摘要:
The present invention provides a liquid-crystalline polyester blend, which is obtained by combining a liquid-crystalline polyester (A) and a liquid-crystalline polyester (B) such that the ratio by weight of (A)/(B) is 99/1 to 80/20: liquid-crystalline polyester (A) which consists of aromatic oxycarbonyl repeating units, aromatic dioxy repeating units and aromatic dicarbonyl repeating units, and contains 40-80 mol % of the repeating unit represented by formula (I) based on the total repeating units constituting the liquid-crystalline polyester (A); liquid-crystalline polyester (B) which comprises repeating units represented by formulae (I) and (II), wherein the molar proportion of the total amount of the repeating units represented by formulae (I) and (II) based on the total amount of the repeating units constituting the liquid-crystalline polyester (B) is greater than or equal to 90 mol % and the molar proportion of the repeating units represented by formulae (I) to (II) is from 10/90 to 50/50. The liquid-crystalline polyester blend of the present invention exhibits excellent dielectric properties in high frequency regions as well as good impact strength and molding processability.
摘要:
The present invention provides a wholly aromatic liquid-crystalline polyester resin, consisting of the repeating units shown by the formulae [I]-[V]: wherein p, q, r, s and t represent molar proportion (mol %) of repeating units respectively in the liquid-crystalline polyester resin and satisfy the following formulae: 25≦p≦45; 2≦q≦10; 10≦r≦20; 10≦s≦20; 20≦t≦40; r>s; p+q+r+s+t=100; having a ratio P1/P2 of equal to or lower than 3.0, wherein P1 is a melt viscosity at a crystalline melting temperature measured under the condition of shear rate 1000 sec−1 and P2 is a melt viscosity at a temperature of the crystalline melting temperature +20° C. measured under the same condition as P1; and having a deflection temperature under load (DTUL) of equal to or higher than 230° C.
摘要翻译:本发明提供了由式[I] - [V]所示的重复单元组成的全芳香族液晶聚酯树脂:其中p,q,r,s和t表示重复单元的摩尔比(mol%) 分别在液晶聚酯树脂中并满足下式:25≦̸ p≦̸ 45; 2≦̸ q≦̸ 10; 10≦̸ r≦̸ 20; 10≦̸ s≦̸ 20; 20≦̸ t≦̸ 40; r> s p + q + r + s + t = 100; 具有等于或小于3.0的比率P1 / P2,其中P1是在剪切速率1000sec -1的条件下测量的结晶熔融温度下的熔体粘度,P2是在结晶熔融温度的温度下的熔体粘度 在与P1相同的条件下测量+ 20℃; 并具有等于或高于230℃的负载挠曲温度(DTUL)
摘要:
The present invention provides a wholly aromatic liquid-crystalline polyester resin, consisting of the repeating units shown by the formulae [I]-[V]: wherein p, q, r, s and t represent molar proportion (mol %) of repeating units respectively in the liquid-crystalline polyester resin and satisfy the following formulae: 25≦p≦45; 2≦q≦10; 10≦r≦20; 10≦s≦20; 20≦t≦40; r>s; p+q+r+s+t=100; having a ratio P1/P2 of equal to or lower than 3.0, wherein P1 is a melt viscosity at a crystalline melting temperature measured under the condition of shear rate 1000 sec−1 and P2 is a melt viscosity at a temperature of the crystalline melting temperature +20° C. measured under the same condition as P1; and having a deflection temperature under load (DTUL) of equal to or higher than 230° C.
摘要翻译:本发明提供了由式[I] - [V]所示的重复单元组成的全芳香族液晶聚酯树脂:其中p,q,r,s和t表示重复单元的摩尔比(mol%) 分别在液晶聚酯树脂中并满足下列公式:25 @ p @ 45; 2 @ q @ 10; 10 @ r @ 20; 10 @ s @ 20; 20 @ t @ 40; r> s p + q + r + s + t = 100; 具有等于或小于3.0的比率P1 / P2,其中P1是在剪切速率1000sec -1的条件下测量的结晶熔融温度下的熔体粘度,P2是在结晶熔融温度的温度下的熔体粘度 在与P1相同的条件下测量+ 20℃; 并具有等于或高于230℃的负载挠曲温度(DTUL)
摘要:
A liquid-crystalline polyester blend composition includes 100 parts by weight of a liquid-crystalline polyester blend and 0.1-300 parts by weight of calcium titanate and/or barium titanate, wherein the liquid-crystalline polyester blend can be obtained by combining liquid-crystalline polyester (A) (LCP A) and liquid-crystalline polyester (B) (LCP B) such that the ratio by weight of (LCP A)/(LCP B) is 99/1 to 80/20, wherein LCP A and LCP B are as defined in the specification, provided that at least one of LCP A and LCP B includes one or two repeating units that come from corresponding minor copolymerizing components selected from aromatic diol, aromatic dicarboxylic acid, aromatic monocarboxylic acid and aromatic monohydroxy compound.
摘要:
The present invention provides a liquid-crystalline polyester blend composition comprising 100 parts by weight of a liquid-crystalline polyester blend and 0.1-300 parts by weight of calcium titanate and/or barium titanate: wherein said liquid-crystalline polyester blend is obtainable by combining liquid-crystalline polyester (A) (LCP A) and liquid-crystalline polyester (B) (LCP B) such that the ratio by weight of (LCP A)/(LCP B) is 99/1 to 80/20; wherein, LCP A consists of 100 molar parts of major repeating units and optionally 0.1-2 molar parts of one or two repeating units that come from corresponding minor copolymerizing components, wherein the major repeating units are selected from the group consisting of aromatic oxycarbonyl repeating unit, aromatic dioxy repeating unit and aromatic dicarbonyl repeating unit, wherein 40-80 mol % of the major repeating units are the unit represented by formula (I); and the amounts of the aromatic dioxy repeating unit and the aromatic dicarbonyl repeating unit in the major repeating units are equimolar; and LCP B is selected from the group consisting of liquid-crystalline polyester (b-1) (LCP b-1) and liquid-crystalline polyester (b-2) (LCP b-2), each consisting of 100 molar parts of major repeating units and optionally 0.1-2 molar parts of one or two repeating units that come from corresponding minor copolymerizing components; wherein the major repeating units of LCP b-1 are aromatic oxycarbonyl repeating units; and the major repeating units of LCP b-2 are selected from the group consisting of aromatic oxycarbonyl repeating unit, aromatic dioxy repeating unit and aromatic dicarbonyl repeating unit, wherein the amounts of aromatic dioxy repeating unit and aromatic dicarbonyl repeating unit in the major repeating units are equimolar, wherein greater than or equal to 90 mol % of the major repeating units of LCP b-1 and LCP b-2 each are repeating units represented by formulae (I) and (II), and the molar proportion of the repeating units represented by formulae (I) to (II) is from 10/90 to 50/50; provided that at least one of LCP A and LCP B comprises one or two repeating units that come from corresponding minor copolymerizing components selected from the group consisting of aromatic diol, aromatic dicarboxylic acid, aromatic monocarboxylic acid and aromatic monohydroxy compound The liquid-crystalline polyester blend composition of the present invention exhibits excellent dielectric properties as well as good mechanical properties and thermal properties.
摘要:
The present invention provides a liquid-crystalline polyester blend, which is obtained by combining a liquid-crystalline polyester (A) and a liquid-crystalline polyester (B) such that the ratio by weight of (A)/(B) is 99/1 to 80/20: liquid-crystalline polyester (A) which consists of aromatic oxycarbonyl repeating units, aromatic dioxy repeating units and aromatic dicarbonyl repeating units, and contains 40-80 mol % of the repeating unit represented by formula (I) based on the total repeating units constituting the liquid-crystalline polyester (A); liquid-crystalline polyester (B) which comprises repeating units represented by formulae (I) and (II), wherein the molar proportion of the total amount of the repeating units represented by formulae (I) and (II) based on the total amount of the repeating units constituting the liquid-crystalline polyester (B) is greater than or equal to 90 mol % and the molar proportion of the repeating units represented by formulae (I) to (II) is from 10/90 to 50/50. The liquid-crystalline polyester blend of the present invention exhibits excellent dielectric properties in high frequency regions as well as good impact strength and molding processability.