Abstract:
The invention provides compositions, each comprising an ethylene/alpha-olefin interpolymer, which has a reduced level of a low density, low molecular weight oligomeric fraction, as indicated by an HCC value, as described herein, and reduced levels of inorganic content or lower Tm. The invention also provides processes for forming such interpolymers.
Abstract:
The present disclosure provides a composition comprising: a) a polypropylene; b) a polyolefin elastomer; and c) a block composite. The polyolefin elastomer has an I10/I2 from greater than 7.5 to 15.0. The composition may optionally include a filler.
Abstract translation:本公开提供了一种组合物,其包含:a)聚丙烯; b)聚烯烃弹性体; 和c)块复合材料。 聚烯烃弹性体具有大于7.5至15.0的I 10 / I 2。 组合物可以任选地包括填料。
Abstract:
The instant invention provides a composition suitable for stretch hood, method of producing the same, and articles made therefrom. The article according to the present invention comprises a multi-layer film according to the present invention has a thickness of at least 3 mils comprising at least one inner layer and two exterior layers, wherein the inner layer comprises at least 50 weight percent polyethylene copolymer having a melt index less than 2 grams/10 minutes, a density less than or equal to 0.910 g/cm3, a total heat of fusion less than 120 Joules/gram and a heat of fusion above 115° C. of less than 5 Joules/gram, the total heat of fusion of the inner layer less than the heat of fusion of either of the two exterior layers, and wherein the multi-layer film has an elastic recovery of at least 40% when stretched to 100% elongation.
Abstract:
The instant invention provides a composition suitable for stretch hood, method of producing the same, and articles made therefrom. The article according to the present invention comprises a multi-layer film according to the present invention has a thickness of at least 3 mils comprising at least one inner layer and two exterior layers, wherein the inner layer comprises at least 50 weight percent polyethylene copolymer having a melt index less than 2 grams/10 minutes, a density less than or equal to 0.910 g/cm3, a total heat of fusion less than 120 Joules/gram and a heat of fusion above 115° C. of less than 5 Joules/gram, the total heat of fusion of the inner layer less than the heat of fusion of either of the two exterior layers, and wherein the multi-layer film has an elastic recovery of at least 40% when stretched to 100% elongation.