Abstract:
Refractory glass-forming tools, including glass-forming molds incorporating protective metal nitride surface coatings, with optional alumina barrier layers disposed between the mold bodies and coating for high-temperature nitride coating stability, offering particular advantages for the manufacture by direct molding of optically finished glass products such as information display cover glasses from refractory alkali aluminosilicate glasses at molding temperatures up to and above 800° C.
Abstract:
A process using a three-piece mold for making a three-dimensionally shaped glass article having a flat area and a curved/bend area is disclosed. The process includes placing a glass sheet on a mold having a shaping surface with a desired surface profile for the shaped glass article including a flat area and a bend area, moving a flat area plunger toward the glass sheet to compress the glass sheet, heating a portion of the glass sheet corresponding to an area above the bend area of the mold to a temperature above a forming temperature, and moving a bend area plunger toward the heated glass sheet to compress the heated glass sheet. A temperature of the glass sheet in the area above the bend area of the mold is higher than a temperature of the glass sheet in the area above the flat area of the mold when compressing the heated glass sheet with the bend area plunger.
Abstract:
A method of forming a shaped glass article includes placing a glass sheet on a mold such that a first glass area of the glass sheet corresponds to a first mold surface area of the mold and a second glass area of the glass sheet corresponds to a second mold surface area of the mold. The first glass area and the second glass area are heated such that the viscosity of the second glass area is 8 poise or more lower than the viscosity of the first glass area. A force is applied to the glass sheet to conform the glass sheet to the mold surface. During the heating of the second glass area, the first mold surface area is locally cooled to induce a thermal gradient on the mold.
Abstract:
A multi-layer coating for a glass-shaping mold is disclosed. The multi-layer coating may include a glass-contacting layer and a diffusion barrier layer. The glass-contacting layer may make contact with glass during glass-shaping and may include titanium oxide, aluminium oxide, or combinations thereof. The diffusion barrier layer may be positioned between the glass-contacting layer and a mold body and may restrict diffusion of base metals from the mold body to the glass-contacting layer and diffusion of glass materials from the glass-contacting layer to the mold body.
Abstract:
A glass-ceramic includes greater than or equal to 55 wt % to less than or equal to 75 wt % SiO2; greater than or equal to 2 wt % to less than or equal to 10 wt % Al2O3; greater than or equal to 8 wt % to less than or equal to 15 wt % Li2O; greater than or equal to 2 wt % to less than or equal to 4 wt % P2O5; greater than or equal to 0.05 wt % and less than or equal to 4.0 wt % CaO; greater than or equal to 5 wt % to less than or equal to 15 wt % ZrO2; and a phase assemblage comprising a crystalline phase and a glass phase, wherein: a ratio of Li2O to Al2O3 is greater than 2 and less than or equal to 4; and a ratio of Li2O to ZrO2 is greater than or equal to 1.2 and less than or equal to 1.7.
Abstract:
A lithium containing glass article is provided. In aspects, the lithium containing glass article includes an intensity coupling profile including a plurality of coupling resonances. A first of the coupling resonances has a half-width half-maximum value that is at least 1.8 times greater than the half-width half-maximum value of a second of the coupling resonances. In aspects, the lithium containing glass article includes a smoothed intensity coupling profile including a plurality of coupling resonances. A second derivative of the smoothed intensity coupling profile at a first of the coupling resonances is at least 1.8 times greater than a second derivative of the smoothed coupling profile at a second of the coupling resonances.
Abstract:
A cover article for a sensor is described herein that includes: a substrate comprising a thickness from 50 μm to 5000 μm, an outer primary surface, and an inner primary surface; and an outer layered film disposed on the outer primary surface. The substrate is a chemically-strengthened glass or glass-ceramic substrate. The cover article exhibits a first-surface average reflectance of less than 10% for wavelengths from 1000 nm to 1700 nm for at least one angle of incidence from 8° to 60°.
Abstract:
Articles are described that may include substrates having a major surface, the major surface comprising a first portion and a second portion. A first direction that is normal to the first portion of the major surface may not be equal to a second direction that is normal to the second portion of the major surface. The angle between the first direction and the second direction may be at least 15 degrees. An optical coating may be disposed on at least the first portion and the second portion of the major surface. The optical coating may form an antireflective surface.