Method and apparatus for bending and tempering glass plates
    1.
    发明授权
    Method and apparatus for bending and tempering glass plates 失效
    玻璃板弯曲和回火的方法和装置

    公开(公告)号:US4990170A

    公开(公告)日:1991-02-05

    申请号:US509163

    申请日:1990-04-16

    摘要: Glass plates are bent by discharging a glass plate from a suction plate onto a concave circumferential bending ring. Within the furnace (1) the glass plate is gripped by the suction plate (27) and is moved with the latter out of the furnace (1) into a combined bending and tempering station (10) and is discharged there onto the circumferential bending ring (19) located between two blowing boxes (11,13). Immediately following the discharge of the flass plate onto the circumferential bending ring (19), the suction plate (27) moves back to its starting position and the glass plate is tempered in this position.

    摘要翻译: 通过将玻璃板从吸盘排出到凹形周向弯曲环上而使玻璃板弯曲。 在炉(1)内,玻璃板被吸板(27)夹住,随后将玻璃板从炉(1)中移出到一个组合的弯曲和回火站(10)中,并被排放到周向弯曲环 (19)位于两个吹风箱(11,13)之间。 在将黄土板排放到周向弯曲环(19)上之后,吸板(28)立即移回其起始位置,玻璃板在该位置回火。

    Heat conditioning chamber
    2.
    发明授权
    Heat conditioning chamber 失效
    热调节室

    公开(公告)号:US5125948A

    公开(公告)日:1992-06-30

    申请号:US542595

    申请日:1990-06-25

    IPC分类号: C03B25/08

    CPC分类号: C03B25/08

    摘要: The invention relates to a heat conditioning chamber for controlled cooling following a high-temperature treatment of plane thin glass sheets, transported in horizontal position by a continuously driven roller conveyor. According to the invention, in the hottest zone in the chamber, the cooling is performed solely by absorption of radiation and continues in other zones by convection.

    摘要翻译: 本发明涉及一种用于在通过连续驱动的辊式输送机在水平位置运输的平面薄玻璃板的高温处理之后受控冷却的热调节室。 根据本发明,在室中最热的区域中,仅通过吸收辐射进行冷却,并且通过对流在其它区域中继续冷却。

    Apparatus for bending glass panes
    3.
    发明授权
    Apparatus for bending glass panes 失效
    用于弯曲玻璃窗的装置

    公开(公告)号:US5059235A

    公开(公告)日:1991-10-22

    申请号:US575487

    申请日:1990-08-30

    IPC分类号: C03B23/025 C03B23/03

    CPC分类号: C03B23/03 C03B23/0256

    摘要: In an apparatus for bending glass panes in a horizontal position, comprising an upper bending mold and a lower frame-shaped mold, the bending force exerted by the bending mold is determined by the self-weight of the bending mold. In order that a uniform pressure shall be exerted by the upper bending mold on the entire periphery of the lower frame-shaped mold, the upper bending is mounted displaceable on its guide rods relative to them in a vertical direction and variable in its angular position relative to the guide rods. To achieve the desired relief of weight of the bending mold, the guide rods are suspended by cables from a frame which can be lowered. On the frame, hydraulic or pneumatic cylinders are disposed, which each exert, via a pulling cable acting on a guide rod, an adjustable force in the opposite direction to the self-weight of the bending mold.

    摘要翻译: 在用于在水平位置弯曲玻璃板的装置中,包括上弯曲模具和下框架模具,弯曲模具施加的弯曲力由弯曲模具的自重决定。 为了通过上部弯曲模具在下部框架形模具的整个周边施加均匀的压力,上部弯曲部被安装在其导向件上相对于它们在垂直方向上移动并且相对于它们的角度位置可变 到导杆。 为了实现对弯曲模具的重量的期望的减轻,导杆通过电缆从可以降低的框架悬挂。 在框架上,设置液压或气动缸,每个缸通过作用在导向杆上的牵引缆线在与弯曲模具的自重相反的方向上发挥可调节的力。

    Method and apparatus for making contact-tempered glass sheets with
reinforced edge stresses
    4.
    发明授权
    Method and apparatus for making contact-tempered glass sheets with reinforced edge stresses 失效
    用于制造具有增强的边缘应力的接触钢化玻璃板的方法和装置

    公开(公告)号:US4826522A

    公开(公告)日:1989-05-02

    申请号:US150191

    申请日:1988-01-29

    摘要: The invention relates to the tempering of sheets of glass and optionally their bending by the so-called contact process. It proposes a process in which the edge stresses of the glass sheets are reinforced by cooling the edges of the glass sheets in relation to their central zone, particularly by blowing on these edges with a cooling gas. It also proposes a device to perform this preferred cooling of the edges, as well as glass sheets thus tempered. The invention applies to the production of glazings having nonfragile edges, particularly for the automobile.

    摘要翻译: 本发明涉及通过所谓的接触方法回火玻璃片和任选地其弯曲。 它提出了一种方法,其中玻璃板的边缘应力通过相对于其中心区域冷却玻璃板的边缘来加强,特别是通过用冷却气体吹在这些边缘上。 它还提出了一种用于对边缘进行优选冷却的装置,以及如此回火的玻璃板。 本发明适用于生产具有非易碎边缘的玻璃,特别是用于汽车。

    Process and apparatus for manufacturing a curved sheet of glass
    6.
    发明授权
    Process and apparatus for manufacturing a curved sheet of glass 失效
    用于制造弯曲玻璃板的方法和设备

    公开(公告)号:US4915722A

    公开(公告)日:1990-04-10

    申请号:US305705

    申请日:1989-02-03

    摘要: A process for bending a glass sheet, in particular one for motor vehicles, with curved areas having small radii of curvature. The bending device used is a bending press having a male type mold and a female type mold. The female type mold consists of at least two mold parts hinged together. After part of the glass sheet heated to bending temperature has been received by the bending press, at least one swivelling mold part of the female type mold is swivelled around the swivel axis, against the male type mold. An adjustable electric motor serves as the drive motor to move the swivelling mold parts. The angular velocity of the swivel action of the swivelling mold parts during the bending process is adjusted as a function of the temperature of the glass sheet and the desired degree of deformation.

    摘要翻译: 用于弯曲玻璃板,特别是用于机动车辆的玻璃板的弯曲区域具有小曲率半径的方法。 使用的弯曲装置是具有阳型模具和阴型模具的弯曲压力机。 阴型模具由铰链在一起的至少两个模具部件组成。 在加热到弯曲温度的玻璃板的一部分已经被弯曲压力机接收之后,阴型模具的至少一个旋转模具部分围绕旋转轴线旋转抵靠阳型模具。 可调电动机用作驱动电机以移动旋转模具部件。 在弯曲过程中旋转模具部件的旋转作用的角速度作为玻璃板的温度和所需的变形程度的函数被调整。

    Material for the tempering of glass
    8.
    发明授权
    Material for the tempering of glass 失效
    玻璃回火材料

    公开(公告)号:US5183491A

    公开(公告)日:1993-02-02

    申请号:US707947

    申请日:1991-05-28

    摘要: Disclosed is a material for a tempering process of glass plates utilizing a so-called contact process. It proposes a material with a base of an arrangement of thin metallic threads exhibiting a heat resistance on the order of 0.25.multidot.10.sup.-3 to 2.5.multidot.10.sup.-3 m.sup.2 .multidot.K.multidot.W.sup.-1 intended to be inserted between the cooling plates and the glass of a contact-tempering installation. The process makes it possible to temper glazings sufficiently so that they are used as automobile glazings and the durability of this thread-based material is compatible with an industrial usage.

    摘要翻译: 公开了一种利用所谓的接触方法进行玻璃板回火处理的材料。 它提出了一种具有薄金属线的布置基部的材料,其具有预期要插入在冷却板和接触回火装置的玻璃之间的0.25×10 -3至2.5×10 -3 m 2×K×W-1的数量级的耐热性 。 该工艺使得可以充分地回火玻璃以便它们被用作汽车玻璃,并且该线基材料的耐久性与工业用途相兼容。

    Bending furnace for glazings
    9.
    发明授权
    Bending furnace for glazings 失效
    弯曲的玻璃炉

    公开(公告)号:US5114454A

    公开(公告)日:1992-05-19

    申请号:US723566

    申请日:1991-07-01

    IPC分类号: C03B23/023 C03B23/03

    摘要: A bending furnace for glazings comprises several heating cells, a station for bending by pressing, at least one cooling cell and a system for intermittent transport of glazings. The glazings are laid on bending rings (2), mounted on mobile carriages (3), coupled to one another in a train. The train is pulled by a pulling machine installed at the end of the furnace and outside the latter. The point of application of the pulling machine which moves carriages (3) and the length of the travel of this pulling machine are controlled as a function of the temperature to take into account the variation of length of the train. The precise positioning of the carriage in the pressing station is obtained by a detector (27) joined to pivoting stops (28, 36).

    摘要翻译: 用于玻璃的弯曲炉包括几个加热单元,用于通过压制弯曲的工位,至少一个冷却单元和用于间歇运送玻璃的系统。 玻璃铺设在弯曲环(2)上,安装在移动托架(3)上,在列车中彼此耦合。 火车由安装在炉子末端的拉机拉出,并在炉外。 移动托架(3)的牵引机的应用点和该牵引机的行程长度作为温度的函数被控制,以考虑列车长度的变化。 通过与枢转止动件(28,36)连接的检测器(27)获得托架在加压站中的精确定位。