Liquid-phase diffusion bonding alloy foils for joining heat-resistant
metals in oxidizing atmospheres
    1.
    发明授权
    Liquid-phase diffusion bonding alloy foils for joining heat-resistant metals in oxidizing atmospheres 失效
    用于在氧化性气氛中接合耐热金属的液相扩散接合合金箔

    公开(公告)号:US5759300A

    公开(公告)日:1998-06-02

    申请号:US716314

    申请日:1996-09-27

    摘要: Alloy foils for liquid-phase diffusion bonding of heat-resisting metals in an oxidizing atmosphere comprise 6.0 to 15.0 percent silicon, 0.1 to 2.0 percent manganese, 0.50 to 30.0 percent chromium, 0.10 to 5.0 percent molybdenum, 0.50 to 10.0 percent vanadium, 0.02 to 1.0 percent niobium, 0.10 to 5.0 percent tungsten, 0.01 to 0.5 percent nitrogen, 0.10 to 5.0 percent boron, plus 0.005 to 1.0 percent carbon, and/or either or both of 0.01 to 5.0 percent titanium and 0.01 to 5.0 percent zirconium, all by mass, with the balance comprising nickel and impurities, and have a thickness of 3.0 to 300 .mu.m. Alloy foils for liquid-phase diffusion bonding of heat-resisting metals in an oxidizing atmosphere are also available with substantially vitreous structures.

    摘要翻译: PCT No.PCT / JP95 / 00594 Sec。 371日期1996年9月27日第 102(e)1996年9月27日PCT 1995年3月29日PCT PCT。 出版物WO95 / 26419 日期:1995年10月5日耐热金属在氧化性气氛中的液相扩散接合用合金箔包含6.0〜15.0%的硅,0.1〜2.0%的锰,0.50〜30.0%的铬,0.10〜5.0%的钼,0.50〜10.0 0.01-0.0%的铌,0.10〜5.0%的钨,0.01〜0.5%的氮,0.10〜5.0%的硼,0.005〜1.0%的碳,和/或0.01〜5.0%的钛和0.01〜5.0 百分比的锆,质量均匀,余量包括镍和杂质,并且具有3.0至300μm的厚度。 用于在氧化气氛中耐热金属的液相扩散接合的合金箔也可用于基本上玻璃质结构。

    Liquid-phase diffusion bonding alloy foils for joining heat-resistant
metals in oxidizing atmospheres
    2.
    发明授权
    Liquid-phase diffusion bonding alloy foils for joining heat-resistant metals in oxidizing atmospheres 失效
    用于在氧化性气氛中接合耐热金属的液相扩散接合合金箔

    公开(公告)号:US5683822A

    公开(公告)日:1997-11-04

    申请号:US716183

    申请日:1996-09-27

    摘要: Alloy foils for liquid-phase diffusion bonding of heat-resisting metals in an oxidizing atmosphere comprise 6.0 to 15.0 percent silicon, 0.1 to 2.0 percent manganese, 0.50 to 30.0 percent chromium, 0.10 to 5.0 percent molybdenum, 0.50 to 10.0 percent vanadium, 0.02 to 1.0 percent niobium, 0.10 to 5.0 percent tungsten, 0.05 to 2.0 percent nitrogen, 0.50 to 20.0 percent phosphorus, plus 0.005 to 1.0 percent carbon, and/or either or both of 0.01 to 5.0 percent titanium and 0.01 to 5.0 percent zirconium, all by mass, with the balance comprising nickel and impurities, and have a thickness of 3.0 to 300 .mu.m. Alloy foils for liquid-phase diffusion bonding of heat-resisting metals in an oxidizing atmosphere are also available with substantially vitreous structures.

    摘要翻译: PCT No.PCT / JP95 / 00673 Sec。 371日期1996年9月27日第 102(e)日期1996年9月27日PCT提交1995年4月6日PCT公布。 公开号WO95 / 27586 日期:1995年10月19日在氧化气氛中耐热金属的液相扩散接合用合金箔包含6.0〜15.0%的硅,0.1〜2.0%的锰,0.50〜30.0%的铬,0.10〜5.0%的钼,0.50〜10.0 的钒,0.02〜1.0%的铌,0.10〜5.0%的钨,0.05〜2.0%的氮,0.50〜20.0%的磷,0.005〜1.0%的碳,和/或0.01〜5.0%的钛和0.01〜5.0 百分比的锆,质量均匀,余量包括镍和杂质,并且具有3.0至300μm的厚度。 用于在氧化气氛中耐热金属的液相扩散接合的合金箔也可用于基本上玻璃质结构。