Mixed aliphatic alcohol production
    1.
    发明授权
    Mixed aliphatic alcohol production 失效
    混合脂肪醇生产

    公开(公告)号:US4607056A

    公开(公告)日:1986-08-19

    申请号:US751703

    申请日:1985-07-03

    IPC分类号: C07C29/156 C07C27/06

    CPC分类号: C07C29/156

    摘要: A method is provided for preparing a mixture of lower aliphatic alcohols characterized by containing a substantial proportion of aliphatic alcohols having from 2 to 6 carbon atoms by reacting a mixture of carbon monoxide and hydrogen under suitable conditions of temperature and pressure in the presence of a catalyst comprising molybdenum, a metal from the group consisting of cobalt, iron and nickel, and rhenium, said catalyst being modified by the addition of a promoter from the class consisting of potassium, cesium and rubidium, said promoter being employed at a concentration ranging from about 1.8 to 13.0 micromoles of said alkali per square meter of surface area of said catalyst.

    摘要翻译: 提供了一种制备低级脂族醇的混合物的方法,其特征在于在合适的温度和压力条件下,在催化剂存在下,通过使一氧化碳和氢气的混合物反应,含有大量的具有2至6个碳原子的脂族醇 包括钼,由钴,铁和镍组成的组中的金属和铼,所述催化剂通过从由钾,铯和铷组成的类中加入助催化剂而被修饰,所述促进剂以约从 每平方米所述催化剂表面积为1.8至13.0微摩尔所述碱。

    Process for producing lower aliphatic alcohols
    3.
    发明授权
    Process for producing lower aliphatic alcohols 失效
    低级脂肪醇的制备方法

    公开(公告)号:US4661525A

    公开(公告)日:1987-04-28

    申请号:US728636

    申请日:1985-04-29

    IPC分类号: C07C29/156 C07C27/06

    CPC分类号: C07C29/156 C12C11/02

    摘要: A method is provided for preparing a mixture of lower aliphatic alcohols characterized by containing a substantial proportion of aliphatic alcohols having from 2 to 6 carbon atoms by reacting a mixture of carbon monoxide and hydrogen under suitable conditions of temperature and pressure in the presence of a catalyst comprising molybdenum and a metal from the group consisting of cobalt, iron and nickel, said catalyst being modified by the addition of a promoter from the class consisting of potassium, cesium and rubidium, said promoter being employed at a concentration ranging from about 1.8 to 13.0 micromoles of said alkali per square meter of surface area of said catalyst.

    摘要翻译: 提供了一种制备低级脂族醇的混合物的方法,其特征在于在合适的温度和压力条件下,在催化剂存在下,通过使一氧化碳和氢气的混合物反应,含有大量的具有2至6个碳原子的脂族醇 包括钼和由钴,铁和镍组成的组中的金属,所述催化剂通过从由钾,铯和铷组成的类中加入助催化剂来修饰,所述促进剂以约1.8至13.0的浓度使用 所述碱的平均米表面积为所述碱的微摩尔数。

    Production of C.sub.2 -C.sub.6 aliphatic alcohols
    4.
    发明授权
    Production of C.sub.2 -C.sub.6 aliphatic alcohols 失效
    生产C 2 -C 6脂族醇

    公开(公告)号:US4616040A

    公开(公告)日:1986-10-07

    申请号:US757408

    申请日:1985-07-22

    IPC分类号: C07C29/156 C07C27/06

    CPC分类号: C07C29/156

    摘要: A method is provided for preparing a mixture of lower aliphatic alcohols characterized by containing a substantial proportion of aliphatic alcohols having from 2 to 6 carbon atoms by reacting a mixture of carbon monoxide and hydrogen under suitable conditions of temperature and pressure in the presence of a catalyst comprising molybdenum, a metal from the group consisting of cobalt, iron and nickel, and copper, said catalyst being modified by the addition of a promoter from the class consisting of potassium, cesium and rubidium, said promoter being employed at a concentration ranging from about 1.8 to 13.0 micromoles of said alkali per square meter of surface area of said catalyst.

    摘要翻译: 提供了一种制备低级脂族醇的混合物的方法,其特征在于在合适的温度和压力条件下,在催化剂存在下,通过使一氧化碳和氢气的混合物反应,含有大量的具有2至6个碳原子的脂族醇 包括钼,由钴,铁和镍组成的组中的金属和铜,所述催化剂通过从由钾,铯和铷组成的类中加入助催化剂来修饰,所述促进剂的使用浓度范围为约 每平方米所述催化剂表面积为1.8至13.0微摩尔所述碱。

    Aliphatic alcohol production
    5.
    发明授权
    Aliphatic alcohol production 失效
    脂肪醇生产

    公开(公告)号:US4607055A

    公开(公告)日:1986-08-19

    申请号:US751696

    申请日:1985-07-03

    IPC分类号: C07C29/156 C07C27/06

    CPC分类号: C07C29/156

    摘要: A method is provided for preparing a mixture of lower aliphatic alcohols characterized by containing a substantial proportion of aliphatic alcohols having from 2 to 6 carbon atoms by reacting a mixture of carbon monoxide and hydrogen under suitable conditions of temperature and pressure in the presence of a catalyst comprising molybdenum, a metal from the group consisting of cobalt, iron and nickel, and silver, said catalyst being modified by the addition of a promoter from the class consisting of potassium, cesium and rubidium, said promoter being employed at a concentration ranging from about 1.8 to 13.0 micromoles of said alkali per square meter of surface area of said catalyst.

    摘要翻译: 提供了一种制备低级脂族醇的混合物的方法,其特征在于在合适的温度和压力条件下,在催化剂存在下,通过使一氧化碳和氢气的混合物反应,含有大量的具有2至6个碳原子的脂族醇 包括钼,由钴,铁和镍组成的组中的金属和银,所述催化剂通过从由钾,铯和铷组成的类中加入助催化剂而被修饰,所述促进剂以约从 每平方米所述催化剂表面积为1.8至13.0微摩尔所述碱。