Abstract:
The invention provides a composition comprising at least the following components: A) a first composition comprising a first ethylene/α-olefin block copolymer consisting of ethylene and C4-C8 α-olefin comonomer; and where the first composition has a density from 0.87 g/cc to 0.90 g/cc, and a melt index (I2) from 6.0 to 20.0 g/10 min; B) at least one filler that is capable of being excited by an alternating electromagnetic field at a frequency greater than, or equal to 10 MHz; C) at least one flame retardant selected from the group consisting of i) from 30.0 to 50.0 wt % of one or more non-halogen, inorganic flame retardant compounds, based on the weight of the composition; and ii) from 8.0 to 30.0 wt % of one or more halogen-containing flame retardant compounds, based on the weight of the composition; and D) at least one polar polymer.
Abstract:
The present disclosure provides and article. The article includes: (A) a polyester fabric; (B) a coating on a surface of the polyester fabric, the coating comprising at least one of (i) an ethylene/vinyl acetate/maleic anhydride terpolymer and (ii) an ethylene/methyl acrylate/glycidyl methacrylate terpolymer.
Abstract:
The present disclosure provides a fabric laminate. In an embodiment, the fabric laminate includes a fabric sheet, a coating layer, and a tie layer. The fabric sheet is composed of propylene-based polymer fibers. The coating layer is composed of one or more ethylene-based polymers. The tie layer is located between the fabric sheet and the coating layer. The tie layer is composed of at least 50 wt % of a crystalline block composite (CBC) and an optional blend component. The CBC includes (i) an isotactic crystalline propylene homopolymer (iPP); (ii) an ethylene/propylene copolymer; and (iii) a diblock with the formula (EP)-(iPP). The CBC has a block composite index (CBCI) from 0.1 to 1.0. The fabric laminate has a peel force from 20 N/15 mm to 40 N/15 mm.
Abstract:
The present disclosure provides a composition. In an embodiment, the composition includes A) an ethylene/acrylate interpolymer or an ethylene/acetate interpolymer; B) an ethylene/α-olefin multi-block copolymer; and C) a flame retardant. In an embodiment, the ethylene/acrylate interpolymer is a functionalized ethylene/acrylate interpolymer. The present composition exhibits improved dirt pick-up resistance.
Abstract:
The invention provides a composition comprising at least the following components: A) a first composition comprising a first ethylene-based interpolymer; and where the first composition has a density less than, or equal to, 0.91 g/cc, and a melt index (I2) from 6.0 to 20.0 g/10 min; B) optionally, at least one filler that is capable of being excited by an alternating electromagnetic field at a frequency greater than, or equal to, 10 MHz; C) at least one flame retardant selected from the following: i) from 30.0 to 50.0 wt % of one or more non-halogen, inorganic flame retardant compounds, based on the weight of the composition; or ii) from 8.0 to 30.0 wt % of one or more halogen-containing flame retardant compounds, based on the weight of the composition; and D) at least one polar polymer.
Abstract:
The present disclosure is directed to a process for producing thermoplastic polyolefin roofing membrane. The process includes directly adding components of a high-load flame retardant TPO formulation to a counter-rotating twin screw extruder. The process includes extruding the formulation with counter-rotation of the twin screws and forming a TPO roofing membrane having a tensile strength of greater than 10 MPa and a flame retardance of rating of classification D as measured in accordance with EN ISO 11925-2, surface exposure test.
Abstract:
The present disclosure is directed to a process for producing thermoplastic polyolefin roofing membrane. The process includes directly adding components of a high-load flame retardant TPO formulation to a counter-rotating twin screw extruder. The process includes extruding the formulation with counter-rotation of the twin screws and forming a TPO roofing membrane having a tensile strength of greater than 10 MPa and a flame retardance of rating of classification D as measured in accordance with EN ISO 1 1925-2, surface exposure test.
Abstract:
The present disclosure is directed to a process for producing thermoplastic polyolefin roofing membrane. The process includes directly adding components of a high-load flame retardant TPO formulation to a counter-rotating twin screw extruder. The process includes extruding the formulation with counter-rotation of the twin screws and forming a TPO roofing membrane having a tensile strength of greater than 10 MPa and a flame retardance of rating of classification D as measured in accordance with EN ISO 1 1925-2, surface exposure test.
Abstract translation:本公开涉及一种生产热塑性聚烯烃屋顶膜的方法。 该方法包括将高负载阻燃TPO制剂的组分直接添加到反向旋转双螺杆挤出机中。 该方法包括按照双螺杆的反向挤压制剂,并形成具有大于10MPa的拉伸强度的TPO屋顶膜和根据EN ISO 1 1925-2测量的分级D的等级的阻燃性, 表面暴露试验。
Abstract:
The present disclosure provides and article. The article includes: (A) a polyester fabric; (B) a coating on a surface of the polyester fabric, the coating comprising at least one of (i) an ethylene/vinyl acetate/maleic anhydride terpolymer and (ii) an ethylene/methyl acrylate/glycidyl methacrylate terpolymer.