Active material for positive electrode used in lithium secondary battery and method of manufacturing same
    2.
    发明授权
    Active material for positive electrode used in lithium secondary battery and method of manufacturing same 有权
    用于锂二次电池的正极活性物质及其制造方法

    公开(公告)号:US06210834B1

    公开(公告)日:2001-04-03

    申请号:US09306345

    申请日:1999-05-06

    IPC分类号: H01M452

    摘要: Disclosed is active material for a positive electrode used in lithium secondary batteries of Formula 1 below and a method of manufacturing the active material. The active material includes large particles of 1 to 25 &mgr;m formed of a plurality of minute particles of 0.4 to 0.7 &mgr;m. The method includes the steps of adding a chelating agent to a mixture derived by dissolving lithium salt, nickel salt and cobalt salt in a solvent to a molar ratio of 0.95-1.06: 0.5-1:0-0.5; producing a gel by heating the mixture; for precursor by thermally decomposing the gel; and heat treating the precursor. LixNi1−yCoyO2  [Formula 1] where x is between 0.95 and 1.06, and y is between 0 and 0.5.

    摘要翻译: 公开了下述式1的锂二次电池中使用的正极活性物质和活性物质的制造方法。 活性物质包括由0.4〜0.7μm的多个微小颗粒形成的1〜25μm的大颗粒。 该方法包括以下步骤:向溶解有锂盐,镍盐和钴盐的混合物中加入螯合剂至摩尔比为0.95-1.06:0.5-1:0-0.5; 通过加热混合物产生凝胶; 用于通过热分解凝胶的前体; 并对前体进行热处理,其中x在0.95和1.06之间,y在0和0.5之间。

    Positive active material for rechargeable lithium battery and method of preparing same
    5.
    发明授权
    Positive active material for rechargeable lithium battery and method of preparing same 有权
    可充电锂电池的正极活性物质及其制备方法

    公开(公告)号:US06183911B2

    公开(公告)日:2001-02-06

    申请号:US09429259

    申请日:1999-10-29

    IPC分类号: H01M450

    CPC分类号: H01M4/505 H01M4/581

    摘要: A positive active material for rechargeable lithium batteries includes an active material component processed from a manganese-based compound. The transition metal compound is selected from LixMnO2, LixMnF2, LixMnS2, LixMnO2-zFz, LixMnO2-xSz, LixMn1-yMyO2, LixMn1-yMyF2, LixMn1-yMyS2, LixMn1-yMyO2-zFz, LixMn1-yMyO2-zSz, LixMn2O4, LixMn2F4, LixMn2S4, LixMn2O4-zFz, LixMn2O4-zSz, LixMn2-yMyO4, LixMn2-yMyF4, LixMn2-yMyS4, LixMn2-yMyO4-zFz, or LixMn2-yMyO4-zSz where O

    摘要翻译: 用于可再充电锂电池的正极活性材料包括从锰基化合物加工的活性材料组分。 过渡金属化合物选自LixMnO2,LixMnF2,LixMnS2,LixMnO2-zFz,LixMnO2-xSz,LixMn1-yMyO2,LixMn1-yMyF2,LixMn1-yMyS2,LixMn1-yMyO2-zFz,LixMn1-yMyO2-zSz,LixMn2O4,LixMn2F4,LixMn2S4 ,LixMn2O4-zFz,LixMn2O4-zSz,LixMn2-yMyO4,LixMn2-yMyF4,LixMn2-yMyS4,LixMn2-yMyO4-zFz或LixMn2-yMyO4-zSz,其中O

    Method for fabricating porous composite oxide
    8.
    发明授权
    Method for fabricating porous composite oxide 失效
    多孔复合氧化物的制造方法

    公开(公告)号:US5962352A

    公开(公告)日:1999-10-05

    申请号:US890766

    申请日:1997-07-11

    摘要: A method for fabricating a porous composite oxide is provided. The method includes the steps of: (a) slowly mixing a solution including a silicon oxide source and a solution including an aluminum oxide source; (b) adding hydrochloric acid to the mixed solution prepared in said step (a) to obtain a sol; and (c) adding sodium hydroxide to said sol, reacting the obtained resultant at room temperature for 30 minutes to 12 hours, and drying the resultant. The porous composite oxide has an abundance of fine pores and the distribution of pore size is relatively uniform, so that the porous composite oxide is suitable for a carrier.

    摘要翻译: 提供一种制造多孔复合氧化物的方法。 该方法包括以下步骤:(a)缓慢混合包含氧化硅源和包含氧化铝源的溶液的溶液; (b)向所述步骤(a)中制备的混合溶液中加入盐酸以获得溶胶; 和(c)向所述溶胶中加入氢氧化钠,使所得产物在室温下反应30分钟至12小时,并干燥所得物。 多孔复合氧化物具有丰富的细孔,孔径分布相对均匀,使多孔复合氧化物适用于载体。

    Positive active material for lithium secondary batteries and method of preparing the same
    10.
    发明授权
    Positive active material for lithium secondary batteries and method of preparing the same 有权
    锂二次电池用正极活性物质及其制备方法

    公开(公告)号:US06749965B1

    公开(公告)日:2004-06-15

    申请号:US09595075

    申请日:2000-06-16

    IPC分类号: H01M440

    摘要: Disclosed is a positive active material for a lithium secondary battery having high capacity and long durability properties and particularly to a powder of LiaNi1-x-yC OxMyO2, LiaNi1-x-yC OxMyO2-zFz or LiaNi1-x-yC OxMyO2-zSz (where M is a metal selected from the group consisting of Al, Mg, Sr, La, Ce, V, and Ti and wherein 0≦0.99, 0.01≦y≦0.1, 0.01≦z≦0.1, and 1.00≦a≦1.1) is surface-treated by a metal alkoxide solution whereby the durability, capacity and structural safety of said positive active material is increased.

    摘要翻译: 公开了具有高容量和长的耐久性的锂二次电池的正极活性材料,特别是对于LiaNi1-x-yC OxMyO2,LiaNi1-x-yC OxMyO2-zFz或LiaNi1-x-yC OxMyO2-zSz的粉末(其中 M是选自Al,Mg,Sr,La,Ce,V和Ti的金属,其中0 <=0.99,0.01≤y≤0.1,0.01≤z≤0.1, = a <= 1.1)由金属醇盐溶液进行表面处理,由此提高所述正极活性物质的耐久性,容量和结构安全性。