摘要:
A membrane-membrane reinforcing member assembly includes: a polymer electrolyte membrane (1) having a substantially quadrilateral shape; a membrane-like first membrane reinforcing member (10a) disposed on a first main surface (F10) of the polymer electrolyte membrane (1) to bend at a substantially right angle at a corner of the polymer electrolyte membrane (1) and extend along sides forming the corner; and a membrane-like second membrane reinforcing member (10b) disposed on a second main surface (F20) of the polymer electrolyte membrane (1) to bend at a substantially right angle at a corner of the polymer electrolyte membrane (1) and extend along sides forming the corner, and the first membrane reinforcing member (10a) and the second membrane reinforcing member (10b) are disposed to extend along four sides of the polymer electrolyte membrane (1) as a whole.
摘要:
A membrane-membrane reinforcing member assembly includes: a polymer electrolyte membrane (1) having a substantially square shape; a pair of membrane-like first membrane reinforcing members (10a) disposed on one main surface of the polymer electrolyte membrane (1) so as to extend along a pair of opposed sides, respectively, of four sides of said one main surface; and a pair of membrane-like second membrane reinforcing members (10b) disposed on another main surface of the polymer electrolyte membrane (1) so as to extend along a pair of opposed sides, respectively, of four sides of said another main surface, wherein: portions of the polymer electrolyte membrane (1) at which portions the first membrane reinforcing members (10a, 10a) and the second membrane reinforcing members (10b, 10b) are disposed are concave; and the first membrane reinforcing members (10a, 10a) and the second membrane reinforcing members (10b, 10b) are disposed such that main surfaces thereof are exposed, and the first membrane reinforcing members (10a, 10a) and the second membrane reinforcing members (10b, 10b) surround a peripheral portion of the polymer electrolyte membrane (1) as a whole.
摘要:
An operation method of a polymer electrolyte fuel cell system including an anode (3) supplied with a fuel gas containing hydrogen, a cathode (4) supplied with an oxidizing gas containing oxygen, and a polymer electrolyte membrane (5) sandwiched between the anode (3) and the cathode (4), comprises supplying to the anode (3) the fuel gas humidified with a higher level than the oxidizing gas to cause the anode (3) to have a humidified state with a higher level than the cathode (4), in start-up of the polymer electrolyte fuel cell system.
摘要:
A polymer electrolyte fuel cell includes: a sealing structure (9) including a substantially rectangular ring-shaped first gasket portion (9a) and a substantially rectangular ring-shaped second gasket portion (9b), the first gasket portion (9a) being positioned outward of a peripheral portion of a first gas diffusion layer (5) and between a first separator (7) and a first catalyst layer (2) positioned at a peripheral portion of a polymer electrolyte membrane 1, the second gasket portion (9b) being positioned outward of the peripheral portion of the polymer electrolyte membrane (1) and between the first separator (7) and a second separator (8); and at least the first catalyst layer (2), a second catalyst layer (3), and a swellable resin portion (II) formed of a swellable resin whose volume expands when water is added thereto, the swellable resin portion (11) being positioned between the first gasket portion (9a) and the first catalyst layer (2) positioned at the peripheral portion of the polymer electrolyte membrane (1).
摘要:
A membrane membrane-reinforcement-member assembly, membrane catalyst-layer assembly, membrane electrode assembly, and polymer electrolyte fuel cell are provided, which are so configured as to ensure sufficient durability and a cost reduction in unit cells and be suited for mass production. To this end, a membrane membrane-reinforcement-member assembly (20) of a membrane catalyst-layer assembly (30) provided in an MEA (5) of a cell (100) has a polymer electrolyte membrane (1), a pair of first membrane reinforcement members (10a) and a pair of second membrane reinforcement members (10b) which members (10a), (10b) are embedded in the polymer electrolyte membrane (1) such that their main surfaces are not exposed therefrom. The first and second membrane reinforcement members (10a), (10b) are embedded in a parallelogrammatic fashion so as to overlap each other in the four corners of the polymer electrolyte membrane (1) when viewed in a thickness direction of the polymer electrolyte membrane.
摘要:
A method for manufacturing a membrane-electrode assembly of the present invention includes: a reinforcing member disposing step of disposing a reinforcing member (104A, 104B), whose frame portion is formed to surround an opening of the reinforcing member, on a polymer electrolyte membrane (102) such that the frame portion covers a peripheral portion of at least one surface of the polymer electrolyte membrane; a catalyst layer applying step of applying a coating of a catalyst layer (109A, 109B) on at least an entire surface of the polymer electrolyte membrane (102) which surface is exposed from the opening of the reinforcing member (104A, 104B); and a gas diffusion layer disposing step of disposing a gas diffusion layer (114A, 114B) such that the gas diffusion layer covers the catalyst layer (109A, 109B).
摘要:
A membrane membrane-reinforcement-member assembly, membrane catalyst-layer assembly, membrane electrode assembly, and polymer electrolyte fuel cell are provided, which are so configured as to ensure sufficient durability and a cost reduction in unit cells and be suited for mass production. To this end, a membrane membrane-reinforcement-member assembly (20) of a membrane catalyst-layer assembly (30) provided in an MEA (5) of a cell (100) has a polymer electrolyte membrane (1), a pair of first membrane reinforcement members (10a) and a pair of second membrane reinforcement members (10b) which members (10a), (10b) are embedded in the polymer electrolyte membrane (1) such that their main surfaces are not exposed therefrom. The first and second membrane reinforcement members (10a), (10b) are embedded in a parallelogrammatic fashion so as to overlap each other in the four corners of the polymer electrolyte membrane (1) when viewed in a thickness direction of the polymer electrolyte membrane.
摘要:
A membrane-membrane reinforcing member assembly (1) of the present invention includes: a polymer electrolyte membrane (10) having a pair of first main surface (F1) and second main surface (F2) which face each other and each has a substantially rectangular shape; a pair of first membrane reinforcing members 22 and 24 which are disposed on portions, respectively, extending along a pair of opposed sides of four sides of the first main surface (F1), each has a main surface smaller than the first main surface (F1) and each has a film shape; and a pair of second membrane reinforcing members (26) and (28) which are disposed on portions, respectively, extending along a pair of opposed sides of four sides of the second main surface (F2), each has a main surface smaller than the second main surface (F2) and each has a film shape, wherein the pair of first membrane reinforcing members (22) and (24) and the pair of second membrane reinforcing members (26) and (28) are disposed so as to extend along four sides as a whole, respectively, of the polymer electrolyte membrane (10) and so as to sandwich four corners of the polymer electrolyte membrane (10).
摘要:
A membrane-membrane reinforcing member assembly includes: a polymer electrolyte membrane (1) having a substantially square shape; a pair of membrane-like first membrane reinforcing members (10a) disposed on one main surface of the polymer electrolyte membrane (1) so as to extend along a pair of opposed sides, respectively, of four sides of said one main surface; and a pair of membrane-like second membrane reinforcing members (10b) disposed on another main surface of the polymer electrolyte membrane (1) so as to extend along a pair of opposed sides, respectively, of four sides of said another main surface, wherein: portions of the polymer electrolyte membrane (1) at which portions the first membrane reinforcing members (10a, 10a) and the second membrane reinforcing members (10b, 10b) are disposed are concave; and the first membrane reinforcing members (10a, 10a) and the second membrane reinforcing members (10b, 10b) are disposed such that main surfaces thereof are exposed, and the first membrane reinforcing members (10a, 10a) and the second membrane reinforcing members (10b, 10b) surround a peripheral portion of the polymer electrolyte membrane (1) as a whole.
摘要:
A polymer electrolyte fuel cell of the present invention comprises a membrane-electrode assembly (5), a first separator (6a), and a second separator (6b); the first separator (6a) having a groove-shaped first reaction gas channel (8) on one main surface of the first separator (6a) which contacts the first electrode (4a) such that a plurality of straight-line-shaped first rib portions (11) run along each other; the second electrode (4b) having a groove-shaped second reaction gas channel (9) on one main surface of the second electrode (4b) which contacts the second separator (6b) such that a plurality of straight-line-shaped second rib portions (12) run along each other; a ratio of a first reaction gas channel width of at least an upstream portion (18b) of the first reaction gas channel (8) with respect to a second rib portion (12) is greater than 0 and not greater than 1.