公开(公告)号:US08182742B2
公开(公告)日:2012-05-22
申请号:US12307681
申请日:2007-07-05
IPC分类号: C22C21/00
CPC分类号: C22C21/00 , C22C21/003 , F16C33/121
摘要: An aluminum-based bearing alloy material and a bearing made therefrom is described, the bearing material having a composition comprising in weight %: 5-10 tin; 0.8-1.3 copper; 0.8-1.3 nickel; 1.5-3 silicon; 0.13-0.19 vanadium; 0.8-1.2 manganese; 0.4-0.6 chromium; balance aluminum apart from incidental impurities.
摘要翻译: 描述了铝基轴承合金材料和由其制成的轴承,所述轴承材料具有重量%的组成:5-10重量份; 0.8-1.3铜; 0.8-1.3镍; 1.5-3硅; 0.13-0.19钒; 0.8-1.2锰; 0.4-0.6铬; 平衡铝与偶然杂质之间的平衡。
-
公开(公告)号:US06296392B1
公开(公告)日:2001-10-02
申请号:US09355640
申请日:1999-07-28
IPC分类号: F16C1700
CPC分类号: F16C33/043 , F16C33/201 , Y10S384/91
摘要: A plain bearing comprises a metal backing, a layer of a porous matrix of sintered metal on the backing and a filled PTFE infiltrated into the interstices of the sintered layer and standing proud of the sintered layer, wherein the PTFE is filled with 1-20% by volume fibrillated aramid fibres and 10-30% by volume glass. The glass is preferably E-glass present as milled filaments of length 0.05-0.30 mm and diameter 0.010-0.020 mm and coated with a silene sizing agent. The fibrillated aramid fibres provide reinforcement and improved load bearing capacity and the glass provides an abrasive filler which abrades asperities on a body and creates a smooth polished surface against which to bear, thereby improving its life. The PTFE preferably also includes ferric oxide and carbon black to about 1.5% and 1.2% by volume respectively which both pigment the polymer and act as an abrasive and lubricant respectively. The carbon black content may be increased to about 10% to provide electrical conductivity. The filler may be prepared as a wet mush or a dry “paper”.
摘要翻译: 滑动轴承包括金属背衬,背衬上的烧结金属多孔基体层和浸入烧结层的间隙中的填充PTFE并且被烧结层骄傲的PTFE,其中PTFE填充有1-20% 体积的原纤维芳族聚酰胺纤维和10-30体积%的玻璃。 优选玻璃优选以长度为0.05-0.30mm和直径为0.010-0.020mm的经研磨的长丝存在并涂覆有硅胶施胶剂。 原纤化芳族聚酰胺纤维提供增强和改善的承载能力,并且玻璃提供磨料填料,其研磨身体上的粗糙度并产生平滑的抛光表面以抵抗该表面,从而改善其寿命。 PTFE优选还包括分别为约1.5%和1.2体积%的氧化亚铁和炭黑,其分别对聚合物着色并用作研磨剂和润滑剂。 炭黑含量可以增加到约10%以提供导电性。 填料可以制成湿糊状物或干燥的“纸”。
-
公开(公告)号:US06688768B2
公开(公告)日:2004-02-10
申请号:US09855854
申请日:2001-05-15
IPC分类号: F16C3304
CPC分类号: F16C33/201 , F16C17/026 , F16C33/04 , F16C33/1065 , F16C33/14 , F16C2220/20 , F16C2220/44 , F16C2220/82 , F16C2223/32 , F16C2240/40 , Y10T29/49668
摘要: A dry bearing (102, FIG. 2(f)) for a hinge pin or the like comprises a bush 402 mounted in a radially supportive housing (16), the bush being formed by a circumferentially discontinuous tubular form made by rolling a strip of steel-backed, bearing material having a filled polymer infiltrated sintered bronze (ISB) lining about a mandrel (FIG. 32, 2(c)). The tubular form is, after mounting and to provide a more uniform inside diameter, burnished by pushing therethrough a burnishing tool (50), having a cylindrical portion (51), of larger diameter than the mounted form. The bearing (and method of manufacture) differ from the art in that a minor part of the lining surface is, prior to passage of the burnishing tool and conveniently when still in strip form, compressed in part as depressions (troughs 442) arrayed over the surface. Such depressions permit burnishing with a less oversize tool to get said uniform inside diameter, thereby requiring less work in driving the tool and with less risk of shearing the lining components and damaging the surrounding housing with radial pressure during burnishing.
摘要翻译: 用于铰链销或类似物的干轴承(102,图2(f))包括安装在径向支撑壳体(16)中的衬套402,衬套由周向不连续的管状形成, 具有填充的聚合物浸入的烧结青铜(ISB)衬套围绕心轴的钢背衬轴承材料(图32,2(c))。 管状形式在安装之后并且提供更均匀的内径,通过推动具有比安装形式更大直径的圆柱形部分(51)的抛光工具(50)来抛光。 轴承(和制造方法)与现有技术不同之处在于,在抛光工具通过之前,方便地当仍然呈带状形式时,衬里表面的较小部分被部分地压缩成凹陷(槽442) 表面。 这种凹陷允许用较小尺寸的工具进行抛光以获得所述均匀的内径,从而在驱动工具时需要较少的工作,并且在抛光期间以较小的剪切衬里部件和径向压力损坏周围壳体的风险较小。
-
公开(公告)号:US06478468B2
公开(公告)日:2002-11-12
申请号:US09861999
申请日:2001-05-18
IPC分类号: F16C3304
CPC分类号: F16C33/043 , F16C33/201 , Y10S384/91
摘要: A plain bearing comprises a metal backing, a layer of a porous matrix of sintered metal on the backing and a filled PTFE infiltrated into the interstices of the sintered layer and standing proud of the sintered layer, wherein the PTFE is filled with 1-20% by volume fibrillated aramid fibres and 10-30% by volume glass. The glass is preferably E-glass present as milled filaments of length 0.05-0.30 mm and diameter 0.010-0.020 mm and coated with a silene sizing agent. The fibrillated aramid fibres provide reinforcement and improved load bearing capacity and the glass provides an abrasive filler which abrades asperities on a body and creates a smooth polished surface against which to bear, thereby improving its life. The PTFE preferably also includes ferric oxide and carbon black to about 1.5% and 1.2% by volume respectively which both pigment the polymer and act as fine abrasive and lubricant respectively. The carbon black content may be increased to about 10% to provide electrical conductivity. The filler may be prepared as a wet mush or a dry “paper”.
摘要翻译: 滑动轴承包括金属背衬,背衬上的烧结金属多孔基体层和浸入烧结层的间隙中的填充PTFE并且被烧结层骄傲的PTFE,其中PTFE填充有1-20% 体积的原纤维芳族聚酰胺纤维和10-30体积%的玻璃。 优选玻璃优选以长度为0.05-0.30mm和直径为0.010-0.020mm的经研磨的长丝存在并涂覆有硅胶施胶剂。 原纤化芳族聚酰胺纤维提供增强和改善的承载能力,并且玻璃提供磨料填料,其研磨身体上的粗糙度并产生平滑的抛光表面以抵抗该表面,从而改善其寿命。 PTFE优选还包括分别为约1.5%和1.2%(体积)的氧化亚铁和炭黑,这两种颜料分别作为细磨料和润滑剂。 炭黑含量可以增加到约10%以提供导电性。 填料可以制成湿糊状物或干燥的“纸”。
-
公开(公告)号:US06272751B1
公开(公告)日:2001-08-14
申请号:US09355641
申请日:1999-07-28
IPC分类号: B21D5300
CPC分类号: F16C33/201 , F16C17/026 , F16C33/04 , F16C33/1065 , F16C33/14 , F16C2220/20 , F16C2220/44 , F16C2220/82 , F16C2223/32 , F16C2240/40 , Y10T29/49668
摘要: A dry bearing (102, FIG. 2(f)) for a hinge pin or the like comprises a bush 402 mounted in a radially supportive housing (16), the bush being formed by a circumferentially discontinuous tubular form made by rolling a strip of steel-backed, bearing material having a filled polymer infiltrated sintered bronze (ISB) lining about a mandrel (FIG. 32, 2(c)). The tubular form is, after mounting and to provide a more uniform inside diameter, burnished by pushing therethrough a burnishing tool (50), having a cylindrical portion (51), of larger diameter than the mounted form. The bearing (and method of manufacture) differ from the art in that a minor part of the lining surface is, prior to passage of the burnishing tool and conveniently when still in strip form, compressed in part as depressions (troughs 442) arrayed over the surface. Such depressions permit burnishing with a less oversize tool to get said uniform inside diameter, thereby requiring less work in driving the tool and with less risk of shearing the lining components and damaging the surrounding housing with radial pressure during burnishing.
摘要翻译: 用于铰链销或类似物的干轴承(102,图2(f))包括安装在径向支撑壳体(16)中的衬套402,衬套由周向不连续的管状形成, 具有填充的聚合物浸入的烧结青铜(ISB)衬套围绕心轴的钢背衬轴承材料(图32,2(c))。 管状形式在安装之后并且提供更均匀的内径,通过推动具有比安装形式更大直径的圆柱形部分(51)的抛光工具(50)来抛光。 轴承(和制造方法)与现有技术不同之处在于,在抛光工具通过之前,方便地当仍然呈带状形式时,衬里表面的较小部分被部分地压缩成凹陷(槽442) 表面。 这种凹陷允许用较小尺寸的工具进行抛光以获得所述均匀的内径,从而在驱动工具时需要较少的工作,并且在抛光期间以较小的剪切衬里部件和径向压力损坏周围壳体的风险较小。
-
公开(公告)号:US20090297392A1
公开(公告)日:2009-12-03
申请号:US12307681
申请日:2007-07-05
IPC分类号: C22C21/02
CPC分类号: C22C21/00 , C22C21/003 , F16C33/121
摘要: An aluminium-based bearing alloy material and a bearing made therefrom is described, the bearing material having a composition comprising in weight %: 5-10 tin; 0.8-1.3 copper; 0.8-1.3 nickel; 1.5-3 silicon; 0.13-0.19 vanadium; 0.8-1.2 manganese; 0.4-0.6 chromium; balance aluminium apart from incidental impurities.
摘要翻译: 描述了铝基轴承合金材料和由其制成的轴承,所述轴承材料具有重量%的组成:5-10重量份; 0.8-1.3铜; 0.8-1.3镍; 1.5-3硅; 0.13-0.19钒; 0.8-1.2锰; 0.4-0.6铬; 平衡铝与偶然杂质之间的平衡。
-
公开(公告)号:US06676898B2
公开(公告)日:2004-01-13
申请号:US09734753
申请日:2000-12-11
IPC分类号: C22C2100
CPC分类号: C22C21/003 , F16C33/121
摘要: A bearing and a bearing alloy composition are described, the bearing alloy comprising in weight %: tin 5-10; copper 0.7-1.3; nickel 0.7-1.3; silicon 1.5-3.5; vanadium 0.1-0.3; manganese 0.1-0.3; and the balance being aluminium apart from unavoidable impurities.
摘要翻译: 描述了一种轴承和一种轴承合金组合物,该轴承合金包含重量%:锡5-10; 铜0.7-1.3; 镍0.7-1.3; 硅1.5-3.5; 钒0.1-0.3; 锰0.1-0.3; 除了不可避免的杂质外,余量为铝。
-
公开(公告)号:US06461679B1
公开(公告)日:2002-10-08
申请号:US09762336
申请日:2001-02-05
IPC分类号: B05D312
CPC分类号: F16C33/201 , C08K3/16 , C08K3/22 , C08L27/12 , C08L27/18 , C08L2205/02 , C08L2666/04
摘要: A bearing material and a method for the production thereof are described. The bearing material comprising a matrix of polytetrafluoroethylene having dispersed therein in volume %: a melt-processable fluoro-polymer in the range from 2 to 10; an inorganic particulate filler material in the range from 10 to 30; and, up to 5 of a ceramic particulate material.
摘要翻译: 对轴承材料及其制造方法进行说明。 轴承材料包括其中以体积%分散的聚四氟乙烯基体:可熔融加工的氟聚合物,其范围为2至10; 无机颗粒填料材料的范围为10-30; 和多达5个陶瓷颗粒材料。
-
公开(公告)号:US06390682B1
公开(公告)日:2002-05-21
申请号:US09622727
申请日:2000-08-21
IPC分类号: F16C3312
CPC分类号: F16C33/201 , C08L27/12 , C08L27/18 , C08L77/10 , C08L2205/02 , C08L2205/16 , F16C33/206 , F16C33/208 , F16C2208/02 , F16C2208/22 , F16C2208/32 , Y10S384/908 , Y10T29/4967 , C08L2666/02
摘要: A plain bearing comprises a metallic backing, a sintered porous metal layer bonded to the backing and a lining layer infiltrated into the pores of the porous metal layer and overlying the sintered metal layer, said lining layer comprising PTFE containing 10-30% by vol. of particulate wear-resistant filler, 2-10% by vol. fibrillated aramid fibers and 2-10% by vol. of a melt processable fluoropolymer. The melt processable fluoropolymer is a copolymer of the group tetrafluoroethylene-hexafluoropropylene, tetrafluoroethylene-perfluoroalkylvinylether and monofluoroalkoxy. Such a bearing exhibits superior cavitation erosion resistance and may, by increasing the temperature and/or duration of the sintering operation that is normally performed after the mixture of ingredients has been applied to a backing material, be made to exhibit significantly improved fatigue strength.
摘要翻译: 滑动轴承包括金属背衬,结合到背衬的烧结多孔金属层和浸入多孔金属层的孔中并覆盖烧结金属层的衬里层,所述衬里层包含含有10-30%(体积)的PTFE。 颗粒状耐磨填料,2-10%(体积) 原纤维芳族聚酰胺纤维和2-10% 的可熔融加工的含氟聚合物。 可熔融加工的含氟聚合物是四氟乙烯 - 六氟丙烯,四氟乙烯 - 全氟烷基乙烯基醚和一氟烷氧基的共聚物。 这种轴承具有优异的抗气蚀侵蚀性,并且可以通过增加在将成分混合物施加到背衬材料之后通常进行的烧结操作的温度和/或持续时间来显示显着提高的疲劳强度。
-
-
-
-
-
-
-
-