Method for providing toughened poly(trimethylene terephthalate) molding resins
    36.
    发明授权
    Method for providing toughened poly(trimethylene terephthalate) molding resins 有权
    提供增韧的聚对苯二甲酸丙二醇酯模塑树脂的方法

    公开(公告)号:US08389604B2

    公开(公告)日:2013-03-05

    申请号:US12916830

    申请日:2010-11-01

    摘要: Disclosed is a method including (A) melt blending first components including (a-1) a poly(trimethylene terephthalate) homopolymer or copolymer resin; and (a-2) one or more ionomer polymers or a combination of one or more ionomer polymers and acid polymers; to provide a first melt blend; and (B) melt blending said first melt blend with one or more Group B polymeric toughener(s) selected from the group consisting of an ethylene copolymers of the formula E/X/Y wherein: E is the radical formed from ethylene; X is selected from the group consisting of radicals formed from CH2═CH(R1)—C(O)—OR2 Y is one or more radicals formed from selected monomers with the proviso that Y must include at least one radical formed from monomers selected from the group consisting of maleic anhydride, (meth)acrylic acid, maleic acid, maleic acid monoesters, itaconic acid, fumaric acid, fumaric acid monoesters, salts of said preceding acids, and glycidyl acrylate, glycidyl methacrylate, and glycidyl vinyl ether.

    摘要翻译: 公开了一种方法,包括(A)熔融共混第一成分,包括(a-1)聚(对苯二甲酸丙二醇酯)均聚物或共聚物树脂; 和(a-2)一种或多种离聚物聚合物或一种或多种离聚物聚合物和酸聚合物的组合; 以提供第一熔融共混物; 和(B)将所述第一熔融共混物与一种或多种选自式E / X / Y的乙烯共聚物的B族聚合物增韧剂熔融共混,其中:E是由乙烯形成的自由基; X选自由CH 2 = CH(R 1)-C(O)-OR 2 Y所形成的基团,Y是由选自单体形成的一个或多个基团,条件是Y必须包括至少一个选自以下的单体形成的基团: 马来酸酐,(甲基)丙烯酸,马来酸,马来酸单酯,衣康酸,富马酸,富马酸单酯,前述酸的盐和丙烯酸缩水甘油酯,甲基丙烯酸缩水甘油酯和缩水甘油基乙烯基醚组成的组。

    Solar cell modules comprising an encapsulant sheet of a blend of ethylene copolymers
    37.
    发明授权
    Solar cell modules comprising an encapsulant sheet of a blend of ethylene copolymers 有权
    太阳能电池组件包括乙烯共聚物共混物的密封片

    公开(公告)号:US08080727B2

    公开(公告)日:2011-12-20

    申请号:US12276846

    申请日:2008-11-24

    申请人: Richard T. Chou

    发明人: Richard T. Chou

    IPC分类号: H01L31/042 H01L31/00

    摘要: Disclosed is a solar cell module comprising a polymeric encapsulant sheet, wherein the polymeric encapsulant sheet comprises a blend composition of an ethylene copolymer A and an ethylene copolymer B, the blend composition having a melt flow rate of less than 100 g/10 min, as determined in accordance with ASTM D1238 at 190° C. and 2.16 kg, and wherein the ethylene copolymer A comprises copolymerized units of ethylene and about 3 to about 20 wt % of an ester or anhydride of a C4-C8 unsaturated acid having two carboxylic acid groups and the ethylene copolymer B comprises copolymerized units of ethylene and about 6 to about 40 wt % of a polar monomer selected from the group consisting of vinyl acetate, alkyl (meth)acrylates, and mixtures thereof.

    摘要翻译: 公开了一种包括聚合物密封片的太阳能电池模块,其中聚合物密封片包含乙烯共聚物A和乙烯共聚物B的共混物组合物,该共混组合物的熔体流动速率小于100g / 10分钟,如 根据ASTM D1238在190℃和2.16kg下测定,其中乙烯共聚物A包含乙烯的共聚单元和约3至约20wt%的具有两个羧酸的C 4 -C 8不饱和酸的酯或酸酐 基团和乙烯共聚物B包含乙烯的共聚单元和约6至约40重量%的选自乙酸乙烯酯,(甲基)丙烯酸烷基酯及其混合物的极性单体。

    METHOD FOR PROVIDING TOUGHENED POLY(TRIMETHYLENE TEREPHTHALATE) MOLDING RESINS
    40.
    发明申请
    METHOD FOR PROVIDING TOUGHENED POLY(TRIMETHYLENE TEREPHTHALATE) MOLDING RESINS 有权
    提供增韧聚(三甲基苯乙烯)模塑树脂的方法

    公开(公告)号:US20110105674A1

    公开(公告)日:2011-05-05

    申请号:US12916830

    申请日:2010-11-01

    IPC分类号: C08L31/08

    摘要: Disclosed is a method including (A) melt blending first components including (a-1) a poly(trimethylene terephthalate) homopolymer or copolymer resin; and (a-2) one or more ionomer polymers or a combination of one or more ionomer polymers and acid polymers; to provide a first melt blend; and (B) melt blending said first melt blend with one or more Group B polymeric toughener(s) selected from the group consisting of an ethylene copolymers of the formula E/X/Y wherein: E is the radical formed from ethylene; X is selected from the group consisting of radicals formed from CH2═CH(R1)—C(O)—OR2 Y is one or more radicals formed from selected monomers with the proviso that Y must include at least one radical formed from monomers selected from the group consisting of maleic anhydride, (meth)acrylic acid, maleic acid, maleic acid monoesters, itaconic acid, fumaric acid, fumaric acid monoesters, salts of said preceding acids, and glycidyl acrylate, glycidyl methacrylate, and glycidyl vinyl ether.

    摘要翻译: 公开了一种方法,包括(A)熔融共混第一成分,包括(a-1)聚(对苯二甲酸丙二醇酯)均聚物或共聚物树脂; 和(a-2)一种或多种离聚物聚合物或一种或多种离聚物聚合物和酸聚合物的组合; 以提供第一熔融共混物; 和(B)将所述第一熔融共混物与一种或多种选自式E / X / Y的乙烯共聚物的B族聚合物增韧剂熔融共混,其中:E是由乙烯形成的自由基; X选自由CH 2 = CH(R 1)-C(O)-OR 2 Y所形成的基团,Y是由选自单体形成的一个或多个基团,条件是Y必须包括至少一个选自以下的单体形成的基团: 马来酸酐,(甲基)丙烯酸,马来酸,马来酸单酯,衣康酸,富马酸,富马酸单酯,前述酸的盐和丙烯酸缩水甘油酯,甲基丙烯酸缩水甘油酯和缩水甘油基乙烯基醚组成的组。