Abstract:
The invention is related to compositions suitable for the fabrication of pipes, and other articles, with excellent performance properties. The invention provides a composition, comprising a blend, wherein said blend comprises a high molecular weight ethylene-based interpolymer and a low molecular weight ethylene-based interpolymer, and the high molecular weight ethylene-based interpolymer is a heterogeneously branched linear or a homogeneously branched linear ethylene-based interpolymer, and has a density from 0.922 g/cc to 0.929 g/cc, and a high load melt index (I21) from 0.2 g/10 min to 1.0 g/10 min, and the low molecular weight ethylene-based interpolymer is heterogeneously branched linear or a homogeneously branched linear ethylene-based interpolymer, and has a density from 0.940 g/cc to 0.955 g/cc, and a melt index (I2) from 6 g/10 min to 50 g/10 min. The blend has a single peak in an ATREF profile eluting above 30° C., and has a coefficient of viscosity average molecular weight (CM?) less than −0.0032 in the log(calculated Mv) versus elution temperature, said CMv calculated in the range of elution temperatures from 70° C. to 90° C. The Mv is the viscosity average molecular weight.
Abstract:
The invention provides a process for extruding a composition, comprising at least one polymer, through a die, comprising applying at least one processing additive (PA) onto at least one surface of the die, and extruding the composition through the die, and wherein the processing additive is applied to the die as a solution. The invention also provides a composition comprising at least one processing additive (PA), and a solvent or a solvent mixture.
Abstract:
A polymer composition comprises a low-molecular-weight (LMW) ethylene polymer component and a high-molecular-weight (HMW) ethylene polymer component coupled with a polysulfonyl azide. Preferably, the LMW polyethylene component and the HMW polyethylene component co-crystallize in the composition such that it exhibits a single or substantially single peak in a lamella thickness distribution (LTD) curve. The ethylene polymer for the LMW and the HMW polyethylene components can be either homopolymer or ethylene copolymer. Preferably, both components are an ethylene copolymer of the same, or different, composition (that is, with the same or different comonomers). A method of making a pipe that includes selecting a polymer composition having a substantially single peak in the LTD curve is described. Compositions comprising a chromium-catalyzed ethylene polymer, coupled with a polysulfonyl azide are also described herein.
Abstract:
A fugitive pattern for making a shell mold for investment casting a metal or alloy comprises a substantially random interpolymer and a low molecular weight polymer in proportions to provide a fugitive pattern having a combination of properties suitable for use in making the shell molds.
Abstract:
This invention includes catalysts comprising rhenium (atomic number 75), nickel, cobalt, boron and copper and/or ruthenium impregnated on a support material and a process for preparing said catalyst, said process comprising (i) impregnating a mixture of metals comprising rhenium, cobalt, copper and/or ruthenium, boron and nickel on a support material selected from the group consisting of alpha-alumina, silica, silica-alumina, kiesolguhrs or diatomaceous earths, and silica-titanias; and (ii) activating said catalyst by heating the catalyst in the presence of hydrogen at an effective temperature preferably in the range of about 150.degree. C. to about 500.degree. C. for a sufficient period preferably of from about 30 minutes to about 6 hours. A further feature of the present invention is a method for producing amine products by the catalytic amination of alkane or arylalkane derivatives including epoxides, monols, diols, polyethers, polyols, alcoholamines, ketones, imino compounds iminoalcohols, ether alcohols, and mixtures thereof, said process comprising contacting said lower alkane or arylalkane derivatives with ammonia and/or reactant amine at an effective temperature preferably from 150.degree. C. to about 500.degree. C. and in the presence of hydrogen and the nickel-rhenium-cobalt-boron-copper and/or ruthenium catalyst as described hereinabove.
Abstract:
Sulfur dioxide is removed from a fluid containing SO.sub.2 by employing as an absorbent therefor an aqueous solution of compounds represented by Formulas I and II: ##STR1## wherein each R.sup.1 or R.sup.2 is independently hydrogen; an alkyl group; a hydroxyalkyl group; an aldehyde group; a carboxylic acid or salt group; an alkyl group containing at least one carboxylic ester, carboxylic acid or salt, ether, aldehyde, ketone or sulfoxide; and wherein at least one R.sup.1 or R.sup.2 is a carbonyl-containing group, such as an aldehyde group, a carboxylic acid containing group, a carboxyl ester group, or a ketone-containing group; ##STR2## wherein each R.sup.3 is independently hydrogen; an alkyl group; a hydroxyalkyl group; an aldehyde group; a carboxylic acid or salt group; or an alkyl, aryl, or aralkyl group containing at least one carboxylic ester, a carboxylic acid or salt, ether, aldehyde, ketones or sulfoxide group. The absorbent solution preferably can be thermally regenerated by heating to remove SO.sub.2.
Abstract:
A continuous process for removing hydrogen sulfide from a gas stream by contacting the gas stream with a solution of ammonium hydroxide to produce an effluent liquid stream comprising ammonium sulfide which is fed to a heating zone maintained at least at the boiling temperature of said solution and supplied with an oxygen containing gas sparge wherein ammonia and hydrogen sulfide are removed from said zone as vapor and sulfur is removed from said zone as an aqueous dispersion, the sulfur being separated in a filtration zone from the residual aqueous liquid which is recycled back to a contact zone together with said ammonia and said hydrogen sulfide vapor.
Abstract:
The invention is related to compositions suitable for the fabrication of pipes, and other articles, with excellent performance properties. The invention provides a composition, comprising a blend, wherein said blend comprises a high molecular weight ethylene-based interpolymer and a low molecular weight ethylene-based interpolymer, and the high molecular weight ethylene-based interpolymer is a heterogeneously branched linear or a homogeneously branched linear ethylene-based interpolymer, and has a density from 0.922 g/cc to 0.929 g/cc, and a high load melt index (I21) from 0.2 g/10 min to 1.0 g/10 min, and the low molecular weight ethylene-based interpolymer is heterogeneously branched linear or a homogeneously branched linear ethylene-based interpolymer, and has a density from 0.940 g/cc to 0.955 g/cc, and a melt index (I2) from 6 g/10 min to 50 g/10 min. The blend has a single peak in an ATREF profile eluting above 30° C., and has a coefficient of viscosity average molecular weight (CM?) less than −0.0032 in the log(calculated Mv) versus elution temperature, said CMv calculated in the range of elution temperatures from 70° C. to 90° C. The Mv is the viscosity average molecular weight.
Abstract:
A blend composition (and fabricated articles therefrom) comprising; (A) one or more alkenyl aromatic polymers; (B) one or more substantially random interpolymers comprising (1) polymer units derived from; (a) at least one vinyl or vinylidene aromatic monomer, or (b) at least one hindered aliphatic or cycloaliphatic vinyl or vinylidene monomer, or (c) a combination of at least one aromatic vinyl or vinylidene monomer and at least one hindered aliphatic or cycloaliphatic vinyl or vinylidene monomer, and (2) polymer units derived from at least one of ethylene and/or a C3-20 &agr;-olefin; and (3) polymer units derived from one or more of ethylenically unsaturated polymerizable monomers other than those derived from (1) and (2); and, (C) one or more compatibilizers; and wherein said blend has; a) a tensile strength greater than 1500 psi; b) a pull force test (⅛″ diameter) greater than 15 lb; c) a Shore A Hardness greater than 79; d) a cycle time in injection molding of less than 30 sec.
Abstract:
This invention includes catalysts comprising rhenium (atomic number 75), nickel, cobalt, boron and copper and/or ruthenium impregnated on a support material and a process for preparing said catalyst, said process comprising (i) impregnating a mixture of metals comprising rhenium, cobalt, copper and/or ruthenium, boron and nickel on a support material selected from the group consisting of alpha-alumina, silica, silica-alumina, kieselguhrs or diatomaceous earths, and silica-titanias; and (ii) activating said catalyst by heating the catalyst in the presence of hydrogen at an effective temperature preferably in the range of about 150.degree. C. to about 500.degree. C. for a sufficient period preferably of from about 30 minutes to about 6 hours. A further feature of the present invention is a method for producing amine products by the catalytic amination of alkane or arylalkane derivatives including epoxides, monols, diols, polyethers, polyols, alcoholamines, ketones, imino compounds iminoalcohols, ether alcohols, and mixtures thereof, said process comprising contacting said lower alkane or arylalkane derivatives with ammonia and/or reactant amine at an effective temperature preferably from 150.degree. C. to about 500.degree. C. and in the presence of hydrogen and the nickel-rhenium-cobalt-boron-copper and/or ruthenium catalyst as described hereinabove.