 0.5% to 3% by weight of manganese (Mn), 2% to 8% by weight of cobalt (Co), 0.1% to 0.5% by weight of carbon (C), and the balance iron (Fe) and unavoidable impurities.