公开(公告)号:US4476266A
公开(公告)日:1984-10-09
申请号:US440491
申请日:1982-11-10
申请人: Tetsuro Maeda , Susumu Ohoka , Masafumi Shingai , Haruo Igawa
发明人: Tetsuro Maeda , Susumu Ohoka , Masafumi Shingai , Haruo Igawa
IPC分类号: C08L31/00 , C08L7/00 , C08L21/00 , C08L23/00 , C08L23/02 , C08L31/02 , C08L31/04 , C08L33/00 , C08L33/04 , C08L51/00 , C08L51/02 , C08L51/04 , C08L55/00 , C08L101/00 , C08L55/02
CPC分类号: C08L23/025 , C08L31/02 , C08L51/04 , C08L2201/52
摘要: (1) A graft copolymer latex obtained by the copolymerization of a rubbery diene polymer latex with an aromatic vinyl monomer and an acrylic monomer is mixed with (2) a copolymer latex having a glass transition point of -40.degree. to 10.degree. C. and a volume-average particle size of at least 0.5.mu. obtained by the copolymerization of an olefin with a vinyl ester of a fatty acid while they are maintained in the form of latex to precipitate a solid resin, whereby a thermoplastic resin composition is obtained. The total solid resin contains at least 11 wt. % of the rubbery diene polymer and at least 1 wt. % of the copolymer of olefin/vinyl ester of fatty acid.
摘要翻译: (1)通过将橡胶二烯聚合物胶乳与芳族乙烯基单体和丙烯酸类单体共聚得到的接枝共聚物胶乳与(2)玻璃化转变点为-40〜10℃的共聚物胶乳混合, 通过将烯烃与脂肪酸的乙烯基酯共聚而得到的体积平均粒径为0.5μm以上,同时将其保持为胶乳形式,使固体树脂沉淀,得到热塑性树脂组合物。 总固体树脂含有至少11wt。 %的橡胶二烯聚合物和至少1wt。 %的脂肪酸的烯烃/乙烯基酯的共聚物。