Abstract:
The present disclosure is directed to a process for producing thermoplastic polyolefin roofing membrane. The process includes directly adding components of a high-load flame retardant TPO formulation to a counter-rotating twin screw extruder. The process includes extruding the formulation with counter-rotation of the twin screws and forming a TPO roofing membrane having a tensile strength of greater than 10 MPa and a flame retardance of rating of classification D as measured in accordance with EN ISO 1 1925-2, surface exposure test.
Abstract translation:本公开涉及一种生产热塑性聚烯烃屋顶膜的方法。 该方法包括将高负载阻燃TPO制剂的组分直接添加到反向旋转双螺杆挤出机中。 该方法包括按照双螺杆的反向挤压制剂,并形成具有大于10MPa的拉伸强度的TPO屋顶膜和根据EN ISO 1 1925-2测量的分级D的等级的阻燃性, 表面暴露试验。
Abstract:
The present disclosure provides a composition. In an embodiment, the composition includes a neat ethylene/propylene/nonconjugated polyene interpolymer. The neat ethylene/propylene/nonconjugated polyene interpolymer includes from greater than 0 wt % to 6.0 wt % nonconjugated polyene. The neat ethylene/propylene/nonconjugated polyene interpolymer has the following properties: (i) a molecular weight (Mw) from 240,000 to 270,000; (ii) a Mooney viscosity (ML (1+4), 125° C.) from 80 to 85; (iii) a rheology ratio (RR) from 35 to 65; (iv) a Mw/Mn from 2.2 to 3.5; (v) a tan delta ratio from 0.6 to 0.9; and (vi) an absolute tan delta slope from 5.0 to less than 10.0.
Abstract:
A composition comprising at least the following components: A) one or more ethylene/alpha-olefin interpolymers, which comprise ≤3.5 wt % of a non-conjugated diene, based on the weight of the one or more ethylene/alpha-olefin interpolymers; B) an acid acceptor selected from the following: MgO, ZnO, or combination thereof.
Abstract:
A composition comprising the following components: a) at least one propylene/ethylene interpolymer or at least one propylene/alpha-olefin interpolymer, each interpolymer comprising the following properties: i) a melting point, Tm, from 60° C. to 85° C., ii) a viscosity (177° C.) from 3,000 cP to 30,000 cP; b) at least one wax; c) at least one oil; and wherein the composition has a weight ratio component b to component c from 0.30 to 4.0.
Abstract:
Polymer compositions include an interpolymer of ethylene, an α-olefin, and a nonconjugated polyene; and from 10% to 40% by weight oil. The polymer composition has a Mooney viscosity from 20 to 70. The interpolymer may include from 66% to 75% by weight monomer units derived from ethylene; and from 0.5% to 10% by weight monomer units derived from the nonconjugated polyene. The neat interpolymer may have: a weight-average molecular weight Mw from 250 kDa to 300 kDa; a Mooney viscosity from 50 to 200; a rheology ratio V0.1/V100 less than 30; a ratio of molecular weight to low-shear viscosity Mw/V0.1 greater than 4.0; a polydispersity index from 2.0 to 3.5; and a tan δ at 0.1 rad/sand 190° C. greater than 2.0. The polymer compositions may be in the form of pellets having desirable flow characteristics. Thermoplastic vulcanizates may include the polymer compositions. Articles may include the thermoplastic vulcanizates.
Abstract:
A composition comprising the following components: A) a first ethylene/alpha-olefin interpolymer with a melt index I2A; B) a second ethylene/alpha-olefin interpolymer with a melt index I2B; and wherein the difference in melt index (I2): (I2A−I2B)≥400, and wherein I2B≤100 g/10 min; C) a filler, and wherein the filler is present in an amount ≥50 wt %, based on the weight of the composition; D) a tackifier; and wherein the melt viscosity, at 165 C, of the composition, excluding the filler (component C), is ≤30,000 cP.
Abstract:
A composition comprising (A) from 10 wt % to 90 wt % of a polymeric ethylene ionomer; (B) from 10 wt % to 40 wt % of a propylene component including at least one propylene based polymer having a propylene content of at least 50.0 wt %, based on the total weight of the propylene based polymer, and a melt flow rate from 0.5 g/10 min to 200.0 g/10 min (according to ASTM D-1238 at 230° C./2.16 kg); and (C) from 5 wt % to 20 wt % of a crystalline block composite.
Abstract:
The invention provides a composition comprising at least the following components: A) an ethylene/α-olefin/nonconjugated polyene interpolymer that has the following properties: i) a rheology ratio (V0.1/V100 at 190° C.) greater than, or equal to, 35; ii) a weight average molecular weight (Mw) greater than, or equal to, 200,000 g/mol; and iii) a CCDB (Chemical Composition Distribution Breadth) less than 7; B) a thermoplastic polymer; C) a vulcanization agent; and wherein the interpolymer comprises incorporated oil. The invention also provides a composition comprising the following: A) a first composition comprising: a) a first ethylene/α-olefin/nonconjugated polyene interpolymer; b) a second ethylene/α-olefin/nonconjugated polyene interpolymer; and wherein the first composition has the following properties: i) an MWD less than, or equal to, 3.5, ii) a Mooney Viscosity (ML (1+4, 125° C.)) greater than, or equal to, 60, iii) a CCDB from 7 to 15; B) a thermoplastic polymer; C) a vulcanization agent; and wherein the first interpolymer and the second interpolymer comprise incorporated oil.
Abstract:
A thermoplastic vulcanizate composition includes (a) a crystalline thermoplastic polyolefin comprising alpha-olefin monomers having from 2 to 5 carbon atoms, (b) a rubber block interpolymer comprising a first block and a second block having differing chemical or physical properties from the first block, the first block is derived from ethylene, a first alpha-olefin monomer having from 3 to 10 carbon atoms, and a first diene monomer having from 2 to 25 carbon atoms, the second block is derived from ethylene, a second alpha-olefin monomer having from 3 to 10 carbon atoms, and optionally a second diene monomer having from 2 to 25 carbon atoms, and an amount of the block interpolymer in the composition being greater than an amount of the thermoplastic polyolefin in the composition, and (c) a curative system.
Abstract:
A composition comprising at least the following (A) an ethylene/α-olefin copolymer; (B) an olefin-based polymer; (C) a crosslinking agent; and (D) a multifunctional acrylate coagent; wherein the ethylene/α-olefin copolymer of component A) has the following properties: (i) has a density from 0.855 to 0.875 g/cc; and (ii) a Mooney Viscosity (ML 1+4, 121° C.) from 10 to 100 is provided.