Abstract:
An acetal-based compound represented by Formula 1, an acetal-based prepolymer, an acetal-based polymer, and a photoresist composition including the same
wherein in Formula 1, R1 to R10, G, a, and b are as defined in the detailed description, and * indicates a linking site.
Abstract:
A laminated film which includes a first layer including a poly(amide-imide) copolymer, and a second layer laminated on at least one surface of the first layer. The second layer includes a poly(amide-imide) copolymer, polyimide, or a combination thereof, which has an amide content of less than or equal to about 30 mol %. The poly(amide-imide) copolymer included in the first layer has a weight average molecular weight of about 30,000 grams/mole to about 200,000 grams/mole, and the polyimide, the poly(amide-imide) copolymer, or the combination thereof, of the second layer has a weight average molecular weight of about 10,000 grams/mole to about 50,000 grams/mole, and the composition for preparing the laminated film.
Abstract:
A poly(amide-imide) copolymer that is a reaction product of a substituted or unsubstituted aromatic diamine having a maximum absorption wavelength in a range from 500 nanometers (nm) to 650 nm in a visible light region, a diamine represented by Chemical Formula 1, a dicarbonyl compound represented by Chemical Formula 2, and a tetracarboxylic acid dianhydride represented by Chemical Formula 3: wherein, in Chemical Formulae 1 to 3, A, R3, R10, R12, R13, X, n7 and n8 are the same as defined in the specification.
Abstract:
A window for a display device including: a plastic substrate including a poly(imide-amide) copolymer, which is a reaction product of a reagent combination of 4,4′-hexafluoroisopropylidene diphthalic anhydride, 3,3′,4,4′-biphenyltetracarboxylic dianhydride, 2,2′-bis-trifluoromethyl-4,4′-biphenyldiamine, and terephthaloyl chloride, and a hard coating layer disposed on at least one side of the plastic substrate, wherein the plastic substrate has pencil scratch hardness of greater than or equal to 3H when measured according to an ASTM D3363 standard at a vertical load of about 0.5 kilograms, and a peak intensity ratio A2/A1 of a peak intensity A2 at a position of about 23.5° in 2θ to a peak intensity A1 at a position of about 15.5° in 2θ of an X-ray diffraction spectrum is greater than or equal to about 0.8.
Abstract:
A composition for preparing poly(imide-benzoxazole) copolymer is described, where the copolymer include: a tetracarboxylic acid dianhydride represented by Chemical Formula 1, a diamine represented by Chemical Formula 2, and a diamine represented by Chemical Formula 3: wherein definitions of groups and variables in Chemical Formulae 1 to 3 are the same as described in the specification.