摘要: A process is provided for extruding a bimodal polyethylene resin. The process includes providing a polyethylene homopolymer or copolymer resin having a bimodal molecular weight distribution; conveying the resin through an extruder having a feed zone in which the resin is not melted, a melt-mixing zone in which at least a portion of the resin is melted, and a melt zone in which the resin is in a molten state, each zone being partially filled with the resin; and contacting the molten resin in the melt zone with a gas mixture of 8 to 40% by volume O2. The resin can be further pelletized. The oxygen-tailored resin can be used to make polyethylene films having improved bubble stability.
摘要翻译: 提供了挤出双峰聚乙烯树脂的方法。 该方法包括提供具有双峰分子量分布的聚乙烯均聚物或共聚物树脂; 将树脂输送通过具有未熔融树脂的进料区域的挤出机,至少部分树脂熔融的熔融混合区域和树脂处于熔融状态的熔融区域 部分地填充有树脂; 并使熔融区中的熔融树脂与8至40体积%O 2的气体混合物接触。 树脂可进一步造粒。 氧气调整树脂可用于制备具有改善气泡稳定性的聚乙烯膜。