摘要:
The coarse-grain CTE of premium coke is reduced by increasing the nominal velocity of the volatile coking by-products in the coking drum to a higher level than the preexisting nominal velocity.
摘要:
A virgin heavy oil is hydrotreated, separated into a light fraction and a heavy fraction which are separately delay coked to obtain (a) a coke product of low sulfur content suitable for use as recarburizer coke or for use in the manufacture of graphite electrodes used in the manufacture of steel and (b) a coke product of higher sulfur content suitable for use in electrodes employed in the manufacture of aluminum.
摘要:
In a delayed premium coking process utilizing as feedstock an aromatic mineral oil having a high aromatic content and a low molecular weight, coke CTE is reduced and coke particle size is increased by sparging with a gas during the coking cycle.
摘要:
A method for reducing furnace fouling in a delayed coking process comprising (a) supplying at least one feed to a delayed coking unit comprised of coker furnace, at least two coke drums and a coker fractionator, (b) increasing the aromaticity of the feed to produce a modified stream by combining with the feed upstream of the coker furnace at least one added stream selected from the group consisting of an aromatic gas oil, a hydrotreated aromatic gas oil and combinations thereof, (c) introducing the modified feed stream into the coker furnace, d) heating the modified feed stream to a coking temperature in the coker furnace to produce a heated modified stream, and e) transferring the heated modified stream from the coker furnace to a coke drum.
摘要:
A polyamide composition comprising the following recurring units: ##STR1## in proportions such that the mole ratio of the dicarboxylic acid moieties in the A, B and C units is about 49.5-0.5/0-20/0.5-49.5 and wherein R is a divalent radical comprising ##STR2## in a mole ratio of about 0.5-50/49.5-0 and preferably having a glass transition temperature of 90.degree. C. or greater and an oxygen transmission rate of about 2.0 cc-mil/100 in.sup.2 -day-atm or less.
摘要:
In a delayed premium coking process the particle size of the premium coke is increased by the addition of a Lewis acid such as aluminum chloride to the coking process. Preferably the aluminum chloride is added during the latter part of the coking cycle.
摘要:
A heavy high-sulfur hydrocarbonaceous feedstock is partially delayed coked and partially formcoked. The coke products are screened, with larger particles being calcined at desulfurizing temperatures and smaller particles being recycled to the formcoker. Overhead products from both coking operations are combined, fractionated, and desulfurized. The heaviest cut from the fractionator is combined with the feedstock as recycle.
摘要:
More uniform premium coke is obtained in a delayed coking process by oxygenating the latter portion of the premium coking feed introduced to the coking drum.
摘要:
Plastic bottles and a process for producing same in which at least one layer comprises a polyamide composition comprising isophthalic acid, terephthalic acid, adipic acid, metaxylylenediamine and hexamethylenediamine moieties in a molar ratio of about 49.5-0.5/0-20/0.5-49.5/0.5-50/49.5-0.
摘要:
Properties of premium coke are improved by coking the feed at a temperature lower than the normal coking temperature and thereafter subjecting the coke to a heat soak at substantially the same temperature as the temperature at which the coke was formed.