Friction member manufacturing apparatus
    31.
    发明申请
    Friction member manufacturing apparatus 失效
    摩擦件制造装置

    公开(公告)号:US20050048160A1

    公开(公告)日:2005-03-03

    申请号:US10865070

    申请日:2004-06-10

    摘要: The present invention provides an improved multi-mold apparatus for manufacturing friction members, with each mold composed of a set comprising a first (top) mold, a second (bottom) mold, and a frame mold. The apparatus is capable of correcting any misalignment in the mountings of the plurality of molds and accurately aligning the molds by movably supporting at least one of the first mold, the second mold and the third mold by first, second and frame bases, respectively, so that the base and molds are movable laterally, in a direction perpendicular to the direction of advance. Projections are formed on one of the first mold and either the frame mold or the back plate and bonding through-holes are formed on the remaining mold or the back plate, so that the projections engage the holes so as to align the first mold and the frame mold accurately.

    摘要翻译: 本发明提供了一种用于制造摩擦构件的改进的多模式装置,每个模具由包括第一(顶部)模具,第二(底部)模具和框架模具的组合构成。 该装置能够校正多个模具的安装中的任何未对准并且通过分别通过第一,第二和框架基座可移动地支撑第一模具,第二模具和第三模具中的至少一个来精确对准模具,因此 基座和模具可以在垂直于前进方向的方向上横向移动。 在第一模具和框架模具或背板中的一个上形成突起,并且在剩余的模具或背板上形成结合通孔,使得突出部与孔对接,以使第一模具和 框架模具准确。

    Manufacturing method for monolithic ceramic part and cutting device for ceramic laminate
    32.
    发明授权
    Manufacturing method for monolithic ceramic part and cutting device for ceramic laminate 有权
    陶瓷层压板的整体陶瓷部件和切割装置的制造方法

    公开(公告)号:US06374820B1

    公开(公告)日:2002-04-23

    申请号:US09670650

    申请日:2000-09-27

    IPC分类号: B28D104

    CPC分类号: B28D1/222 B28D5/0023

    摘要: A manufacturing method for a monolithic ceramic part permitting a ceramic laminate to be cut stably and speedily, even if the thickness of the ceramic laminate is large. In order to divide a mother ceramic laminate into individual laminates of monolithic ceramic part units, the ceramic laminate is cut with a cutting blade, using a pair of guides disposed on opposite sides of the cutting blade in the vicinity of one principal plane of the ceramic laminate to control the cutting direction, and then individual ceramic laminates thus obtained by cutting are fired.

    摘要翻译: 即使陶瓷层叠体的厚度大,也能够稳定,快速地切断陶瓷层叠体的整体式陶瓷部件的制造方法。 为了将母体陶瓷层压体分成单块陶瓷部件单元的单个叠层体,用切割刀片切割陶瓷层压体,使用设置在切割刀片的相对侧上的一对导轨,该导向件在陶瓷的一个主平面附近 层压体以控制切割方向,然后烧制由此获得的各陶瓷层压体。

    Method and liquid coating composition for the formation of silica-based
coating film on substrate surface
    34.
    发明授权
    Method and liquid coating composition for the formation of silica-based coating film on substrate surface 失效
    用于在基材表面形成二氧化硅基涂膜的方法和液体涂料组合物

    公开(公告)号:US5496402A

    公开(公告)日:1996-03-05

    申请号:US307063

    申请日:1994-09-16

    摘要: Proposed is a liquid coating composition for the formation of a siliceous coating film having good storage stability against gelation for the protection, levelling or electric insulation of various substrate surfaces. The composition is a uniform solution comprising:(A) a partial cohydrolysis-cocondensation product of(a) a first hydrolyzable silane compound represented by the general formulaHSi(OR).sub.3, in which each R is, independently from the others, an alkyl group having 1 to 4 carbon atoms or a phenyl group, and(b) a second hydrolyzable silane compound represented by the general formulaSi(OR).sub.4, in which each R has the same meaning as defined above, in a molar ratio of (a):(b) in the range from 1:9 to 9:1; and (B) an organic solvent to dissolve the component (A). The storage stability of the coating composition can be improved by removing the alcohol contained therein as the hydrolysis product of the silane compounds to such a content as not to exceed 15% by weight.

    摘要翻译: 提出了一种液体涂料组合物,用于形成具有良好保存稳定性的硅质涂膜,用于各种基材表面的保护,调平或电绝缘。 该组合物是均匀的溶液,其包含:(A)(a)由通式HSi(OR)3表示的第一可水解硅烷化合物的部分共水解 - 缩聚产物,其中每个R独立地为烷基 具有1至4个碳原子的基团或苯基,和(b)由通式Si(OR)4表示的第二可水解硅烷化合物,其中每个R具有与上述相同的含义,摩尔比为 a):( b)在1:9至9:1的范围内; 和(B)有机溶剂以溶解组分(A)。 通过将其中含有的醇作为硅烷化合物的水解产物除去不超过15重量%的含量,可以提高涂料组合物的保存稳定性。