Abstract:
A catalyst for the polymerization of olefins comprising:(A) a catalyst component obtained by a process comprising contacting (a) a fatty acid salt of magnesium, (b) a carbonate of magnesium or a substance containing said carbonate, (c) diester of an aromatic dicarboxylic acid, and (d) a titanium halide of the general formula: TiX.sub.4, wherein X represents a halogen atom;(B) a silicon compound represented by the general formula: SiR.sub.m (OR').sub.4-m, wherein R is hydrogen, alkyl group or aryl group, R' is alkyl group or aryl group, and m is represented as O.ltoreq.m.ltoreq.4; and(C) an organoaluminium compound.Polymerization of olefins by use of the catalyst provides such advantages as high polymerization activity per unit weight of the catalyst component, prolonged polymerization activity, high yield of stereoregular polymer, and a produced polymer free of such an estereal odor as in the prior art, and having high bulk density as well as uniform particle size and shape.
Abstract:
A catalyst for the polymerization of olefins comprising:(A) a catalyst component obtained by a process comprising contacting (a) a fatty acid salt of magnesium and (b) dialkoxymagnesium, (c) mono or diester of an aromatic dicarboxylic acid, (d) a halogenated hydrocarbon and (e) a titanium halide of the general formula: TiX.sub.4, wherein X represents a halogen atom;(B) a silicon compound represented by the general formula: SiR.sub.m (OR').sub.4-m, wherein R is hydrogen, alkyl group or aryl group, R' is alkyl group or aryl group, and m is represented as O.ltoreq.m.ltoreq.4; and(C) an organoaluminum compound.Polymerization of olefins by use of the catalyst provides such advantages as high polymerization activity per unit weight of the catalyst component, prolonged polymerization activity, high yield of stereoregular polymer, and a produced polymer free of such an estereal odor as in the prior art.
Abstract translation:一种用于烯烃聚合的催化剂,包括:(A)通过以下方法获得的催化剂组分,该方法包括:(a)镁的脂肪酸盐和(b)二烷氧基镁,(c)芳族二羧酸的单或二酯,(d )卤代烃和(e)以下通式的卤化钛:TiX 4,其中X表示卤素原子; (B)由通式SiRm(OR')4-m表示的硅化合物,其中R是氢,烷基或芳基,R'是烷基或芳基,m表示为O m = 4; 和(C)有机铝化合物。 通过使用催化剂进行烯烃的聚合提供了以下优点:每单位重量的催化剂组分具有高聚合活性,延长的聚合活性,立体有规聚合物的高收率,以及与现有技术中没有这种亲和气味的生产聚合物。
Abstract:
A waste gas exhausted from a chlorination furnace during the manufacture of titanium tetrachloride or zirconium tetrachloride which contains larger quantities of CO.sub.2 and harmful substances such as chlorides and the like is subjected to treatment which comprises the sequential steps of scrubbing the waste gas in a water scrubbing column, removing moisture from the waste gas to allow the waste gas to have a dew point of no more that 5.degree. C., and adsorbing the waste gas in an activated carbon packed column. The process is capable of reducing the content of chlorides in the waste gas to a level of no more than 5 ppm in HCl equivalent.
Abstract:
ABSTRACT: The titanium porous body according to the present invention is in a form of a sheet, and has a thickness of 0.3 mm or less, and a bending strain at break of 0.005 or more, wherein, for a three-dimensional surface texture of at least one surface of the titanium porous body, an arithmetic mean height Sa is 2.5 μm or less, a maximum height Sz is 30 μm or less, an aspect ratio Str of the surface texture is 0.93 or more, and an arithmetic mean curvature Spc of a peak is 4.8 (1/μm) or less.
Abstract:
Provided is a solid catalyst component for olefin polymerization which is capable of exerting favorable ethylene responsiveness while forming a propylene homopolymer having high stereoregularity, when subjected to ethylene-propylene copolymerization reaction. The present invention provides a solid catalyst component for olefin polymerization, comprising titanium, magnesium, halogen, and an internal electron-donating compound, wherein the internal electron-donating compound comprises an electron-donating compound (i) having a phthalic acid ester structure, and an electron-donating compound (ii) having two or more kinds of groups selected from an ether group, an ester group and a carbonate group and having no phthalic acid ester structure, wherein a content ratio of the electron-donating compound (ii) having two or more kinds of groups selected from an ether group, an ester group and a carbonate group and having no phthalic acid ester structure is 0.5 to 1.5% by mass.
Abstract:
The titanium-based porous body according to the present invention is in a form of a sheet and contains titanium, and the titanium-based porous body has a thickness of 0.8 mm or less, a porosity of 30% to 65%, a maximum height Rz1 of one sheet surface of 30 μm or less, a ratio of a maximum height Rz2 of other sheet surface to the maximum height Rz1 of the one sheet surface (Rz2/Rz1) of 1.2 or more, and a compression deformation rate of 19% or less.
Abstract:
A method for producing a titanium foil according to the present invention includes an electrodeposition step of performing electrolysis with electrodes including an anode and a cathode using a molten salt bath comprising titanium ions and having at least one molten chloride to deposit metal titanium onto an electrolytic surface of the cathode, wherein the electrodeposition step includes maintaining a ratio of a molar concentration of titanium ions to the total molar concentration of metal ions in the molten salt bath at 7% or more, and maintaining a temperature of the molten salt bath at 510° C. or less, and conducting a current to the electrodes under conditions where a continuous stop time of current conduction is less than 1.0 second, a current density is 0.10 A/cm2 or more and 1.0 A/cm2 or less, and a time for electrodepositing the metal titanium onto the electrolytic surface of the cathode is 120 minutes or less.
Abstract:
A method for producing metal titanium by carrying out electrolysis using an anode and a cathode in a molten salt bath, the method using an anode containing metal titanium as the anode, the method comprising a titanium deposition step of depositing metal titanium on the cathode, wherein, in the titanium deposition step, a temperature of the molten salt bath is from 250° C. or more and 600° C. or less, and an average current density of the cathode in a period from the start to 30 minutes later of the titanium deposition step is maintained in a range of 0.01 A/cm2 to 0.09 A/cm2.
Abstract:
Provided is a molybdenum oxychloride characterized in having a purity of 99.9995 wt % or higher. Additionally provided is a manufacturing method of a molybdenum oxychloride including the steps of reacting MoO3 and Cl2 and synthesizing the molybdenum oxychloride in a reaction chamber, and cooling the synthesized molybdenum oxychloride gas and precipitating the molybdenum oxychloride in a recovery chamber, wherein an impurity trap is provided between the reaction chamber and the recovery chamber, and impurities are removed with the impurity trap. An object of the present invention is to provide a high-purity molybdenum oxychloride and a manufacturing method therefor.
Abstract:
A porous titanium-based sintered body, having a porosity of 45% to 65%, an average pore diameter of 5 μm to 15 μm, and a bending strength of 100 MPa or more. According to the present invention, a porous titanium-based sintered body having good pore diameter and porosity that are compatible with each other and having a high strength can be provided.