Thermoplastic moulding compositions of ABS and hydrogenated nitrile
rubber
    62.
    发明授权
    Thermoplastic moulding compositions of ABS and hydrogenated nitrile rubber 失效
    ABS和氢化丁腈橡胶的热塑性成型组合物

    公开(公告)号:US4857591A

    公开(公告)日:1989-08-15

    申请号:US65024

    申请日:1987-06-22

    CPC分类号: C08L51/04 C08L55/02

    摘要: Thermoplastic moulding compositions consisting ofI. 75 to 99.5% by weight of a polymer ofA. 0 to 95% by weight, 95% or less by weight; of a graft copolymer prepared by grafting polymerization ofA.1 5 to 95% by weight of a mixture ofA.1.1 50 to 95% by weight of styrene, .alpha.-methylstyrene, nuclear-substituted styrene, methyl methacrylate or mixtures thereof andA.1.2 50 to 5% by weight of (meth)acrylonitrile, methyl methacrylate, maleic anhydride, N-substituted maleimide or mixtures thereof onA.2 95 to 5% by weight of a rubber with a glass transition temperature Tg or

    摘要翻译: 热塑性成型组合物由I组成,重量百分比为75%至99.5%的聚合物,重量百分比为重量百分比为95% 通过接枝A.1.5至95重量%的A.1.1 50至95重量%的苯乙烯,α-甲基苯乙烯,核取代的苯乙烯,甲基丙烯酸甲酯或其混合物的混合物和A.1.1的混合物制备的接枝共聚物 .1.2在A.2的95至5重量%的玻璃化转变温度Tg或0℃的橡胶中,50至5重量%的(甲基)丙烯腈,甲基丙烯酸甲酯,马来酸酐,N-取代的马来酰亚胺或其混合物 C.和B.100至5重量%的B.1的热塑性聚合物95至50重量%的苯乙烯,α-甲基苯乙烯,核取代的苯乙烯或甲基丙烯酸甲酯或其混合物,B.2-5至50 (甲基)丙烯腈,甲基丙烯酸甲酯,马来酸酐,N-取代的马来酰亚胺或其混合物的重量%。 25〜0.5重量%的氢化丁腈橡胶。

    Thermoplastic molding compounds of polyamide and hydrogenated nitrile
rubber
    65.
    发明授权
    Thermoplastic molding compounds of polyamide and hydrogenated nitrile rubber 失效
    聚酰胺和氢化丁腈橡胶的热塑性模塑料

    公开(公告)号:US5387647A

    公开(公告)日:1995-02-07

    申请号:US246555

    申请日:1994-05-19

    IPC分类号: C08L77/00

    CPC分类号: C08L77/00

    摘要: The invention relates to thermoplastic molding compounds of 70 to 99.5% by weight thermoplastic polyamides and 30 to 0.5% by weight hydrogenated nitrile rubber and 0 to 29.5% by weight thermoplastic resin components and, optionally, standard additives in typical quantities. These thermoplastic molding compounds show high strength values, very good moldability and, above all, high weathering resistance.

    摘要翻译: 本发明涉及70-99.5重量%热塑性聚酰胺和30- 0.5重量%氢化丁腈橡胶和0-29.5重量%热塑性树脂组分的热塑性模塑料,和任选的典型量的标准添加剂。 这些热塑性成型化合物显示出高强度值,非常好的成型性,最重要的是耐高温性。