BENT WINDOWPANE
    1.
    发明申请

    公开(公告)号:US20140011000A1

    公开(公告)日:2014-01-09

    申请号:US13990391

    申请日:2011-12-12

    IPC分类号: B60J1/00

    摘要: A vehicle glazing is described. The vehicle glazing has at least one windowpane having a height from 900 mm to 1650 mm, a top upper edge, a side edge of a pillar, a body edge, and two rectangular surfaces A and B. The surface A has an extent of 800 mm*800 mm and the surface B has an extent of 1000 mm*700 mm. Surface A and surface B are centrally bounded by the lowest contact point of the at least one windowpane with the body edge horizontally with respect to the ground, and the lowest contact point and the point of the top upper edge at the shortest distance from the contact point form a Y0 axis and the points at the furthest distance with respect to the width of the windowpane form a Z0 axis.

    摘要翻译: 描述车辆玻璃。 车辆玻璃具有至少一个具有900mm至1650mm的高度的窗玻璃,顶部上边缘,柱的侧边缘,主体边缘和两个矩形表面A和B.表面A具有800 mm * 800mm,表面B的尺寸为1000mm×700mm。 表面A和表面B由至少一个窗玻璃的最低接触点中心地界定,其中主体边缘相对于地面水平,并且最低接触点和顶部上边缘与距接触点最短距离的点 点形成Y0轴,并且相对于窗玻璃的宽度的最远距离处的点形成Z0轴。

    Apparatus for laminating laminated glazing assemblies
    2.
    发明授权
    Apparatus for laminating laminated glazing assemblies 有权
    叠层玻璃组件的层压装置

    公开(公告)号:US06340045B2

    公开(公告)日:2002-01-22

    申请号:US09790494

    申请日:2001-02-23

    IPC分类号: C03C2712

    摘要: A process for laminating multi-layer pre-forms into laminated glazing assemblies is provided. The pre-forms are first subjected to a vacuum in an inlet lock. Then, the pre-forms are heated to an assembly or bonding temperature in a heating chamber, while still being subjected to vacuum. Next, the pre-forms are pressed using pressing pieces in a pressing chamber, which is also subjected to vacuum. A greater pressure is exerted along the edges of the laminated glazing assemblies so as to bond the edges, preferably by using membranes. In an outlet lock which follows the pressing chamber, the laminated glazing assemblies are again vented to atmospheric pressure. An apparatus suitable for carrying out the process is also provided. The apparatus has chambers which are connected together by conveyors so as to achieve a quasi-continuous flow of material.

    摘要翻译: 提供了一种将多层预成型件层压成层压玻璃窗组件的方法。 预成型件首先在入口锁中进行真空。 然后,将预制件加热到加热室中的组装或粘合温度,同时仍然进行真空。 接下来,使用压缩室中的压制件压制预制件,压制室也受到真空。 较大的压力沿层压的玻璃窗组件的边缘施加,以便优选地通过使用膜来粘结边缘。 在紧随按压室的出口锁中,叠层的玻璃窗组件再次被排放到大气压。 还提供了适于执行该过程的装置。 该装置具有通过输送机连接在一起的室,以实现准连续流动的材料。

    Method for cambering glass sheets by suction
    3.
    发明授权
    Method for cambering glass sheets by suction 有权
    通过抽吸弯曲玻璃板的方法

    公开(公告)号:US08109117B2

    公开(公告)日:2012-02-07

    申请号:US11813145

    申请日:2005-12-15

    IPC分类号: C03B23/035

    摘要: A method and device for bending superposed sheets of glass. The sheets are picked up by a top form furnished with a suction creating an upward airflow blowing over the rim of the sheets, the suction being sufficient to lift and hold the superposed sheets against the top form, then the sheets are pressed between the top form and a full surface solid concave bottom form furnished with openings, the pressing beginning conducted while the suction is not yet finished or is finishing, then the superposed sheets are formed, by suction of the main face of the bottom sheet through the openings of the bottom concave mold, the forming by suction beginning while the pressing is not yet finished, and then the sheets are cooled. Windshields free of optical defects may thus be produced.

    摘要翻译: 一种用于弯曲叠加玻璃片的方法和装置。 纸张被带有抽吸的顶部形式拾取,产生向上吹动的纸张边缘的气流,吸力足以提升和保持叠置的纸张抵靠顶部形状,然后将纸张压在顶部形式 并且具有开口的全表面实心凹形底部形式,当抽吸尚未完成或正在完成时,按压开始,然后通过底部片的主面通过底部的开口抽吸而形成叠置的片材 凹模,在压制尚未完成时通过抽吸开始成型,然后将片冷却。 因此可以产生没有光学缺陷的挡风玻璃。

    Process for laminating laminated glazing assemblies
    5.
    发明授权
    Process for laminating laminated glazing assemblies 有权
    叠层玻璃窗组装的方法

    公开(公告)号:US06432240B1

    公开(公告)日:2002-08-13

    申请号:US09984209

    申请日:2001-10-29

    IPC分类号: C03C2712

    摘要: A process for laminating multi-layer pre-forms into laminated glazing assemblies is provided. The pre-forms are first subjected to a vacuum in an inlet lock. Then, the pre-forms are heated to an assembly or bonding temperature in a heating chamber, while still being subjected to vacuum. Next, the pre-forms are pressed using pressing pieces in a pressing chamber, which is also subjected to vacuum. A greater pressure is exerted along the edges of the laminated glazing assemblies so as to bond the edges, preferably by using membranes. In an outlet lock which follows the pressing chamber, the laminated glazing assemblies are again vented to atmospheric pressure. An apparatus suitable for carrying out the process is also provided. The apparatus has chambers which are connected together by conveyors so as to achieve a quasi-continuous flow of material.

    摘要翻译: 提供了一种将多层预成型件层压成层压玻璃窗组件的方法。 预成型件首先在入口锁中进行真空。 然后,将预制件加热到加热室中的组装或粘合温度,同时仍然进行真空。 接下来,使用压缩室中的压制件压制预制件,压制室也受到真空。 较大的压力沿层压的玻璃窗组件的边缘施加,以便优选地通过使用膜来粘结边缘。 在紧随按压室的出口锁中,叠层的玻璃窗组件再次被排放到大气压。 还提供了适于执行该过程的装置。 该装置具有通过输送机连接在一起的室,以实现准连续流动的材料。

    Process for the manufacture of a pane of laminated glass
    7.
    发明授权
    Process for the manufacture of a pane of laminated glass 有权
    用于制造夹层玻璃板的方法

    公开(公告)号:US06280547B1

    公开(公告)日:2001-08-28

    申请号:US09147278

    申请日:1999-08-27

    IPC分类号: B32B1700

    摘要: The present document describes a process for manufacturing a pane of laminated glass without recourse to an autoclave. The pack of layers are composed of stacked layers (6, 7, 8), is raised to the softening temperature of the thermoplastic interlayer of the pack of layers in a preheat channel (1). The preheated pack of layers is put under vacuum in a vacuum assembly station (2) for the purpose of extracting the gas from the spaces separating the layers (6, 7, 8). After the gas has been extracted, the edge of the pack of layers, which is heid under vacuum, is mechanically compressed inside the vacuum box and is thus sealed. Finally, the pack of layers is brought to atmospheric pressure and its temperature further increased in a postheat channel (4).

    摘要翻译: 本文件描述了用于制造夹层玻璃板的方法,而不需要使用高压釜。 一层层由叠层(6,7,8)组成,在预热通道(1)中升高到一层层的热塑性中间层的软化温度。 在真空组装站(2)中将预热的层包装在真空下,以从分离层(6,7,8)的空间中提取气体。 在气体被抽出之后,将真空下盖的层的边缘在真空箱内被机械地压缩并因此被密封。 最后,使一包层达到大气压,并且在后加热通道(4)中其温度进一步增加。

    HEATING OBJECTS ON A LINE-PRODUCTION OVEN
    9.
    发明申请
    HEATING OBJECTS ON A LINE-PRODUCTION OVEN 审中-公开
    加热生产线上的物体

    公开(公告)号:US20090197215A1

    公开(公告)日:2009-08-06

    申请号:US12302374

    申请日:2007-05-21

    IPC分类号: F27D3/12 F27B5/02 F27D3/00

    摘要: A device for heating objects and a method that has recourse to the device, particularly for heating and/or bending one or more glass panes positioned one on top of the other, covering each other. The device includes a furnace line, plural supports, particularly transport molds that transport and/or bend the objects, the objects being placed on the supports positioned on transport carriages, a drive device that progresses the transport carriages through the furnace line and plural heating elements provided above the objects in the furnace line. In the device the heating elements are positioned on the whole above the entire furnace line and the heating elements can be operated and regulated so as to form heating zones suited to dimensions of the objects.

    摘要翻译: 一种用于加热物体的装置和一种方法,其特征在于用于加热和/或弯曲彼此覆盖的一个或多个玻璃板相互覆盖的装置。 该设备包括炉线,多个支撑件,特别是运输和/或弯曲物体的运输模具,物体被放置在位于运输托架上的支撑件上;驱动装置,其使运输托架通过炉管线和多个加热元件 在炉线上面的物体上方。 在装置中,加热元件整体位于整个炉管线上方,并且加热元件可以被操作和调节,以便形成适合物体尺寸的加热区域。

    Method For Cambering Glass Sheets By Suction
    10.
    发明申请
    Method For Cambering Glass Sheets By Suction 有权
    吸水玻璃板弯曲方法

    公开(公告)号:US20080134722A1

    公开(公告)日:2008-06-12

    申请号:US11813145

    申请日:2005-12-15

    摘要: The invention relates to a method and device for bending superposed sheets of glass, comprising the sheets being picked up by a top form furnished with suction means creating an upward airflow blowing over the rim of the sheets, said suction being sufficient to lift and hold the superposed sheets against said top form, then the pressing of the sheets between the top form and a full surface solid concave bottom form furnished with openings, said pressing beginning while the suction of the preceding step is not yet finished or is finishing, then the forming of the superposed sheets, by suction of the main face of the bottom sheet through the openings of the bottom concave mold, said forming by suction beginning while the pressing is not yet finished, then the cooling of the sheets. Windshields free of optical defects may thus be produced.

    摘要翻译: 本发明涉及一种用于弯曲叠加的玻璃片的方法和装置,其包括由装有抽吸装置的顶部形式拾起的片材,产生向上吹过片材边缘的气流,所述抽吸足以提升并保持 叠置的片材抵靠所述顶部形式,然后在顶部形式和全表面实心凹形底部形式之间压制片材,其具有开口,所述按压开始于前一步骤的抽吸尚未完成或正在完成,然后形成 通过底部凹模的开口的底部片的主面的抽吸,通过在压制尚未完成时通过吸力开始形成,然后冷却片材。 因此可以产生没有光学缺陷的挡风玻璃。