Thermally fused integral ferrule and its manufacturing method, and fiber array manufacturing method
    1.
    发明授权
    Thermally fused integral ferrule and its manufacturing method, and fiber array manufacturing method 有权
    热熔整体套管及其制造方法,以及光纤阵列的制造方法

    公开(公告)号:US06519406B1

    公开(公告)日:2003-02-11

    申请号:US09217507

    申请日:1998-12-21

    IPC分类号: G02B600

    摘要: There is provided a thermally fused integral ferrule in which a first glass substrate is at least partly unitarily combined with a second glass substrates by means of thermal fusion. The first glass substrate includes optical-fiber fixing V-shaped grooves on its side opposed to the second glass substrate, and also includes on the optical-fiber fixing V-shaped grooves in the first glass substrate, a guide section having a predetermined void between the first and second glass substrates. The thermally fused integral ferrule is manufactured by contacting the surface to be thermally fused of the first glass substrate in which the optical-fiber fixing V-shaped grooves are formed, with the surface to be thermally fused of the second glass substrate, followed by thermal fusion of the surfaces of the first and second glass substrates at a temperature of (Tg1−100) to (Tg2+150)° C. (where Tg1 is the glass transition temperature of one of the first and second glass substrates that is higher than that of the other and Tg2 is the lower glass transition temperature).

    摘要翻译: 提供了一种热熔融整体式套圈,其中通过热熔融将第一玻璃基板与第二玻璃基板至少部分地整体结合。 第一玻璃基板在其与第二玻璃基板相对的一侧包括光纤固定V形槽,并且还包括在第一玻璃基板中的光纤固定V形槽上,引导部分之间具有预定的空隙 第一和第二玻璃基板。 通过将形成有光纤固定V形槽的第一玻璃基板的热熔接表面与第二玻璃基板的热熔合表面接触,制成热熔融整体式套圈,然后进行热 在(Tg1-100)至(Tg2 + 150)℃的温度下熔融第一和第二玻璃基板的表面(其中Tg1是第一和第二玻璃基板之一的玻璃化转变温度高于 另一个和Tg2是较低的玻璃化转变温度)。

    Heat-fused unitary ferrule and method for producing the same
    2.
    发明授权
    Heat-fused unitary ferrule and method for producing the same 失效
    热熔合单体套管及其制造方法

    公开(公告)号:US6103344A

    公开(公告)日:2000-08-15

    申请号:US4567

    申请日:1998-01-08

    摘要: A heat-fused unitary ferrule includes a first glass substrate and a second glass substrate. The first glass substrate and the second glass substrate are unitarily joined by heat-fusion. A method for producing a heat-fused unitary ferrule includes the steps of: bringing a surface to be heat-fused of the first glass substrate having a groove for fixing an optical fiber into contact with a surface to be heat-fused of the second glass substrate; and subjecting the first and second glass substrates to heat-fusion at a temperature ranging from (Tg1-100).degree. C. to (Tg2+150).degree. C. (Tg1 denotes the higher glass transition temperature, and Tg2 denotes the lower glass transition temperature of the first and second glass substrates).

    摘要翻译: 热熔合单体套圈包括第一玻璃基板和第二玻璃基板。 第一玻璃基板和第二玻璃基板通过热熔接一体接合。 一种热熔融整体式套管的制造方法,其特征在于,具备将具有用于固定光纤的槽的第一玻璃基板的被热熔接的表面与第二玻璃的热熔接面接触 基质; 并使第一玻璃基板和第二玻璃基板在(Tg1〜100℃)〜(Tg2 + 150)℃的范围内进行热熔融(Tg1表示较高的玻璃化转变温度,Tg2表示较低的玻璃化转变温度 第一和第二玻璃基板的温度)。

    Press-forming die for glass elements
    3.
    发明授权
    Press-forming die for glass elements 有权
    用于玻璃元件的成型模具

    公开(公告)号:US06354111B1

    公开(公告)日:2002-03-12

    申请号:US09211081

    申请日:1998-12-14

    IPC分类号: C03B1106

    摘要: A platinum thin film having a thickness of 0.01 to 5 &mgr;m is formed by means of the sputtering method on a press face of a die based on the use of a cemented carbide base material. A nickel thin film having a thickness of 0.05 to 0.5 &mgr;m and a thin film made of an alloy of platinum and iridium are allowed to intervene between the cemented carbide base material and the platinum thin film, if necessary. Alternatively, an alloy thin film having a thickness of 0.01 to 5 &mgr;m, which contains 10 to 70% by weight of iridium and 30 to 90% by weight of one or more species of metals selected from metals of the platinum group except for iridium, may be allowed to intervene between the cemented carbide base material and the platinum thin film.

    摘要翻译: 基于使用硬质合金基材,通过溅射法在模具的压制面上形成厚度为0.01〜5μm的铂薄膜。 如果需要,可以将厚度为0.05至0.5μm的镍薄膜和由铂和铱的合金制成的薄膜插入硬质合金基体材料和铂薄膜之间。 或者,可以使用厚度为0.01〜5μm的合金薄膜,其含有10〜70重量%的铱和30〜90重量%的选自铂族除了铱的金属的一种或多种金属, 可以允许介入硬质合金基体材料和铂薄膜之间。

    Glass material and glass ceramic product
    4.
    发明授权
    Glass material and glass ceramic product 有权
    玻璃材料和玻璃陶瓷制品

    公开(公告)号:US06689704B2

    公开(公告)日:2004-02-10

    申请号:US09821791

    申请日:2001-03-29

    IPC分类号: C03C1012

    摘要: A SiO2—Al2O3—Li2O component-based glass material, which comprises, as basic components, SiO2: 60-63 wt %; Al2O3: 23-25 wt %; and Li2O: 4-5 wt % and, as modifying components, ZrO2: 1.5-2.5 wt %; TiO2: 0.5-2.5 wt %; MgO: 0.5-1.5 wt %; ZnO: 0.5-1.2 wt %; Na2O: 0.5-2.0 wt %; and K2O: 0.5-2.0 wt %, and further comprises any one of BaO: 0.5-1.0 wt, CaO: 1.0-2.0 wt %, and B2O3: 0.01-1.0 wt %. This can be reheat-formed in a glass state and has a low thermal expansion coefficient.

    摘要翻译: 作为基本成分的SiO 2·Al 2 O 3·Li 2 O成分为基础的玻璃材料为SiO 2:60〜63重量% Al2O3:23-25重量% 和Li 2 O:4-5重量%,作为改性成分,ZrO 2:1.5〜2.5重量% TiO 2:0.5〜2.5重量% MgO:0.5〜1.5重量% ZnO:0.5-1.2重量% Na2O:0.5-2.0重量% K2O:0.5〜2.0重量%,进一步含有BaO:0.5〜1.0重量%,CaO:1.0〜2.0重量%,B 2 O 3:0.01〜1.0重量%。 这可以在玻璃状态下重新加热并具有低的热膨胀系数。

    Optical fiber array
    5.
    发明授权
    Optical fiber array 有权
    光纤阵列

    公开(公告)号:US06215945B1

    公开(公告)日:2001-04-10

    申请号:US09276298

    申请日:1999-03-25

    IPC分类号: G02B600

    摘要: An optical fiber array includes an upper substrate and a lower substrate in which V-shaped grooves are formed, optical fibers being inserted and arranged in the V-shaped grooves. The tips of a plurality of protruding portions formed between the plurality of V-shaped grooves are shaped like planes. The optical fiber array can prevent optical fibers from being damaged or cut while preventing substrates from being cut when the fibers are placed in V-shaped grooves for alignment.

    摘要翻译: 光纤阵列包括上基板和下基板,其中形成有V形槽,光纤被插入并布置在V形槽中。 形成在多个V形槽之间的多个突出部分的尖端成形为类似的平面。 光纤阵列可以防止光纤被损坏或切割,同时防止当纤维放置在V形槽中进行对准时基板被切割。

    Glass substrate and two-stage molding method therefor
    6.
    发明授权
    Glass substrate and two-stage molding method therefor 失效
    玻璃基板及其两段成型方法

    公开(公告)号:US06321020B1

    公开(公告)日:2001-11-20

    申请号:US09277491

    申请日:1999-03-26

    IPC分类号: G02B636

    摘要: There is provided a glass substrate having a V-groove portion for arranging an optical fiber core and a countersunk portion for containing an optical fiber coated portion, formed on the extension of the V-groove portion, on the surface thereof. The surface roughness of an inside side face of the countersunk portion is 1 &mgr;m or less in Rmax, or 0.2 &mgr;m or less in Ra at least at the connecting portion of the V-groove portion and the countersunk portion. The glass substrate is manufactured by a two-stage molding method in which a first molding step for forming a concave portion in the surface of a glass substrate molded body by grinding or pressing, and a second molding step for pressing the glass substrate molded body obtained by the first molding step from the top and bottom surfaces while reheating the molded body are performed.

    摘要翻译: 提供一种玻璃基板,其具有用于布置光纤芯的V形槽部分和用于容纳形成在V形槽部分的延伸部上的光纤涂覆部分的埋头部分。 锪孔部的内侧面的表面粗糙度在Rmax为1um以下,至少在V槽部和埋头部的连接部分为Ra为0.2μm以下。 玻璃基板通过两阶段成型方法制造,其中通过研磨或压制在玻璃基板成型体的表面形成凹部的第一成型步骤和用于挤压所获得的玻璃基板成型体的第二成型步骤 通过从顶部和底部表面的第一模制步骤,同时重新加热成型体。

    Die and production method thereof, glass substrate and production method thereof and method of forming pattern on the glass substrate
    7.
    发明授权
    Die and production method thereof, glass substrate and production method thereof and method of forming pattern on the glass substrate 有权
    模具及其制造方法,玻璃基板及其制造方法以及在玻璃基板上形成图案的方法

    公开(公告)号:US06379777B1

    公开(公告)日:2002-04-30

    申请号:US09367729

    申请日:1999-11-02

    IPC分类号: B32B300

    摘要: On the pressing surface of a die, a first protrusion having a substantially triangular cross section and a second protrusion having a length which is greater than a width thereof and a substantially trapezoidal cross section in planes extending through both length and width dimensions thereof are provided. By press forming, a groove with a substantially V-shaped cross section to mount an optical part, and a groove with a substantially inverse-trapezoidal cross section providing an alignment marking are formed, being inverse-transferred in correspondence with the respective protrusions on one principal surface of a glass substrate. Forming such a pattern on a glass substrate produced with a die enables alignment of the glass substrate with a mask for photolithography with high accuracy.

    摘要翻译: 在模具的按压面上,设置具有大致三角形横截面的第一突起和具有大于其宽度的长度的第二突起和在其长度和宽度尺寸上延伸的平面中的大致梯形横截面。 通过压制成形,形成具有大致V形横截面的槽以安装光学部件,并且形成具有提供对准标记的基本上为倒梯形的横截面的槽,其中一个对应于相应的突起 玻璃基板的主表面。 在用模具制造的玻璃基板上形成这样的图案,可以高精度地对玻璃基板与光刻用掩模进行对准。

    Press mold for glass substrate
    8.
    发明授权
    Press mold for glass substrate 失效
    压模用于玻璃基板

    公开(公告)号:US06223561B1

    公开(公告)日:2001-05-01

    申请号:US09272113

    申请日:1999-03-19

    IPC分类号: C03B1112

    摘要: A press mold for glass substrate includes an upper mold and a lower mold, and a pressure apparatus for applying pressure to the upper mold and the lower mold, for molding a plate-shaped glass substrate having a predetermined thickness between the upper mold and the lower mold. An engaging projected piece is projectingly provided on the side portion of the upper mold, an engaging projected piece supporting portion for supporting the engaging projected piece is provided on the side portion of the lower mold, and an end portion of the upper mold is formed so as to be released from the lower mold with the engaging projected piece as a rotating shaft. Variance in pressure on mold surfaces between the upper mold and lower mold is detected, and a buffer made of material having lower compressive yield strength than material constituting the lower mold is inserted between the lower mold and the pressure apparatus in a position corresponding to the mold surface portion at lower pressure. It is possible to prevent the molded object or the mold from being damaged, and to apply uniform pressure on an entire mold surface by eliminating pressure variance on the mold surface of the mold as far as possible, and therefore, a large glass substrate molded object of excellent quality can be molded.

    摘要翻译: 玻璃基板用压模包括上模和下模,以及用于向上模和下模施加压力的压力装置,用于在上模和下模之间成型具有预定厚度的板状玻璃基板 模子。 在上模的侧部突出设置有接合的突出片,在下模的侧部设置有用于支撑接合突出片的接合突出片支撑部,并且形成上模的端部 以与作为旋转轴的接合突出片从下模释放。 检测上模和下模之间的模具表面的压力差异,并且在与模具相对应的位置中将下模和压装置之间的压缩屈服强度较低的材料制成的缓冲器插入下模和加压装置之间 表面部分处于较低压力。 可以通过尽可能地消除模具的模具表面上的压力变化来防止模制对象或模具被损坏并且对整个模具表面施加均匀的压力,因此,大的玻璃基板模制对象 优良的品质可以模塑。