APPARATUS AND METHOD FOR THE PROCESSING OF CELLULOSE FIBRES
    1.
    发明申请
    APPARATUS AND METHOD FOR THE PROCESSING OF CELLULOSE FIBRES 有权
    纤维素纤维加工装置及方法

    公开(公告)号:US20130192776A1

    公开(公告)日:2013-08-01

    申请号:US13508321

    申请日:2010-11-05

    IPC分类号: D21B1/34 D21D1/34

    摘要: The invention according to the present invention relates to the manufacture of paper and or boards and/or binding agents and a method and apparatus related to the same by providing for the defibrillation of cellulose fibres into a form in which the same can be subsequently sued to form the finished product directly or can be used to bind other materials together and then be formed into the finished product. The apparatus includes a twin screw conveyor through the material and liquid passes to be processed..

    摘要翻译: 根据本发明的本发明涉及纸和/或板和/或粘合剂的制造,以及与其相关的方法和装置,通过提供将纤维素纤维除纤维形成其中可以随后起诉至 直接形成成品或者可以将其他材料结合在一起,然后形成成品。 该设备包括通过材料的双螺旋输送机和待处理的液体通道。

    Method and apparatus for defibrillating cellulose fibers
    2.
    发明授权
    Method and apparatus for defibrillating cellulose fibers 有权
    除纤维素纤维的方法和装置

    公开(公告)号:US08833681B2

    公开(公告)日:2014-09-16

    申请号:US13379778

    申请日:2010-06-23

    摘要: The current invention is directed to a method and apparatus for defibrillating cellulose fibers achieved through single or multiple passes of raw or pre-processed cellulose fiber slurry with a preferred solid material consistency range of 35% to 55% through twin-screw fiber processing machines. During this processing operation fiber slurries are optionally further enhanced with additional fiber and mineral additives to optimize performance of the material for specific end purposes. The hyper defibrillated fiber slurry produced can be defined as one reaching a Schopper-Riegler (SR) level between 75 SR and 85 SR and/or producing a pressed, dried board with a density of preferably at least 850 kg/m3.

    摘要翻译: 本发明涉及一种通过双螺杆纤维加工机器通过单次或多次通过原料或预处理的纤维素纤维浆料达到35%至55%的优选固体物质稠度范围来除纤维素纤维的方法和装置。 在该加工操作期间,纤维浆料任选地被额外的纤维和矿物添加剂进一步增强,以优化用于特定最终目的的材料的性能。 产生的超除颤纤维浆料可以定义为在75 SR和85 SR之间达到Schopper-Riegler(SR)水平和/或生产密度优选至少为850kg / m 3的压制干燥板的一种。

    Apparatus and method for the processing of cellulose fibres
    3.
    发明授权
    Apparatus and method for the processing of cellulose fibres 有权
    用于处理纤维素纤维的装置和方法

    公开(公告)号:US08752776B2

    公开(公告)日:2014-06-17

    申请号:US13508321

    申请日:2010-11-05

    IPC分类号: B02C1/00 B02C17/00 B02C19/22

    摘要: The invention according to the present invention relates to the manufacture of paper and or boards and/or binding agents and a method and apparatus related to the same by providing for the defibrillation of cellulose fibers into a form in which the same can be subsequently sued to form the finished product directly or can be used to bind other materials together and then be formed into the finished product. The apparatus includes a twin screw conveyor through the material and liquid passes to be processed.

    摘要翻译: 根据本发明的本发明涉及纸和/或板和/或粘合剂的制造,以及与其相关的方法和装置,通过提供将纤维素纤维除纤维形成其中可以随后起诉至 直接形成成品或者可以将其他材料结合在一起,然后形成成品。 该装置包括通过材料的双螺旋输送机和待处理的液体通道。

    Method and Apparatus for Defibrillating Cellulose Fibers
    4.
    发明申请
    Method and Apparatus for Defibrillating Cellulose Fibers 有权
    纤维素纤维除纤维的方法和装置

    公开(公告)号:US20120187226A1

    公开(公告)日:2012-07-26

    申请号:US13379778

    申请日:2010-06-23

    IPC分类号: D21B1/30 B02C23/18 B02C19/22

    摘要: The current invention is directed to a method and apparatus for defibrillating cellulose fibers achieved through single or multiple passes of raw or pre-processed cellulose fiber slurry with a preferred solid material consistency range of 35% to 55% through twin-screw fiber processing machines. During this processing operation fiber slurries are optionally further enhanced with additional fiber and mineral additives to optimize performance of the material for specific end purposes. The hyper defibrillated fiber slurry produced can be defined as one reaching a Schopper-Riegler (SR) level between 75 SR and 85 SR and/or producing a pressed, dried board with a density of preferably at least 850 kg/m3.

    摘要翻译: 本发明涉及一种通过双螺杆纤维加工机器通过单次或多次通过原料或预处理的纤维素纤维浆料达到35%至55%的优选固体物质稠度范围来除纤维素纤维的方法和装置。 在该加工操作期间,纤维浆料任选地被额外的纤维和矿物添加剂进一步增强,以优化用于特定最终目的的材料的性能。 产生的超除颤纤维浆料可以定义为在75 SR和85 SR之间达到Schopper-Riegler(SR)水平和/或生产密度优选至少为850kg / m 3的压制干燥板的一种。