COMPOSITIONS PROVIDING FROST APPEARANCE FOR PRINTING ON GLASS OR CERAMIC SUBSTRATES AND METHODS FOR THE USE THEREOF
    1.
    发明申请
    COMPOSITIONS PROVIDING FROST APPEARANCE FOR PRINTING ON GLASS OR CERAMIC SUBSTRATES AND METHODS FOR THE USE THEREOF 有权
    提供玻璃或陶瓷基材印刷的外观的组合物及其使用方法

    公开(公告)号:US20130017388A1

    公开(公告)日:2013-01-17

    申请号:US13547543

    申请日:2012-07-12

    IPC分类号: C09D5/00 B32B17/00 C03C17/04

    摘要: A method of producing a substrate having a frosted appearance, an article having a frosted appearance and frost-imparting compositions are disclosed. The method includes applying a frost-imparting composition onto a ceramic substrate and firing the coated substrate above 400° C. to impart the frost appearance. The frost-imparting composition comprises a liquid vehicle, 20% to 90% by weight of glass frit particles and less than 10% by weight of at least one gas-releasing material, inactive below an activation temperature of at least 400° C. The gas releasing material may include carbonate, nitrate, iodate, bromate, chlorate, fluoride, manganate, dimanganate and sulfate compounds. The firing temperature is chosen to be above the activation temperature of the gas-releasing material, above which the gas-releasing material yields gas bubbles and above a temperature that causes the glass frit particles to behave as a viscous liquid.

    摘要翻译: 公开了一种具有磨砂外观的基材的制造方法,具有磨砂外观的物品和赋予霜的组合物。 该方法包括将施加霜剂的组合物施加到陶瓷基底上,并将涂覆的基底烧制在高于400℃以赋予霜状外观。 赋予霜的组合物包含液体载体,20重量%至90重量%的玻璃料颗粒和少于10重量%的至少一种气体释放材料,在至少400℃的活化温度下无活性。 气体释放材料可以包括碳酸盐,硝酸盐,碘酸盐,溴酸盐,氯酸盐,氟化物,锰酸盐,二高锰酸盐和硫酸盐化合物。 选择烧制温度高于气体释放材料的活化温度,在该温度之上,气体释放材料产生气泡并高于导致玻璃料颗粒表现为粘性液体的温度。

    Compositions providing frost appearance for printing on glass or ceramic substrates and methods for the use thereof
    3.
    发明授权
    Compositions providing frost appearance for printing on glass or ceramic substrates and methods for the use thereof 有权
    提供用于在玻璃或陶瓷基材上印刷的霜外观的组合物及其使用方法

    公开(公告)号:US09340448B2

    公开(公告)日:2016-05-17

    申请号:US13547543

    申请日:2012-07-12

    摘要: A method of producing a substrate having a frosted appearance, an article having a frosted appearance and frost-imparting compositions are disclosed. The method includes applying a frost-imparting composition onto a ceramic substrate and firing the coated substrate above 400° C. to impart the frost appearance. The frost-imparting composition comprises a liquid vehicle, 20% to 90% by weight of glass frit particles and less than 10% by weight of at least one gas-releasing material, inactive below an activation temperature of at least 400° C. The gas releasing material may include carbonate, nitrate, iodate, bromate, chlorate, fluoride, manganate, dimanganate and sulfate compounds. The firing temperature is chosen to be above the activation temperature of the gas-releasing material, above which the gas-releasing material yields gas bubbles and above a temperature that causes the glass frit particles to behave as a viscous liquid.

    摘要翻译: 公开了一种具有磨砂外观的基材的制造方法,具有磨砂外观的物品和赋予霜的组合物。 该方法包括将施加霜剂的组合物施加到陶瓷基底上,并将涂覆的基底烧制在高于400℃以赋予霜状外观。 赋予霜的组合物包含液体载体,20重量%至90重量%的玻璃料颗粒和少于10重量%的至少一种气体释放材料,在至少400℃的活化温度下无活性。 气体释放材料可以包括碳酸盐,硝酸盐,碘酸盐,溴酸盐,氯酸盐,氟化物,锰酸盐,二高锰酸盐和硫酸盐化合物。 选择烧制温度高于气体释放材料的活化温度,在该温度之上,气体释放材料产生气泡并高于导致玻璃料颗粒表现为粘性液体的温度。