SCRATCH RESISTANT GLASS AND METHOD OF MAKING

    公开(公告)号:US20220411324A1

    公开(公告)日:2022-12-29

    申请号:US17894693

    申请日:2022-08-24

    Abstract: Methods of manufacturing a glass-based article includes exposing a glass-based substrate having a lithium aluminosilicate composition to an ion exchange treatment to form the glass-based article. The ion exchange treatment including a molten salt bath having a concentration of a sodium salt in a range from 8 mol % to 100 mol %. The glass-based article includes sodium having a non-zero varying concentration extending from a surface of the glass-based article to a depth of the glass-based article The glass-based article has compressive stress layer extending from the surface to a spike depth of layer from 4 micrometers to 8 micrometers. The glass-based article includes a molar ratio of potassium oxide (K2O) to sodium oxide (Na2O) averaged over a distance from the surface to a depth of 0.4 micrometers that is greater than or equal to 0 and less than or equal to 1.8.

    Scratch resistant glass and method of making

    公开(公告)号:US11472733B2

    公开(公告)日:2022-10-18

    申请号:US16826473

    申请日:2020-03-23

    Abstract: Glass-based articles comprise stress profiles providing improved scratch resistance. A glass-based article comprises a lithium aluminosilicate composition and a molar ratio of potassium oxide (K2O) to sodium oxide (Na2O) averaged over a distance from the surface to a depth of 0.4 micrometers that is greater than or equal to 0 and less than or equal to 1.8. The article comprises sodium having a non-zero varying concentration extending from a surface of the glass-based article to a depth of the glass-based article and a spike depth of layer that is greater than or equal to 4 micrometers and less than or equal to 8 micrometers. The article may comprise an average compressive stress of greater than or equal to 150 MPa over a depth from 15 micrometers to 40 micrometers.

    Methods for reducing surface defects

    公开(公告)号:US11261129B2

    公开(公告)日:2022-03-01

    申请号:US16506116

    申请日:2019-07-09

    Abstract: Methods for reducing a defective area in a strengthened substrate to produce a non-defective substrate are provided. The methods include contacting a strengthened defective substrate with a heated salt bath containing at least one monovalent salt, and removing the strengthened substrate from the bath. The strengthened substrate, before being contacted with the salt bath, is a defective substrate having at least one defective area and one or more non-defective area. Upon removal from the salt bath, at least one defective area has been reduced or substantially removed to produce a non-defective substrate.

    Enclosures having an anti-fingerprint surface

    公开(公告)号:US11229131B2

    公开(公告)日:2022-01-18

    申请号:US15544630

    申请日:2016-01-19

    Abstract: Embodiments of an enclosure including a substrate having an anti-fingerprint surface are disclosed. The anti-fingerprint surface may include a textured surface, a coated surface or a coated textured surface that exhibits a low fingerprint visibility, when a fingerprint is applied to the anti-fingerprint surface. In one or more embodiments, the enclosure exhibits any one of the following attributes (1) radio, and microwave frequency transparency, as defined by a loss tangent of less than 0.03 and at a frequency range of between 15 MHz to 3.0 GHz; (2) infrared transparency; (3) a fracture toughness of greater than 0.6 MPa·m1/2; (4) a 4-point bend strength of greater than 350 MPa; (5) a Vickers hardness of at least 450 kgf/mm2 and a Vickers median/radial crack initiation threshold of at least 5 kgf; (6) a Young's Modulus in the range from about 50 GPa to about 100 GPa; and (7) a thermal conductivity of less than 2.0 W/m° C.